Low-temperature sintering and properties of (Pb, Ba, Sr)(Zr, Ti, Sb)O3 piezoelectric ceramics using sintering aids

被引:44
作者
Hayashi, T [1 ]
Inoue, T
Akiyama, Y
机构
[1] Shonan Inst Technol, Kanagawa 2518511, Japan
[2] RICOH Co Ltd, R&D Ctr, Tuzuki Ku, Yokohama, Kanagawa 2240035, Japan
来源
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS | 1999年 / 38卷 / 9B期
关键词
low-temperature sintering; sintering aid; piezoelectric ceramic; actuator;
D O I
10.1143/JJAP.38.5549
中图分类号
O59 [应用物理学];
学科分类号
摘要
Low-temperature sintering of (Pb0.86Ba0.04Sr0.12)(Zr0.56Ti0.44Sb0.02)O-3 (PBSZT) powders was investigated using Pb5Ge3O11 (PGO) or LiBiO2 (LBiO) as sintering aids. 1 wt% PGO or 1 wt% LBiO-added PBSZT powders could be densified into sintered bodies at 800 degrees C for 2 h with a relative density of approximately 96%. The addition of PGO or LBiO significantly improved the sinterability of PBSZT powders, resulting in a reduction of sintering temperature by about 200 degrees C. Dielectric and piezoelectric properties of LBiO-added PBSZT ceramics were superior to those fabricated without sintering aids. However. the addition of PGO was not effective in improving the dielectric and piezoelectric properties. This may be attributable to the microstructural change involving the solid solution reaction between the PBSZT matrix and the PGO additive. The 1 wt% LBiO-added PBSZT bodies sintered at 1000 degrees C exhibited a dielectric constant of 2600, remanent polarization of 14.7 mu C/cm(2), and longitudinal strain of 0.24%.