EVALUATION OF STRESS CORROSION RESISTANCE PROPERTIES OF 15CrMoR(H) IN H2S ENVIRONMENT

被引:0
|
作者
Zhang, Yiliang [1 ]
Wang, Jing [1 ]
Wu, Mingyao [1 ]
Li, Shurui [2 ]
Liu, Wenbin [2 ]
机构
[1] Beijing Univ Technol, Coll Mech Engn & Appl Elect Technol, Beijing 100124, Peoples R China
[2] Wuhan Iron & Steel Grp Corp, Wuhan 430083, Peoples R China
关键词
15CrMoR(H) Materials; Stress Corrosion; Hydrogen Induced Cracking; H2S Environment;
D O I
暂无
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
To evaluate the hydrogen resistant properties of the 15CrMoR(H) with new smelting process, according to NACE and National Standards, three tests including NACE standard tensile test, NACE standard bent-beam test and hydrogen induced cracking test are executed in saturated hydrogen sulfide(H2S) environment. Stress-life mathematical model of this material is given by analyzing and fitting the results of tensile test. Test results show that the threshold sigma th of tensile test is 0.7R(eL)(252MPa); the threshold nominal stress Sc of bent-beam is higher than 4.5 R-eL (1620MPa); for HIC test, the crack length rate CLR is 4.40%, the crack thickness rate CTR is 0.87% and the crack sensitive rate CSR is 0.04%. Compare with EFC standard, the safety margin of HIC test is 3.4, 3.4 and 37.5 times respectively. All the experimental results show that the new 15CrMoR(H) material has excellent H2S environmental cracking resistance properties.
引用
收藏
页码:821 / 829
页数:9
相关论文
共 50 条
  • [21] Stress corrosion cracking of 2205 duplex stainless steel in H2S–CO2 environment
    Z. Y. Liu
    C. F. Dong
    X. G. Li
    Q. Zhi
    Y. F. Cheng
    Journal of Materials Science, 2009, 44 : 4228 - 4234
  • [22] Multiphasic inhibition of mild steel corrosion in H2S gas environment
    Kannan, P.
    Jithinraj, P.
    Natesan, M.
    ARABIAN JOURNAL OF CHEMISTRY, 2018, 11 (03) : 388 - 404
  • [23] H2S corrosion in urea plant
    不详
    MATERIALS PERFORMANCE, 2002, 41 (10) : 44 - 44
  • [24] H2S corrosion at low temperature
    不详
    MATERIALS PERFORMANCE, 2006, 45 (12) : 62 - 62
  • [25] 15CrMoR与800H异种钢焊接问题的探讨
    高海水
    中国锅炉压力容器安全, 2002, 18 (02) : 38 - 39
  • [26] Stress corrosion behavior of FV520B steel in H2S/CO2 environment
    School of Mechanical Engineering, Shandong University, Jinan
    250061, China
    不详
    264209, China
    不详
    264209, China
    Dongbei Daxue Xuebao, 12 (1790-1794): : 1790 - 1794
  • [27] Stress Corrosion Behavior and Cracking Mechanism of 2205 Duplex Stainless Steel in Acidic H2S Environment
    Yang, Shizhou
    Li, Chunfu
    Li, Hui
    Wen, Ping
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2018, 47 (03): : 904 - 909
  • [28] Stress Corrosion Behavior and Cracking Mechanism of 2205 Duplex Stainless Steel in Acidic H2S Environment
    Yang Shizhou
    Li Chunfu
    Li Hui
    Wen Ping
    RARE METAL MATERIALS AND ENGINEERING, 2018, 47 (03) : 904 - 909
  • [29] Evaluation of H2S working environment effects on installation components
    Fleser, T
    REVISTA DE CHIMIE, 2005, 56 (01): : 35 - 38
  • [30] Prevention of wet H2S stress corrosion cracking by thermal spraying
    Zhang, YL
    Sun, YF
    STRUCTURAL INTEGRITY AND MATERIALS AGING: FRACTURE MECHANICS AND APPLICATIONS, 2003, : 215 - 218