Comparative Study of Physical, Mechanical and Tribological Properties of Al2024 Alloy and SiC-TiB2Composites

被引:19
作者
Dey, Dipankar [1 ]
Biswas, Ajay [1 ]
机构
[1] NIT Agartala, Dept Mech Engn, Agartala 799046, India
关键词
Al2024; SiC; TiB2; Mechanical properties; Tribological properties; DRY SLIDING WEAR; TENSILE PROPERTIES; ALUMINUM-ALLOY; FRACTURE-BEHAVIOR; CORROSIVE WEAR; PARTICLE-SIZE; COMPOSITES; MICROSTRUCTURE; TIB2; PARAMETERS;
D O I
10.1007/s12633-020-00560-9
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This paper encapsulates the comparative study of physical, mechanical as well as tribological properties of Al2024 alloy and its composites Al2024-SiC and Al2024-TiB(2)prepared by stir casting technique. Microstructural characterization were conducted using SEM (scanning electron microscope) with EDS (energy-dispersive X-ray spectroscopy). Experimental investigation of density, porosity, microhardness, ultimate tensile strength and wear behaviour of Al2024 alloy and its composites were carried out. Microstructural characterization confirms uniform distribution of SiC and TiB(2)particulates and excellent matrix-reinforcement interfacial bonding. Enhanced mechanical and tribological properties were observed for both the prepared composites compared to Al2024 alloy; this increment was higher for Al2024-TiB(2)composite than Al2024-SiC composite. Al2024-TiB(2)composite exhibits superior wear resistance with non-existence of plastic deformation and adhesion on the wear tracks. The size and shape of the debris also play an important role in determining the wear rates of Al2024 alloy and its composites.
引用
收藏
页码:1895 / 1906
页数:12
相关论文
共 47 条
  • [1] Effects of silicon carbide reinforcement on microstructure and properties of cast Al-Si-Fe/SiC particulate composites
    Aigbodion, V. S.
    Hassan, S. B.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 447 (1-2): : 355 - 360
  • [2] Tensile and fracture behavior of nano/micro TiB2 particle reinforced casting A356 aluminum alloy composites
    Akbari, M. Karbalaei
    Baharvandi, H. R.
    Shirvanimoghaddam, K.
    [J]. MATERIALS & DESIGN, 2015, 66 : 150 - 161
  • [3] Fabrication and study on mechanical properties and fracture behavior of nanometric Al2O3 particle-reinforced A356 composites focusing on the parameters of vortex method
    Akbari, M. Karbalaei
    Mirzaee, O.
    Baharvandi, H. R.
    [J]. MATERIALS & DESIGN, 2013, 46 : 199 - 205
  • [4] Microstructure evolution and wear properties of in situ synthesized TiB2 and TiC reinforced steel matrix composites
    Akhtar, Farid
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 459 (1-2) : 491 - 497
  • [5] Boopathi M. Mahendra, 2013, American Journal of Applied Sciences, V10, P219, DOI 10.3844/ajassp.2013.219.229
  • [6] Interfacial strength and structure of joining between 2024 aluminum alloy and SiCp/2024 Al composite in semi-solid state
    Cheng, Y. S.
    Zhang, X. H.
    [J]. MATERIALS & DESIGN, 2015, 65 : 7 - 11
  • [7] Evaluation of wear performance of Al2024-SiC ex -situ composites
    Dey, Dipankar
    Chintada, Sudhir Kumar
    Bhowmik, Abhijit
    Biswas, Ajay
    [J]. MATERIALS TODAY-PROCEEDINGS, 2020, 26 : 2996 - 2999
  • [8] Wear behavior of stir casted aluminum -titanium diboride (Al2024-TiB 2 ) composite
    Dey, Dipankar
    Bhowmik, Abhijit
    Biswas, Ajay
    [J]. MATERIALS TODAY-PROCEEDINGS, 2020, 26 : 1203 - 1206
  • [9] Effects of stirring parameters on microstructure and tensile properties of (ABOw+SiCp)/6061Al composites fabricated by semi-solid stirring technique
    Guan Li-na
    Geng Lin
    Zhang Hong-wei
    Huang Lu-jun
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 : S274 - S279
  • [10] Aluminum Silicon Carbide Particulate Metal Matrix Composite Development Via Stir Casting Processing
    Inegbenebor, A. O.
    Bolu, C. A.
    Babalola, P. O.
    Inegbenebor, A. I.
    Fayomi, O. S. I.
    [J]. SILICON, 2018, 10 (02) : 343 - 347