Effect of air-drying dentin surfaces on dentin bond strength of a solvent-free one-step adhesive

被引:5
作者
Takai, Tomoyuki [1 ]
Hosaka, Keiichi [1 ]
Kambara, Keisuke [1 ]
Thitthaweerat, Suppason [1 ]
Matsui, Naoko [1 ]
Takahashi, Masahiro [1 ]
Kishikawa, Ryuzo [1 ]
Nakajima, Masatoshi [1 ]
Otsuki, Masayuki [1 ]
Foxton, Richard M. [2 ,3 ,4 ]
Tagami, Junji [5 ]
机构
[1] Tokyo Med & Dent Univ, Oral Restitut Dept, Grad Sch Med & Dent Sci, Bunkyo Ku, Tokyo 1138549, Japan
[2] Kings Coll London, Dept Conservat Dent, Inst Dent, Guys Hosp, London SE1 9RT, England
[3] Kings Coll London, Dept Conservat Dent, Inst Dent, Kings Hosp, London SE1 9RT, England
[4] Kings Coll London, Dept Conservat Dent, Inst Dent, St Thomas Hosp, London SE1 9RT, England
[5] Tokyo Med & Dent Univ, Global Ctr Excellence Program, Int Res Ctr Mol Sci Tooth & Bone Dis, Tokyo 1138549, Japan
关键词
Solvent-free; One-step self-etch adhesive; Microtensile bond strength; Dentin bonding; Air-drying; SELF-ETCH ADHESIVES; MECHANICAL-PROPERTIES; OVERWET PHENOMENON; WATER SORPTION; SINGLE-STEP; EVAPORATION; HEMA; MOISTURE; SYSTEMS; LAYER;
D O I
10.4012/dmj.2012-034
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The purpose was to evaluate the effect of air-drying dentin surfaces on the microtensile bond strength (mu TBS) of a solvent-free onestep adhesive (Bond 1 SF). Twelve human molars were ground with 600-grit SiC paper. Before applying bonding agent, the dentin surface was rinsed with distilled water and blot-dried with tissue paper, followed by air-drying for 0, 3, 30, and 60 s using with a dental air syringe. After applying and curing Bond 1 SF, resin composite was incrementally built up. Specimens were then stored in distilled water for 24 h and then mu TBSs were measured at a cross-head speed of 1 mm/min. Higher mu TBS were observed when the dentin surface was air-dried for 3 s (33.2 +/- 6.8MPa)>0 s (26.7 +/- 4.5MPa)>30 s (22.6 +/- 5.5MPa)=60 s (20.4 +/- 5.0MPa). The results suggested that prolonged air-drying of the dentin surface removed water and decreased the bond strengths of Bond 1 SF.
引用
收藏
页码:558 / 563
页数:6
相关论文
共 38 条
[1]   Degree of conversion and permeability of dental adhesives [J].
Cadenaro, M ;
Antoniolli, F ;
Sauro, S ;
Tay, FR ;
Di Lenarda, R ;
Prati, C ;
Biasotto, M ;
Contardo, L ;
Breschi, L .
EUROPEAN JOURNAL OF ORAL SCIENCES, 2005, 113 (06) :525-530
[2]   Effects of residual ethanol on the rate and degree of conversion of five experimental resins [J].
Cadenaro, Milena ;
Breschi, Lorenzo ;
Rueggeberg, Frederick A. ;
Suchko, Michael ;
Grodin, Evan ;
Agee, Kelli ;
Di Lenarda, Roberto ;
Tay, Franklin R. ;
Pashley, David H. .
DENTAL MATERIALS, 2009, 25 (05) :621-628
[3]  
Carrilho MRO, 2005, AM J DENT, V18, P315
[4]  
Carvalho RM, 2004, J ADHES DENT, V6, P13
[5]   Water movement in the hybrid layer after different dentin treatments [J].
Chersoni, S ;
Suppa, P ;
Breschi, L ;
Ferrari, M ;
Tay, FR ;
Pashley, DH ;
Prati, C .
DENTAL MATERIALS, 2004, 20 (09) :796-803
[6]   Bonding of an auto-adhesive luting material to enamel and dentin [J].
De Munck, J ;
Vargas, M ;
Van Landuyt, K ;
Hikita, K ;
Lambrechts, P ;
Van Meerbeek, B .
DENTAL MATERIALS, 2004, 20 (10) :963-971
[7]   Characterisation of resin-dentine interfaces by compressive cyclic loading [J].
Frankenberger, R ;
Pashley, DH ;
Reich, SM ;
Lohbauer, U ;
Petschelt, A ;
Tay, FR .
BIOMATERIALS, 2005, 26 (14) :2043-2052
[8]   Self-etch vs etch-and-rinse adhesives: effect of thermo-mechanical fatigue loading on marginal quality of bonded resin composite restorations [J].
Frankenberger, R ;
Tay, FR .
DENTAL MATERIALS, 2005, 21 (05) :397-412
[9]   Influence of drying time and temperature on bond strength of contemporary adhesives to dentine [J].
Garcia, Fernanda C. P. ;
Almeida, Julio C. F. ;
Osorio, Raquel ;
Carvalho, Ricardo M. ;
Toledano, Manuel .
JOURNAL OF DENTISTRY, 2009, 37 (04) :315-320
[10]  
Hosaka K, 2007, J ADHES DENT, V9, P437