摘要
Glare, a fibre metal laminate (FML), consists of several thin 2014-T6 aerospace aluminium alloy layers alternately bonded with E-glass fibre based composite prepregs in the present work. As cracked Glare is subjected to load, load or fibre bridging over cracks in soft aluminium layers causes diversion of load away from the cracks towards stronger intact fibres in the prepregs resulting in stress reduction or shielding effect at the crack tips. Fibre bridging diminishes if delaminations, caused by the development of interfacial cracks at the interfaces of aluminium and fibre layers, exist in the laminate. The paper investigates the cracked but non-delaminated Glare containing normal Mode I cracks in all its aluminium layers. Different crack lengths are considered in the laminates to examine the influence of crack size over bridging. A theoretical model is presented to determine fibre bridging stress for estimation of fibre bridging stress intensity parameter that quantifies the effect of bridging in the laminate. Crack tip stress intensity parameter is also found. The model is successfully validated by undertaking finite element analysis of series of un-identically cracked Glare laminates without delaminations under critical or fracture loads that are obtained experimentally by subjecting the laminates to load-extension test. Plain aerospace aluminium alloy specimens are also tested for fracture. Fracture toughness values of the laminates are seen to be significantly higher than that of plain aluminium specimens. The phenomenon of fibre bridging in the laminates is well substantiated and quantified by all the adopted procedures. (C) 2013 Elsevier Masson SAS. All rights reserved.
引用
收藏
页码:152 / 170
页数:19
相关论文
共 27 条
[1]  
Abdullah S., 2009, EUR J SCI RES, V35, P43
[2]   Analytical prediction model for fatigue crack propagation and delamination growth in Glare [J].
Alderliesten, R. C. .
INTERNATIONAL JOURNAL OF FATIGUE, 2007, 29 (04) :628-646
[3]   Fatigue and damage tolerance issues of Glare in aircraft structures [J].
Alderliesten, R. C. ;
Homan, J. J. .
INTERNATIONAL JOURNAL OF FATIGUE, 2006, 28 (10) :1116-1123
[4]   On the available relevant approaches for fatigue crack propagation prediction in Glare [J].
Alderliesten, R. C. .
INTERNATIONAL JOURNAL OF FATIGUE, 2007, 29 (02) :289-304
[5]   Modelling cyclic shear deformation of fibre/epoxy layers in fibre metal laminates [J].
Alderliesten, Rene ;
Campoli, Glanni ;
Benedictus, Rinze .
COMPOSITES SCIENCE AND TECHNOLOGY, 2007, 67 (11-12) :2545-2555
[6]   The meaning of threshold fatigue in fibre metal laminates [J].
Alderliesten, Rene ;
Rans, Calvin .
INTERNATIONAL JOURNAL OF FATIGUE, 2009, 31 (02) :213-222
[7]   Computational Investigation of Glare with Several Cracks and Delaminations under Monotonic and Cyclic Loads of Constant Amplitude [J].
Bhat, Sunil ;
Patibandla, Rajasekhar .
MECHANICS OF ADVANCED MATERIALS AND STRUCTURES, 2014, 21 (08) :607-630
[8]  
Brown K, 2000, STRUCT MAT, V6, P323
[9]  
Callister Jr WD, 2004, MAT SCI ENG INTRO, P737
[10]   Modeling of fatigue crack growth in notched fiber metal laminates [J].
Chang, Po-Yu ;
Yang, Jenn-Ming .
INTERNATIONAL JOURNAL OF FATIGUE, 2008, 30 (12) :2165-2174