Effect of grain refinement on mechanical properties and sliding wear resistance of extruded Sc-free 7042 aluminum alloy

被引:38
作者
Farahani, M. Vasheghani [1 ]
Emadoddin, E. [1 ]
Emamy, M. [2 ]
Raouf, A. Honarbakhsh [1 ]
机构
[1] Semnan Univ, Fac Mat & Met, Semnan, Iran
[2] Univ Tehran, Coll Engn, Sch Met & Mat Engn, Tehran, Iran
关键词
Aluminum alloys; Grain refinement; Mechanical properties; Wear resistance; AL-ZN-MG; TENSILE PROPERTIES; CU ALLOY; HEAT-TREATMENT; BEHAVIOR; MICROSTRUCTURE; STRENGTH; COMPOSITES; ADDITIONS; ZR;
D O I
10.1016/j.matdes.2013.08.044
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present study deals with an investigation on dry sliding wear behavior of grain refined Sc-free 7042 aluminum alloy by using a pin-on-disc wear test machine. Al-5Ti-1B and Al-15Zr master alloys were used as grain refining agents. The optimum amounts of added Ti and Zr in the alloy were found to be 0.03 wt.% and 0.3 wt.%, respectively. Extrusion was carried out and T6 heat treatment ware applied for all rod specimens before testing. Significant improvement in mechanical properties was obtained with the addition of grain refiners. The worn surfaces were characterized by energy dispersive X-ray spectrometry microanalysis. Results showed that the wear resistance of unrefined alloy increased with the addition of both grain refiners. Furthermore, the worn surface studies showed a mixed type of wear mechanisms; delaminating, adhesive and abrasive which took place at higher applied load. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:361 / 367
页数:7
相关论文
共 33 条
  • [1] The effect of Al-8B grain refiner and heat treatment conditions on the microstructure, mechanical properties and dry sliding wear behavior of an Al-12Zn-3Mg-2.5Cu aluminum alloy
    Alipour, M.
    Azarbarmas, M.
    Heydari, F.
    Hoghoughi, M.
    Alidoost, M.
    Emamy, M.
    [J]. MATERIALS & DESIGN, 2012, 38 : 64 - 73
  • [2] Investigation of the effect of Al-5Ti-1B grain refiner on dry sliding wear behavior of an Al-Zn-Mg-Cu alloy formed by strain-induced melt activation process
    Alipour, Mohammad
    Aghdam, Baharak Ghorbanian
    Rahnoma, Hamid Ebrahimi
    Emamy, M.
    [J]. MATERIALS & DESIGN, 2013, 46 : 766 - 775
  • [3] Mechanical properties and wear behavior of Al-2 wt.% Cu alloy composites reinforced by B4C nanoparticles and fabricated by mechanical milling and hot extrusion
    Alizadeh, A.
    Taheri-Nassaf, E.
    [J]. MATERIALS CHARACTERIZATION, 2012, 67 : 119 - 128
  • [4] Dry sliding wear behaviour of Al-12Si-4Mg alloy with cerium addition
    Anasyida, A. S.
    Daud, A. R.
    Ghazali, M. J.
    [J]. MATERIALS & DESIGN, 2010, 31 (01) : 365 - 374
  • [5] Chaubey AK, 2008, J DEFECT DIFFUS FORU, V279, P97
  • [6] CROSSLEY FA, 1951, T AM I MIN MET ENG, V191, P1143
  • [7] Sliding wear and friction behaviour of Al-18% Si-0.5% Mg alloy
    Dwivedi, DK
    Arjun, TS
    Thakur, P
    Vaidya, H
    Singh, K
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2004, 152 (03) : 323 - 328
  • [8] The microstructure, hardness and tensile properties of a new super high strength aluminum alloy with Zr addition
    Ebrahimi, S. H. Seyed
    Emamy, M.
    Pourkia, N.
    Lashgari, H. R.
    [J]. MATERIALS & DESIGN, 2010, 31 (09) : 4450 - 4456
  • [9] Effects of Al-5Ti-1B and Al-5Zr master alloys on the structure, hardness and tensile properties of a highly alloyed aluminum alloy
    Ebrahimi, S. H. Seyed
    Emamy, M.
    [J]. MATERIALS & DESIGN, 2010, 31 (01) : 200 - 209
  • [10] The microstructural evolution of an Al-Zn-Mg-Cu alloy during homogenization
    Fan, XG
    Jiang, DM
    Meng, QC
    Zhong, L
    [J]. MATERIALS LETTERS, 2006, 60 (12) : 1475 - 1479