摘要
The creep of commercially pure polycrystalline metals under constant stress has four stages: a virtually instantaneous extension, decelerating Andrade beta creep, almost steady-state Andrade kappa creep, and an acceleration towards failure. Little is known about the first stage, and the fourth stage has been extensively reviewed elsewhere. The limited experimental evidence on the physical mechanism of the second stage is reviewed and a critical discussion is given of various theories of this stage. The dependence of strain rate on stress in the third, steady-state, period seems to fall into two regimes, a power law with an exponent of about 4-5, and a rather closely exponential law. The limits of the parameters within which a simple theory of the exponential dependence can be expected to be valid are discussed, and found to be compatible with experiments. Theories of the power-law dependence are discussed, and, appear to be unconvincing. The theoretical models do not relate closely to the metallographic and other physical observations. In view of the weakness of theory, experiments which may indicate the physical processes dominant in steady-state creep are reviewed. It is usually not clear whether they pertain to the power-law or the exponential regime. While the theories all assume that most of the deformation occurs homogeneously within the grains, most experimental observations point strongly to a large deformation at or close to the grain boundaries. However, a detailed study of dislocation processes in a single grain of polycrystalline foil strained in the electron microscope shows that most of the observed strain can be accounted for by the motion of single dislocations through the subgrain structure. There is no clear reconciliation of these two sets of observations. Grain-boundary sliding cannot occur without intragranular deformation. One or other process may dominate the overall deformation; the geometrically dominant process may not be the rate-controlling one. (c) 2005 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:263 / 295
页数:33
相关论文
共 113 条
[1]   MEASUREMENT OF INTERNAL STRESSES DURING CREEP OF AL AND AL-MG ALLOYS [J].
AHLQUIST, CN ;
NIX, WD .
ACTA METALLURGICA, 1971, 19 (04) :373-&
[2]   A PHENOMENOLOGICAL THEORY OF STEADY STATE CREEP BASED ON AVERAGE INTERNAL AND EFFECTIVE STRESSES [J].
AHLQUIST, CN ;
GASCANER.R ;
NIX, WD .
ACTA METALLURGICA, 1970, 18 (06) :663-&
[3]  
Andrade END, 1932, P R SOC LOND A-CONTA, V138, P348
[4]  
ANDRADE END, 1952, J IRON STEEL I, V171, P217
[5]  
Andrade END, 1910, P R SOC LOND A-CONTA, V84, P1
[6]  
ANDRADE END, 1960, PROC R SOC LON SER-A, V254, P291
[7]  
ANDRADE END, 1956, P ROY SOC A, V213, P3
[8]   Microstructure evolution of AISI 316L in torsion at high temperature [J].
Angella, G ;
Wynne, BP ;
Rainforth, WM ;
Beynon, JH .
ACTA MATERIALIA, 2005, 53 (05) :1263-1275
[9]  
[Anonymous], 1996, PHYS METALLURGY, DOI DOI 10.1016/B978-044489875-3/50012-0
[10]  
[Anonymous], 1946, J W SCOTL IRON STEEL