Microstructural evolution of mechanically alloyed and spark plasma sintered Ni-W alloy matrix composites

被引:5
作者
Genc, Aziz [1 ]
Kaya, Pinar [2 ]
Ayas, Erhan [2 ]
Ovecoglu, M. Lutfi [1 ]
Turan, Servet [2 ]
机构
[1] Istanbul Tech Univ, Dept Met & Mat Engn, TR-34469 Istanbul, Turkey
[2] AU, Dept Mat Sci & Engn, TR-26480 Eskisehir, Turkey
关键词
Ni-W alloys; Mechanical alloying; Spark plasma sintering; Transmission electron microscopy; SOLID-SOLUTION ALLOYS; HEAT-TREATMENT; POWDER-METALLURGY; NICKEL-TUNGSTEN; AMORPHIZATION; HARDNESS; FABRICATION; KINETICS; BEHAVIOR; FIELD;
D O I
10.1016/j.jallcom.2013.03.238
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Microstructural evolution of Ni(W) solid solution alloys fabricated via mechanical alloying (MA) of Ni - 30 wt.% W powders and spark plasma sintering (SPS) at 1000 degrees C for 3 min were presented in this study. Due to contaminations during MA, fabricated alloys are termed as Ni(W) solid solution alloy matrix composites. Effects of modifications on the processing conditions such as covering the graphite dies with hexagonal boron nitride spray and/or annealing of the as-MA'd powders on the microstructure of the SPS'ed Ni(W) alloy matrix composites were investigated via analytical transmission electron microscopy (TEM) studies. X-ray diffraction (XRD) and/or TEM investigations revealed that all the samples comprise Ni(W), WC and WO2 phases. A slightly reduced amount of 13.24 wt.% WC by covering the graphite dies, significantly reduced to 3.90 wt.% with the annealing of the MA'd powders. It is found that covering the graphite dies has led significant grain growth, whereas annealing of the powders had no significant effect on the grain size of SPS'ed samples. A 96.7% relative density value was increased to 97.3% with the covering of graphite dies, which further increased to 99.4% for the sample fabricated via SPS of the annealed powders with covered graphite dies. Although the amount of WC is decreased, a microhardness value of 4.28 GPa for the sample fabricated via SPS of as-MA'd powders, slightly increased to 4.35 GPa for the samples sintered by spray covered graphite dies, which further increased to 4.52 GPa with the applied annealing, revealing the enhancement of the microhardness values by increased W solubility in Ni lattices. (C) 2013 Elsevier B. V. All rights reserved.
引用
收藏
页码:159 / 167
页数:9
相关论文
共 41 条
  • [11] Amorphization and crystallization behaviors of glassy Zr70Pd30 alloys prepared by different techniques
    El-Eskandarany, MS
    Saida, J
    Inoue, A
    [J]. ACTA MATERIALIA, 2002, 50 (10) : 2725 - 2736
  • [12] Kinetics and formation mechanism of amorphous Fe52Nb48 alloy powder fabricated by mechanical alloying
    El-Eskandarany, MS
    Bahgat, AA
    Gomaa, NS
    Eissa, NA
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 1999, 290 (1-2) : 181 - 190
  • [13] Synthesis and characterization of nickel tungsten alloys by electrodeposition
    Eliaz, N
    Sridhar, TM
    Gileadi, E
    [J]. ELECTROCHIMICA ACTA, 2005, 50 (14) : 2893 - 2904
  • [14] Decarburization of TiC in Ni activated sintered W-xTiC (x=0, 5, 10, 15 wt%) composites and the effects of heat treatment on the microstructural and physical properties
    Genc, A.
    Coskun, S.
    Ovecoglu, M. L.
    [J]. INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2010, 28 (03) : 451 - 458
  • [15] Genc A., 2012, METALS MAT IN PRESS
  • [16] Fabrication of in situ Ni(W)-WC nano composites via mechanical alloying and spark plasma sintering
    Genc, Aziz
    Ayas, Erhan
    Ovecoglu, M. Lutfi
    Turan, Servet
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 542 : 97 - 104
  • [17] Fabrication and characterization of Ni-W solid solution alloys via mechanical alloying and pressureless sintering
    Genc, Aziz
    Ovecoglu, M. Lutfi
    Baydogan, Murat
    Turan, Servet
    [J]. MATERIALS & DESIGN, 2012, 42 : 495 - 504
  • [18] Characterization investigations during mechanical alloying and sintering of Ni-W solid solution alloys dispersed with WC and Y2O3 particles
    Genc, Aziz
    Ovecoglu, M. Lutfi
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 508 (01) : 162 - 171
  • [19] Microstructure and mechanical behavior of ultrafine-grained Ni processed by different powder metallurgy methods
    Gubicza, J.
    Bui, H-Q
    Fellah, F.
    Dirras, G. F.
    [J]. JOURNAL OF MATERIALS RESEARCH, 2009, 24 (01) : 217 - 226
  • [20] Elevated temperature deformation behavior of spark plasma sintered nanometric nickel with varied grain size distributions
    Holland, T. B.
    Ovid'ko, I. A.
    Wang, H.
    Mukherjee, A. K.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 528 (02): : 663 - 671