Multi-scale analysis of hypochlorite induced PES/PVP ultrafiltration membranes degradation

被引:78
作者
Pellegrin, Bastien [1 ,2 ]
Prulho, Romain [3 ,4 ]
Rivaton, Agnes [3 ,4 ]
Therias, Sandrine [3 ,4 ]
Gardette, Jean-Luc [3 ,4 ]
Gaudichet-Maurin, Emmanuelle [5 ]
Causserand, Christel [1 ,2 ]
机构
[1] Univ Toulouse, INPT, UPS, Lab Genie Chim, F-31062 Toulouse 09, France
[2] CNRS, UMR 5503, Lab Genie Chim, F-31062 Toulouse, France
[3] Univ Clermont Ferrand, Univ Blaise Pascal, ICCF, F-63000 Clermont Ferrand, France
[4] CNRS, UMR 6505, ICCF, F-63171 Aubiere, France
[5] Veolia Environm Res & Innovat, Maisons Laffitte Res Ctr, F-78603 Maisons Laffitte, France
关键词
Ageing; Hypochlorite cleaning; PES; PVP; Ultrafiltration; BLEACH; PYRROLIDONE); TEMPERATURE; CONTACT; BLENDS; WATER; FLUX;
D O I
10.1016/j.memsci.2013.07.026
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
In drinking water production plants, the use of oxidants such as sodium hypochlorite during in place cleanings may impair the membrane integrity and radically impact the ultrafiltration process efficiency, leading to potential contamination of the permeate water with pathogens. This study investigates the effects of hypochlorite exposure on the properties of a commercially available UP hollow fiber. Mechanical performances and water permeability appeared to be greatly affected by the contact with hypochlorite. Monitoring the molecular changes by X-ray photoelectron spectroscopy (XPS), attenuated total reflectance infrared spectroscopy (ATR-IR), size exclusion chromatography (SEC) and VITA mode atomic force microscopy (VITA-AFM) revealed high stability of the main polymer constituting the membrane (i.e. polyethersulfone (PES)) and very high reactivity of the additive (i.e poly(N-vinyl pyrrolidone) (PVP)) towards immersion in aqueous sodium hypochlorite solution with maximal reaction rate for neutral to slightly basic pH. Correlation of those results unexpectedly leads to the conclusion that the overall membrane properties changes are governed by the additive fate. (c) 2013 Elsevier B.V. All tights reserved
引用
收藏
页码:287 / 296
页数:10
相关论文
共 25 条
[1]   Impact of chemical cleaning on properties and functioning of polyethersulfone membranes [J].
Arkhangelsky, Elizabeth ;
Kuzmenko, Denis ;
Gitis, Vitaly .
JOURNAL OF MEMBRANE SCIENCE, 2007, 305 (1-2) :176-184
[2]   Hypochlorite cleaning causes degradation of polymer membranes [J].
Arkhangelsky, Elizabeth ;
Kuzmenko, Denis ;
Gitis, Norm V. ;
Vinogradov, Michael ;
Kuiry, Suresh ;
Gitis, Vitaly .
TRIBOLOGY LETTERS, 2007, 28 (02) :109-116
[3]   Ageing of polysulfone membranes in contact with bleach solution: Role of radical oxidation and of some dissolved metal ions [J].
Causserand, Christel ;
Rouaix, Sandrine ;
Lafaille, Jean-Pierre ;
Aimar, Pierre .
CHEMICAL ENGINEERING AND PROCESSING-PROCESS INTENSIFICATION, 2008, 47 (01) :48-56
[4]   Fiber failure frequency and causes of hollow fiber integrity loss [J].
Gijsbertsen-Abrahamse, AJ ;
Cornelissen, ER ;
Hofman, JAMH .
DESALINATION, 2006, 194 (1-3) :251-258
[5]   Photooxidation of poly(N-vinylpyrrolidone) (PVP) in the solid state and in aqueous solution [J].
Hassouna, Fatima ;
Therias, Sandrine ;
Mailhot, Gilles ;
Gardette, Jean-Luc .
POLYMER DEGRADATION AND STABILITY, 2009, 94 (12) :2257-2266
[6]   Photo-crosslinked acrylates degradation kinetics [J].
Krongauz, Vadim V. ;
Ling, Michael T. K. .
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2009, 96 (03) :715-725
[7]   The effects of polymer chain rigidification, zeolite pore size and pore blockage on polyethersulfone (PES)-zeolite A mixed matrix membranes [J].
Li, Y ;
Chung, TS ;
Cao, C ;
Kulprathipanja, S .
JOURNAL OF MEMBRANE SCIENCE, 2005, 260 (1-2) :45-55
[8]  
Mark J.E., 1999, POLYM DATA HDB, P962
[9]  
Mark J.E., 1999, POLYM DATA HDB, P480
[10]   ACID IONIZATION CONSTANT OF HOCL FROM 5 TO 35 DEGREES [J].
MORRIS, JC .
JOURNAL OF PHYSICAL CHEMISTRY, 1966, 70 (12) :3798-&