Effect of specimen thickness on the creep response of a Ni-based single-crystal superalloy

被引:109
作者
Srivastava, A. [1 ]
Gopagoni, S. [1 ]
Needleman, A. [1 ]
Seetharaman, V. [2 ]
Staroselsky, A. [2 ]
Banerjee, R. [1 ]
机构
[1] Univ N Texas, Dept Mat Sci & Engn, Denton, TX 76203 USA
[2] Pratt & Whitney, E Hartford, CT 06108 USA
关键词
Creep; Creep damage; Nickel-based single-crystal superalloys; Oxidation; Dynamic recrystallization; HIGH-TEMPERATURE; SURFACE RECRYSTALLIZATION; MECHANICAL-PROPERTIES; PLASTICITY; DEFORMATION; SIMULATIONS; DIMENSIONS; STRENGTH; POROSITY; HARDNESS;
D O I
10.1016/j.actamat.2012.06.043
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Creep tests on Ni-based single-crystal superalloy sheet specimens typically show greater creep strain rates and/or reduced strain or time to creep rupture for thinner specimens than predicted by current theories, which predict a size-independent creep strain rate and creep rupture strain. This size-dependent creep response is termed the thickness debit effect. To investigate the mechanism of the thickness debit effect, isothermal, constant nominal stress creep tests were performed on uncoated PWA1484 Ni-based single-crystal superalloy sheet specimens of thicknesses 3.18 and 0.51 mm under two test conditions: 760 degrees C/758 MPa and 982 degrees C/248 MPa. The specimens contained initial microvoids formed during the solidification and homogenization processes. The dependence of the creep response on specimen thickness differed under the two test conditions: at 760 degrees C/758 MPa there was a reduction in the creep strain and the time to rupture with decreasing section thickness, whereas at 982 degrees C/248 MPa a decreased thickness resulted in an increased creep rate even at low strain levels and a decreased time to rupture but with no systematic dependence of the creep strain to rupture on specimen thickness. For the specimens tested at 760 degrees C/758 MPa microscopic analyses revealed that the thick specimens exhibited a mixed failure mode of void growth and cleavage-like fracture while the predominant failure mode for the thin specimens was cleavage-like fracture. The creep specimens tested at 982 degrees C/248 MPa in air showed the development of surface oxides and a near-surface precipitate-free zone. Finite-element analysis revealed that the presence of the alumina layer at the free surface imposes a constraint that locally increases the stress triaxiality and changes the value of the Lode parameter (a measure of the third stress invariant). The surface cracks formed in the oxide scale were arrested by further oxidation; for a thickness of 3.18 mm the failure mode was void nucleation, growth and coalescence, whereas for a thickness of 0.51 mm there was a mixed mode of ductile and cleavage-like fracture. (c) 2012 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:5697 / 5711
页数:15
相关论文
共 50 条
  • [21] The Effect of Cooling Rate from Solution Treatment on γ′ Reprecipitates and Creep Behaviors of a Ni-Based Superalloy Single-Crystal Casting
    Huang, Jiapeng
    Ai, Cheng
    Ru, Yi
    Shang, Yong
    Pei, Yanling
    Li, Shusuo
    Gong, Shengkai
    Zhang, Heng
    CRYSTALS, 2022, 12 (09)
  • [22] Thickness debit effect in Ni-based single crystal superalloys at different stress levels
    Yu, Z. Y.
    Wang, X. M.
    Liang, H.
    Li, Z. X.
    Li, L.
    Yue, Z. F.
    INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2020, 170 (170)
  • [23] Effect of rhenium addition on isothermal oxidation behavior of single-crystal Ni-based superalloy
    Huang, L.
    Sun, X. F.
    Guan, H. R.
    Hu, Z. Q.
    SURFACE & COATINGS TECHNOLOGY, 2006, 200 (24) : 6863 - 6870
  • [24] Thickness Debit Effect in Creep Performance of a Ni3Al-Based Single-Crystal Superalloy with [001] Orientation
    Zhang, Shuangqi
    Ma, Guoquan
    Wang, Haibo
    Guo, Wenqi
    Zhao, Haigen
    Shang, Yong
    Pei, Yanling
    Li, Shusuo
    Gong, Shengkai
    CRYSTALS, 2023, 13 (02)
  • [25] Study on oxidation-creep behavior of a Ni-based single crystal superalloy based on crystal plasticity theory
    Pei, Haiqing
    Yang, Yizhe
    Gu, Shuning
    Zhao, Yanchao
    Yao, Xiaohu
    Wen, Zhixun
    Yue, Zhufeng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 839
  • [26] Effect of thermal exposure on the microstructure and creep properties of a fourth-generation Ni-based single crystal superalloy
    Huang, Yeshun
    Wang, Xinguang
    Cui, Chuanyong
    Tan, Zihao
    Li, Jinguo
    Yang, Yanhong
    Liu, Jinlai
    Zhou, Yizhou
    Sun, Xiaofeng
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 69 (69): : 180 - 187
  • [27] Microstructure Evolution and Dislocation Mechanism of a Third-Generation Single-Crystal Ni-Based Superalloy during Creep at 1170 ?C
    Xu, Ruida
    Li, Ying
    Yu, Huichen
    MATERIALS, 2023, 16 (14)
  • [28] Effect of Surface Treatment and Crystal Orientation on Microstructural Changes in Aluminized Ni-Based Single-Crystal Superalloy
    Kasai, Kazuki
    Murakami, Hideyuki
    Kuroda, Seiji
    Imai, Hachiro
    MATERIALS TRANSACTIONS, 2011, 52 (09) : 1768 - 1772
  • [29] Effect of Surface Treatment and Crystal Orientation on Microstructural Changes in Aluminized Ni-Based Single-Crystal Superalloy
    Kasai, Kazuki
    Murakami, Hideyuki
    Kuroda, Seiji
    Imai, Hachiro
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2010, 74 (01) : 19 - 23
  • [30] The effect of heat treatment on the homogenization of CMSX-4 Single-Crystal Ni-Based Superalloy
    Paraschiv, Alexandru
    Matache, Gheorghe
    Puscasu, Cristian
    AEROSPACE EUROPE CEAS 2017 CONFERENCE, 2018, 29 : 303 - 311