The Effects of Thermophysical Properties and Environmental Conditions on Fire Performance of Intumescent Coatings on Glass Fibre-Reinforced Epoxy Composites

被引:33
作者
Kandola, Baljinder K. [1 ]
Luangtriratana, Piyanuch [1 ]
Duquesne, Sophie [2 ]
Bourbigot, Serge [2 ]
机构
[1] Univ Bolton, Inst Mat Res & Innovat, Bolton BL3 5AB, England
[2] Univ Lille, Ecole Natl Super Chim Lille, Grp React & Resistance Fire R2Fire, Unite Mat & Transformat UMET,CNRS,UMR 8207, F-59652 Villeneuve Dascq, France
基金
英国工程与自然科学研究理事会;
关键词
intumescent coatings; char expansion; cone calorimetry; thermal conductivity at high temperatures; durability; mechanical properties; SURFACE-COATINGS; PROTECTION;
D O I
10.3390/ma8085216
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Intumescent coatings are commonly used as passive fire protection systems for steel structures. The purpose of this work is to explore whether these can also be used effectively on glass fibre-reinforced epoxy (GRE) composites, considering the flammability of the composites compared to non-flammable steel substrate. The thermal barrier and reaction-to-fire properties of three commercial intumescent coatings on GRE composites have been studied using a cone calorimeter. Their thermophysical properties in terms of heating rate and/or temperature dependent char expansion ratios and thermal conductivities have been measured and correlated. It has been suggested that these two parameters can be used to design coatings to protect composite laminates of defined thicknesses for specified periods of time. The durability of the coatings to water absorption, peeling, impact, and flexural loading were also studied. A strong adhesion between all types of coatings and the substrate was observed. Water soaking had a little effect on the fire performance of epoxy based coatings. All types of 1 mm thick coatings on GRE helped in retaining similar to 90% of the flexural property after 2 min exposure to 50 kW/m(2) heat flux whereas the uncoated laminate underwent severe delamination and loss in structural integrity after 1 min.
引用
收藏
页码:5216 / 5237
页数:22
相关论文
共 26 条
[1]  
[Anonymous], 2014, 834102014 ISO
[2]  
[Anonymous], 2007, 24092007 ISO
[3]  
[Anonymous], 2012, D7136D713612 ASTM IN
[4]   Assessing the performance of intumescent coatings using bench-scaled cone calorimeter and finite difference simulations [J].
Bartholmai, M. ;
Schartel, B. .
FIRE AND MATERIALS, 2007, 31 (03) :187-205
[5]  
BSI Standards Publication Fire Tests on Building Materials and StructuresPart 15, 1993, 476151993 BSI
[6]  
BSI Standards Publication Test Methods for Determining the Contribution to the Fire Resistance of Structural Members, 2010, 1338182010 BS EN
[7]  
Camino G, 2001, FIRE RETARDANT MATERIALS, P318
[8]   Intumescent paints: fire protective coatings for metallic substrates [J].
Duquesne, S ;
Magnet, S ;
Jama, C ;
Delobel, R .
SURFACE & COATINGS TECHNOLOGY, 2004, 180 :302-307
[9]   Thermal degradation and fire performance of intumescent silicone-based coatings [J].
Gardelle, B. ;
Duquesne, S. ;
Rerat, V. ;
Bourbigot, S. .
POLYMERS FOR ADVANCED TECHNOLOGIES, 2013, 24 (01) :62-69
[10]   Resistance to fire of silicone-based coatings: Fire protection of steel against cellulosic fire [J].
Gardelle, Bastien ;
Duquesne, Sophie ;
Vandereecken, Patrick ;
Bourbigot, Serge .
JOURNAL OF FIRE SCIENCES, 2014, 32 (04) :374-387