Microstructure and tribological property of nanocrystalline Co-W alloy coating produced by dual-pulse electrodeposition

被引:36
|
作者
Su, Feng-hua [1 ]
Huang, Ping [1 ]
机构
[1] S China Univ Technol, Sch Mech & Automot Engn, Guangzhou 510641, Guangdong, Peoples R China
基金
中国国家自然科学基金;
关键词
Coatings; Nanostructure; Tribology; Electrodeposition; SLIDING WEAR BEHAVIOR; COBALT-TUNGSTEN ALLOYS; NI-W; FE-W; IRON ALLOYS; THIN-FILMS; GRAIN-SIZE; ELECTROLYTES; RESISTANCE; FRICTION;
D O I
10.1016/j.matchemphys.2012.03.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The nanocrystalline Co-W alloy coatings were produced by dual-pulse electrodeposition from aqueous bath with cobalt sulfate and sodium tungstate (Na2WO4). Influence of the current density and Na2WO4 concentration in bath on the microstructure, morphology and hardness of the Co-W alloy coatings were investigated using an X-ray diffraction, a scanning electronic microscope and a Vickers hardness tester, respectively. In addition, the friction and wear properties of the Co-W alloy coating electrodeposited under different condition were evaluated with a ball-on-disk UMT-3MT tribometer. The correlation between the electrodeposition condition, the microstructure and alloy composition, and the hardness and tribological properties of the deposited Co-W alloy coatings were discussed in detail. The results showed that the microhardness of the deposited Co-W alloy coating was significantly affected by its average grain size, W content and crystal orientation. Smaller grain size, higher W content and strong hcp (1 0 0) orientation favor the improvement of the hardness for Co-W alloy coatings. The deposited Co-W alloy coating could obtain the maximum microhardness over 1000 kgf mm(-2) by careful control of the electrodeposition conditions. The tribological properties of the electrodeposited Co-W alloy coating were greatly affected by its grain size, microhardness, surface morphologies and composition, and could be significantly improved by optimizing the electrodeposition condition. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:350 / 359
页数:10
相关论文
共 45 条
  • [21] Size effect of microhardness of nanocrystalline Co-W coatings produced from citrate and gluconate solutions
    Silkin S.A.
    Gotelyak A.V.
    Tsyntsaru N.I.
    Dikusar A.I.
    Surface Engineering and Applied Electrochemistry, 2015, 51 (03) : 228 - 234
  • [22] Effects of Co and W alloying elements on the electrodeposition aspects and properties of nanocrystalline Ni alloy coatings
    Farzaneh, M. A.
    Zamanzad-Ghavidel, M. R.
    Raeissi, K.
    Golozar, M. A.
    Saatchi, A.
    Kabi, S.
    APPLIED SURFACE SCIENCE, 2011, 257 (13) : 5919 - 5926
  • [23] Nanocrystalline Co-Ni alloy coating produced with supercritical carbon dioxide assisted electrodeposition with excellent wear and corrosion resistance
    Liu, Cansen
    Su, Fenghua
    Liang, Jizhao
    SURFACE & COATINGS TECHNOLOGY, 2016, 292 : 37 - 43
  • [24] Influence of pulse parameters on microstructure and corrosion characteristics of electrodeposited Ni-W alloy coating
    Chen, Yu-Hao
    Huang, Sheng-Jie
    Booncam, Jindaluck
    Liang, Jui-Teng
    Lin, Hwai-En
    MATERIALS TODAY COMMUNICATIONS, 2024, 38
  • [25] Influence of pulse-electroplating parameters on the morphology, structure, chemical composition and corrosion behavior of Co-W alloy coatings
    Zehtab, M.
    Najafisayar, P.
    RESULTS IN SURFACES AND INTERFACES, 2024, 15
  • [26] Electrochemical Synthesis of Amorphous Layers from a Nonequilibrium Co-W Alloy as a Precursor for Nanocomposite Coating Formation
    Krasikov, A. V.
    Kastsova, A. G.
    Markov, M. A.
    Bykova, A. D.
    Kravchenko, I. N.
    Galinovskii, A. L.
    RUSSIAN METALLURGY, 2022, 2022 (06): : 666 - 673
  • [27] Microstructure, tribological property and high temperature tensile property of Co-Cr-Ni-W alloy parts fabricated by laser directed energy deposition
    Huang, Y. C.
    Wu, H.
    Xu, T. Z.
    Wang, R.
    Zhang, S.
    Zhang, C. H.
    Wu, C. L.
    Chen, H. T.
    SURFACE & COATINGS TECHNOLOGY, 2024, 483
  • [28] Tribological properties of Ni-W-TiO2-GO composites produced by ultrasonically-assisted pulse electro co-deposition
    Uysal, Mehmet
    Algul, Hasan
    Duru, Erhan
    Kahraman, Yasar
    Alp, Ahmet
    Akbulut, Hatem
    SURFACE & COATINGS TECHNOLOGY, 2021, 410
  • [29] EFFECTS OF CURRENT DENSITY ON MICROSTRUCTURE OF W COATING ON V-4Cr-4Ti ALLOY BY ELECTRODEPOSITION
    Li Xuliang
    Zhang Yingchun
    Jiang Fan
    Wang Lili
    Liu Yanhong
    Sun Ningbo
    ACTA METALLURGICA SINICA, 2013, 49 (06) : 745 - 750
  • [30] Microstructure and tribological performance of sulfurizing layer prepared on the laser cladding Co-based alloy coating
    Cui, Gang
    Han, Bin
    Zhao, Jianbo
    Yang, Zinan
    SURFACE & COATINGS TECHNOLOGY, 2017, 331 : 27 - 34