In-situ nano-silica deposition and air-abrasion with Bioglass 45S5 or aluminium oxide: Effects on methacrylate bonding to yttria-tetragonal zirconia polycrystal

被引:3
作者
Darvizeh, Atanaz [1 ]
Luzi, Arlinda [1 ]
Amin, Ali Abedi [1 ]
Oliveira-Ogliari, Aline [2 ]
Ogliari, Fabricio A. [3 ]
Feitosa, Victor P. [4 ]
Garcia-Esparza, Maria Angeles [5 ]
Pascual, Agustin [6 ]
Sauro, Salvatore [1 ]
机构
[1] Univ CEU Cardenal Herrera, Fac Ciencias Salud, Dept Odontol, Valencia, Spain
[2] Univ Fed Pelotas, Dent Sch Mat Engn, Pelotas, Brazil
[3] Univ Fed Pelotas, Sch Dent, Biomat Dev & Control Ctr, Pelotas, Brazil
[4] Univ Fed Ceara, Sch Dent, Fortaleza, Ceara, Brazil
[5] Univ CEU Cardenal Herrera, Fac Ciencias Salud, Inst Ciencias Biomed, Dept Farm, Valencia, Spain
[6] Univ Valencia, Fac Med & Odontol, Valencia, Spain
关键词
Bonding; Ceramics; Bioglass; Silica-coating; Tribochemical; Yttrium-tetragonal zirconia; FIXED DENTAL PROSTHESES; ADHESIVE PERFORMANCE; RESIN CEMENTS; LUTING CEMENT; CERAMICS; STRENGTH; INTERFACE; REMOVAL;
D O I
10.1016/j.ijadhadh.2015.06.008
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
This study aimed at assessing the bonding performance after water storage (24 h/6-month) of a methacrylate-based cement applied onto Yttria-Tetragonal Zirconia Polycrystal(Y-TZP) pre-treated using an innovative in-situ silica nanoparticle deposition method and/or air-abrasion with Bioglass 45S5 (BAG) or aluminium oxide (AIO). Pre-sintered blocks of Y-TZP were coated with nano-silica using an experimental in-situ deposition method or used as received (control/silica-free). Air-abrasion was performed with AIO or BAG particles both on silica-coated and control Y-TZP specimens. All the specimens were then analysed using SEMEDX. Further specimens were treated as described above, bonded using a dual-cure resin cement system and submitted to shear bond strength test after water storage (24 h and 6 months). Fracture analysis was subsequently performed using a stereo-microscope. Uniform nano-silica deposition was achieved in the Y-TZP specimens after in-situ silica deposition treatment. However, AIO air-abrasion removed the nano-silica and roughened the Y-TZP surfaces. Conversely, BAG air-abrasion caused partial removal of the nano-silica layer and created only little retention in the control/silica-free Y-TZP specimens. The highest bond strength both at 24 h and 6-month water storage was attained with the silica-coated specimens air-abraded with BAG and with those which received no air-abrasion. AIO air-abrasion increased the bond strength (24 h) in the Y-TZP specimens compared to the control/silica-free specimens which received no air-abrasion or BAG air-abrasion. The in-situ nano-silica coating method employed in this study may be a suitable, simplified and low-cost approach to provide reliable bond strength to Y-TZP ceramics. No air-abrasion is required after insitu nano-silica deposition. However, AIO air-abrasion can create micro-retentions on the surface of silica-free Y-TZP ceramics and increases the immediate bond strength of methacrylate-based resin cements. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:32 / 39
页数:8
相关论文
共 36 条
  • [21] Pelaez J, 2012, INT J PROSTHODONT, V25, P451
  • [22] A PROSPECTIVE EVALUATION OF ZIRCONIA POSTERIOR FIXED DENTAL PROSTHESES: THREE-YEAR CLINICAL RESULTS
    Pelaez, Jesus
    Cogolludo, Pablo G.
    Serrano, Benjamin
    Lozano, Jose F. L.
    Suarez, Maria J.
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 2012, 107 (06) : 373 - 379
  • [23] Surface modification for enhanced silanation of zirconia ceramics
    Piascik, J. R.
    Swift, E. J.
    Thompson, J. Y.
    Grego, S.
    Stoner, B. R.
    [J]. DENTAL MATERIALS, 2009, 25 (09) : 1116 - 1121
  • [24] Development of a novel surface modification for improved bonding to zirconia
    Piascik, Jeffrey R.
    Wolter, Scott D.
    Stoner, Brian R.
    [J]. DENTAL MATERIALS, 2011, 27 (05) : E99 - E105
  • [25] A RETROSPECTIVE ANALYSIS OF 102 ZIRCONIA SINGLE CROWNS WITH KNIFE-EDGE MARGINS
    Poggio, Carlo E.
    Dosoli, Riccardo
    Ercoli, Carlo
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 2012, 107 (05) : 316 - 321
  • [26] Bioactive effects of a calcium/sodium phosphosilicate on the resin-dentine interface: a microtensile bond strength, scanning electron microscopy, and confocal microscopy study
    Profeta, Andrea C.
    Mannocci, Francesco
    Foxton, Richard M.
    Thompson, Ian
    Watson, Timothy F.
    Sauro, Salvatore
    [J]. EUROPEAN JOURNAL OF ORAL SCIENCES, 2012, 120 (04) : 353 - 362
  • [27] Influence of air-abrasion executed with polyacrylic acid-Bioglass 45S5 on the bonding performance of a resin-modified glass ionomer cement
    Sauro, Salvatore
    Watson, Timothy F.
    Thompson, Ian
    Toledano, Manuel
    Nucci, Cesare
    Banerjee, Avijit
    [J]. EUROPEAN JOURNAL OF ORAL SCIENCES, 2012, 120 (02) : 168 - 177
  • [28] Long-term microtensile bond strength of surface modified zirconia
    Smith, Robert L.
    Villanueva, Carlos
    Rothrock, James K.
    Garcia-Godoy, Cristina E.
    Stoner, Brian R.
    Piascik, Jeffrey R.
    Thompson, Jeffrey Y.
    [J]. DENTAL MATERIALS, 2011, 27 (08) : 779 - 785
  • [29] Adhesion/cementation to zirconia and other non-silicate ceramics: Where are we now?
    Thompson, Jeffrey Y.
    Stoner, Brian R.
    Piascik, Jeffrey R.
    Smith, Robert
    [J]. DENTAL MATERIALS, 2011, 27 (01) : 71 - 82
  • [30] Aspects of bonding between resin luting cements and glass ceramic materials
    Tian, Tian
    Tsoi, James Kit-Hon
    Matinlinna, Jukka P.
    Burrow, Michael F.
    [J]. DENTAL MATERIALS, 2014, 30 (07) : E147 - E162