Effect of Non-Thermal Atmospheric Pressure Plasma (NTP) and Zirconia Primer Treatment on Shear Bond Strength between Y-TZP and Resin Cement

被引:23
|
作者
Ahn, Jong-Ju [1 ]
Kim, Dae-Sung [1 ]
Bae, Eun-Bin [1 ]
Kim, Gyoo-Cheon [2 ,3 ]
Jeong, Chang-Mo [1 ]
Huh, Jung-Bo [1 ]
Lee, So-Hyoun [1 ]
机构
[1] Pusan Natl Univ, Dent Res Inst, Dent & Life Sci Inst, Dept Prosthodont, Yangsan 50612, South Korea
[2] Pusan Natl Univ, Sch Dent, Dept Oral Anat & Cell Biol, Yangsan 50612, South Korea
[3] FEAGLE Corp, Res & Dev Ctr, Yangsan 50614, South Korea
基金
新加坡国家研究基金会;
关键词
non-thermal atmospheric pressure plasma (NTP); yttria-stabilized tetragonal zirconia polycrystal; surface treatment; zirconia primer; sandblasting; dentistry; bonding; SURFACE CHARACTERIZATION; COMPOSITE RESIN; ADHESION; RESTORATIONS; POLYCRYSTAL; CERAMICS;
D O I
10.3390/ma13183934
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The purpose of this study was to investigate the effect of non-thermal atmospheric pressure plasma (NTP) treatment on the sandblasting of mechanical method and zirconia primer of chemical method used to increase the bond strength between zirconia and resin cement. In this study, Y-TZP was divided into 4 groups according to the surface treatment methods as follows: Zirconia primer (Pr), NTP + Zirconia primer (NTP + Pr), Sandblasting + Zirconia primer (Sb + Pr), Sandblasting + NTP + Zirconia primer (Sb + NTP + Pr). Then, two types of resin cement (G-CEM LinkAce and Rely X-U200) were used to measure the shear bond strength (SBS) and they were divided into non-thermal cycling group and thermal cycling group for aging effect. Statistical analyses were performed using the Kruskal-Wallis test and Mann-Whitney U test. The result of the surface energy (SE), there was no significant difference among the groups (p> 0.05). As a result of the SBS test, the Sb + Pr group had a significantly higher SBS value than the other groups regardless of the resin cement type (p< 0.05), and the decrease rate after thermal cycling treatment was the lowest. On the other hand, the NTP + Pr group showed significantly lower SBS values than the other groups except for the case of using Rely X-U200 (p< 0.05), and the reduction rate after thermal cycling was the highest. The Sb + NTP + Pr group did not differ significantly from the Pr group (p> 0.05). Within the limitations of two successive studies, treatment with NTP after sandblasting used for mechanical bond strength showed a positive effect on initial SBS. However, when NTP was treated before the zirconia primer used for the chemical bond strength, it showed a negative effect on SBS compared to other treatment methods, which was noticeable after the thermal cycling treatment.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Influence of Non-Thermal Atmospheric Pressure Plasma Treatment on Shear Bond Strength between Y-TZP and Self-Adhesive Resin Cement
    Kim, Dae-Sung
    Ahn, Jong-Ju
    Bae, Eun-Bin
    Kim, Gyoo-Cheon
    Jeong, Chang-Mo
    Huh, Jung-Bo
    Lee, So-Hyoun
    MATERIALS, 2019, 12 (20)
  • [2] Ceramic Primer Heat-Treatment Effect on Resin Cement/Y-TZP Bond Strength
    Silva, L. H.
    Costa, A. K. F.
    Queiroz, J. R. C.
    Bottino, M. A.
    Valandro, L. F.
    OPERATIVE DENTISTRY, 2012, 37 (06) : 634 - 640
  • [3] Effect of Argon Plasma on the Shear Bond Strength of Y-TZP Zirconia Ceramic Resin Interface
    Karakis, Duygu
    Akay, Canan
    Pat, Suat
    ECS JOURNAL OF SOLID STATE SCIENCE AND TECHNOLOGY, 2021, 10 (05)
  • [4] The effect of a zirconia primer on the shear bond strength of Y-TZP ceramic to three different core materials by using a self-adhesive resin cement
    Giti, Rashin
    Zarkari, Reza
    JOURNAL OF INDIAN PROSTHODONTIC SOCIETY, 2019, 19 (02): : 134 - 140
  • [5] Effect of thermal cycling and low pressure sandblasting on the bond strength of a self-adhesive cement to Y-TZP zirconia
    Re, Dino
    Augusti, Gabriele
    Merlati, Giuseppe
    Gianni, Aldo Bruno
    Augusti, Davide
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2015, 29 (16) : 1745 - 1757
  • [6] Effect of sandblasting and various metal primers on the shear bond strength of resin cement to Y-TZP ceramic
    Yun, Jeong-yeon
    Ha, Seung-ryong
    Lee, Jai-bong
    Kim, Sung-hun
    DENTAL MATERIALS, 2010, 26 (07) : 650 - 658
  • [7] Influence of atmospheric pressure low-temperature plasma treatment on the shear bond strength between zirconia and resin cement
    Ito, Yuki
    Okawa, Takahisa
    Fukumoto, Takahiro
    Tsurumi, Akiko
    Tatsuta, Mitsuhiro
    Fujii, Takamasa
    Tanaka, Junko
    Tanaka, Masahiro
    JOURNAL OF PROSTHODONTIC RESEARCH, 2016, 60 (04) : 289 - 293
  • [8] The effect of plasma on shear bond strength between resin cement and colored zirconia
    Park, Chan
    Yoo, Seung-Hwan
    Park, Sang-Won
    Yun, Kwi-Dug
    Ji, Min-Kyung
    Shin, Jin-Ho
    Lim, Hyun-Pil
    JOURNAL OF ADVANCED PROSTHODONTICS, 2017, 9 (02): : 118 - 123
  • [9] In vitro shear bond strength of Y-TZP ceramics to different core materials with the use of three primer/resin cement systems
    Al-Harbi, Fahad A.
    Ayad, Neveen M.
    Khan, Zahid A.
    Mahrous, Amr A.
    Morgano, Steven M.
    JOURNAL OF PROSTHETIC DENTISTRY, 2016, 115 (01): : 84 - 89
  • [10] Surface analysis and shear bond strength of zirconia on resin cements after non-thermal plasma treatment and/or primer application for metallic alloys
    Vechiato-Filho, Aljomar Jose
    Matos, Adaias Oliveira
    Landers, Richard
    Goiato, Marcelo Coelho
    Rangel, Elidiane Cipriano
    De Souza, Grace Mendonca
    Ricardo Barao, Valentim Adelino
    dos Santos, Daniela Micheline
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2017, 72 : 284 - 292