A method for obtaining titanium dioxide (TiO2) nanoparticles by laser ablation has been developed. Pulsed laser irradiation at an intensity of 10(9) W/m(2) leads to sputtering of titanium dioxide in the form of particles with dimensions within 10-50 nm. The phase composition and morphology of obtained nanoparticles have been studied by the methods of transmission electron microscopy and X-ray diffraction. Thermal annealing above 600A degrees C leads to an increase in the average particle size and induces the structural transition of titanium dioxide from anatase to rutile modification. Quantitative dependences of the particle size and phase composition on the annealing temperature are established. It is established that, using the laser ablation method, it is possible to obtain the anatase phase of TiO2 with increased thermal stability.
引用
收藏
页码:328 / 331
页数:4
相关论文
共 12 条
[1]   Small size TiO2 nanoparticles prepared by laser ablation in water [J].
Barreca, F. ;
Acacia, N. ;
Barletta, E. ;
Spadaro, D. ;
Curro, G. ;
Neri, F. .
APPLIED SURFACE SCIENCE, 2010, 256 (21) :6408-6412
[2]   Neodymium ion dopant effects on the phase transformation in sol-gel derived titania nanostructures [J].
Burns, A ;
Hayes, G ;
Li, W ;
Hirvonen, J ;
Demaree, JD ;
Shah, SI .
MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2004, 111 (2-3) :150-155
[3]   Titanium dioxide nanomaterials: Synthesis, properties, modifications, and applications [J].
Chen, Xiaobo ;
Mao, Samuel S. .
CHEMICAL REVIEWS, 2007, 107 (07) :2891-2959
[4]  
Karlak R. F., 1966, ANAL CHEM, V38, P183
[5]   Preparation of F-doped titania nanoparticles with a highly thermally stable anatase phase by alcoholysis of TiCl4 [J].
Lv, Yingying ;
Yu, Leshu ;
Huang, Heyong ;
Liu, Hailong ;
Feng, Yuying .
APPLIED SURFACE SCIENCE, 2009, 255 (23) :9548-9552
[6]   Photocatalytic degradation of methylene blue with metal-doped mesoporous titania under irradiation of white light [J].
Miyake, Y ;
Tada, H .
JOURNAL OF CHEMICAL ENGINEERING OF JAPAN, 2004, 37 (05) :630-635
[7]   Dispersion of Zirconium Dioxide by Pulsed Laser Radiation [J].
Pugachevskii, M. A. ;
Zavodinskii, V. G. ;
Kuz'menko, A. P. .
TECHNICAL PHYSICS, 2011, 56 (02) :254-258
[8]   Preparation of a highly thermally stable titania anatase phase by addition of mixed zirconia and silica dopants [J].
Reidy, DJ ;
Holmes, JD ;
Morris, MA .
CERAMICS INTERNATIONAL, 2006, 32 (03) :235-239
[9]   Anatase TiO2 single crystals with a large percentage of reactive facets [J].
Yang, Hua Gui ;
Sun, Cheng Hua ;
Qiao, Shi Zhang ;
Zou, Jin ;
Liu, Gang ;
Smith, Sean Campbell ;
Cheng, Hui Ming ;
Lu, Gao Qing .
NATURE, 2008, 453 (7195) :638-U4
[10]   Electronic structure and the optical and photocatalytic properties of anatase doped with vanadium and carbon [J].
Zainullina, V. M. ;
Zhukov, V. P. ;
Krasil'nikov, V. N. ;
Yanchenko, M. Yu. ;
Buldakova, L. Yu. ;
Polyakov, E. V. .
PHYSICS OF THE SOLID STATE, 2010, 52 (02) :271-280