Abrasive wear behavior in dry condition of a plasticity-induced transformation steel

被引:1
|
作者
Sergio Pacheco-Cedeno, Jose [1 ]
de Jesus Cruz-Rivera, Jose [2 ]
Medina Flores, Ariosto [3 ]
Guerra Lopez, Francisco Vapeani [3 ]
Vite-Torres, Manuel [4 ]
Bernal, J. L. [5 ]
Garnica-Gonzalez, Pedro [6 ]
机构
[1] Univ Autonoma Estado Hidalgo, Escuela Super Ciudad Sahagan Ingn Mecan, Carretera Cd SahagUn O Tumba S-N, Zona Ind 43990, Hidalgo, Mexico
[2] Univ Autonoma San Luis Potosi, Inst Metalurgia, Lomas 2a Secci6n, Sierra Leona 550,Lomas 2a Secc, San Luis Potosi 78210, San Luis Potosi, Mexico
[3] UMSNH, Inst Invest Metalurgia & Mat, Edif U Ciudad Univ, Morelia 58040, Michoacan, Mexico
[4] SEPI ESIME IPN, Grp Tribol, Dept Ingn Mecan, UZ Edif 5,Av IPN S-N, Mexico City 07738, DF, Mexico
[5] Inst Tecnol Orizaba, Dept Ingn Mecan, Ote 9, Orizaba 94320, Veracruz, Mexico
[6] Tecnol Nacl Mexico, Div Estudios Posgrad, Campus Inst Tecnol Morelia,Av Tecnol 1500, Morelia 58120, Michoacan, Mexico
关键词
heat-treated; abrasive; wear; abrasive wear; TRIP steel; microstructure; wear and tribology; FATIGUE-CRACK GROWTH; RETAINED AUSTENITE; MICROSTRUCTURAL FEATURES; MECHANICAL-PROPERTIES; RESISTANCE; PERFORMANCE; HARDNESS; WET;
D O I
10.1088/2051-672X/ac9071
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The microstructural, mechanical, and tribological evaluation was carried out through an abrasion test of low alloy steel: 0,21%C, 1,22%Mn, and 2,16%Si with/without heat treatment. The steel was manufactured in an electric induction furnace from AISI-1018 steel with additions of FeMn and FeSi. Later it was hot rolled and heat treated. The microstructure of steel without heat treatment is ferritic-pearlitic with sigma (u) = 714 MPa, S = 8%, and a hardness of 21 HRC. The microstructure of the heat-treated steel corresponds to a Plasticity Induced Transformation (TRIP) steel with sigma (u) = 890 MPa, S = 30%, and hardness of 22 HRC. Both types of steel were subjected to abrasive wear (ASTM G-65) with silica sand particles and loads of 45, 66,5, and 130 N. The TRIP effect (transformation of retained austenite into martensite during plastic deformation) was evaluated before and after the tensile test by x-ray diffraction analysis. The results of the abrasion tests showed that the TRIP steel did not present high resistance characteristics, however, it shows better performance than steels with high carbon and/or alloy contents. The results show that with 45 N the TRIP steel is less resistant than the ferritic-pearlitic steel, however, with 66,5 and 130 N, its abrasive wear performance improved by 17% concerning the ferritic-pearlitic steel, which is attributed to the deformation capacity of TRIP steel. The main wear mechanisms present in TRIP steel are: ploughing, fractures, plastic deformation, pits, cracks, cutting, and micro-cutting. On the other hand, the surface hardness in the abrasion test footprint did not show any change that could be related to the TRIP effect. The microstructure analysis reveals that the material's detachment occurs at the grain boundaries of the ferrite, in which the cracks that cause the detachment of the material were generated and propagated.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] The influence of cryogenic rolling on a transformation-induced plasticity steel
    Hu, Zhiping
    Liu, Rendong
    Lin, Li
    Wang, Guodong
    MATERIALS SCIENCE AND TECHNOLOGY, 2020, 36 (13) : 1381 - 1388
  • [32] Sliding wear behavior of a high-Mn austenitic twinning induced plasticity (TWIP) steel microalloyed with Nb
    Mejia, I.
    Bedolla-Jacuinde, A.
    Pablo, J. R.
    WEAR, 2013, 301 (1-2) : 590 - 597
  • [33] Tribological Behavior of a 0.33% C Dual-Phase Steel with Pre I/C Hardening and Tempering Treatment under Abrasive Wear Condition
    Shukla, Neha
    Roy, Himadri
    Show, Bijay Kumar
    TRIBOLOGY TRANSACTIONS, 2016, 59 (04) : 593 - 603
  • [34] In situ postweld heat treatment of transformation induced plasticity steel resistance spot welds
    Sajjadi-Nikoo, S.
    Pouranvari, M.
    Abedi, A.
    Ghaderi, A. A.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2018, 23 (01) : 71 - 78
  • [35] Effect of Pre-corrosion Damage on Dry Sliding Wear Behavior of Differently Heat-Treated Martensitic Stainless Steel
    Khare, Neelima
    Bonagani, Sunil Kumar
    Limaye, P. K.
    Kumar, Naveen
    Kain, Vivekanand
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (02) : 618 - 633
  • [36] Low-alloyed steel with superior dry abrasive wear resistance and mechanical properties processed via steel mold casting
    Boehm, Anne, V
    Bader, Mark A.
    Kochta, Fabian
    Kunz, Clemens
    Kuehn, Uta
    Neufeld, Kai
    Giebeler, Lars
    Hufenbach, Julia K.
    WEAR, 2025, 566
  • [37] Friction and Wear Behavior of 45# Steel with Different Plant Abrasive
    Yang, Chuan-jia
    Huang, Xiao-peng
    Wu, Jing-feng
    Wan, Fang-xin
    ADVANCES IN MANUFACTURING SCIENCE AND ENGINEERING, PTS 1-4, 2013, 712-715 : 74 - 77
  • [38] The effect of cementite size and morphology on the abrasive wear behavior of UHC steel
    Ozdemir, Niyazi
    Sarsilmaz, Furkan
    Orhan, Nuri
    JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2008, 130 (02): : 1 - 5
  • [39] Abrasive wear behavior of a pearlitic (0.4%C) steel microalloyed with vanadium
    Katsuki, Futoshi
    Watari, Kouji
    Tahira, Hiroaki
    Umino, Masahide
    WEAR, 2008, 264 (3-4) : 331 - 336
  • [40] Dry Sliding and Abrasive Wear Behavior of Nanostructure Zr–W–N Coating
    V. Chauhan
    P. Dubey
    S. Verma
    R. Jayaganthan
    R. Chandra
    Transactions of the Indian Institute of Metals, 2015, 68 : 799 - 807