Preparation of Al2O3/SiC nanocomposites with in-situ formed SiC

被引:0
作者
Hopf, J
Asian, M
Schmidt, H
机构
[1] Leibniz Inst Neue Mat Gem GmbH, D-66123 Saarbrucken, Germany
[2] Univ Saarland, Lehrstuhl Neue Mat, D-66125 Saarbrucken, Germany
来源
CFI-CERAMIC FORUM INTERNATIONAL | 2006年 / 83卷 / 04期
关键词
Al2O3; SiC; nanocomposites; mechanical properties; in situ formation;
D O I
暂无
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Powder mixtures containing Al2O3, SiO2 and carbon black were calcined at 1625 degrees C to form nanoscaled SiC within Al2O3 by means of the carbothermal reduction of SiO2. The prepared powders contained 5 and 10 Vol. % SiC. These powders were densified by hot pressing, and composite ceramics with densities up to 99 % obtained. Microstructural analyses of the hot-pressed composites showed a homogeneous distribution of SiC particles with a particle size mainly under 100 nm. The fracture mode was intragranular. The fracture toughness determined by the ICL method using the Niihara approach for Palmqvist cracks was in the range of 5 MPa.m(0.5). The fracture strength determined in a four-point bending test was around 540 MPa for the hot-pressed samples and around 630 MPa for the hot-pressed and postannealed samples.
引用
收藏
页码:E39 / E44
页数:6
相关论文
共 50 条
[31]   Al2O3 coating for densification of SiC ceramics and sintering kinetics [J].
Luo, Yang ;
Wu, Yinghong ;
Xiao, Dezhi ;
Tang, Kaiwei ;
Huang, Chao ;
Fu, Ricky K. Y. ;
Zheng, Shili ;
Chu, Paul K. .
SURFACE & COATINGS TECHNOLOGY, 2019, 374 :603-609
[32]   Influence of the SiC grain size on the wear behaviour of Al2O3/SiC composites [J].
Belmonte, M ;
Nieto, MI ;
Osendi, MI ;
Miranzo, P .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2006, 26 (07) :1273-1279
[33]   Mechanical and corrosion behaviours of Al/SiC and Al/Al2O3 metal matrix nanocomposites fabricated using powder metallurgy route [J].
Mahmoud, T. S. ;
El-Kady, E. Y. ;
Al-Shihri, A. .
CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2012, 47 (01) :45-53
[34]   Effects of Y2O3 additives and powder purity on the densification and grain boundary composition of Al2O3/SiC nanocomposites [J].
Shapiro, I. P. ;
Todd, R. I. ;
Titchmarsh, J. M. ;
Roberts, S. G. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2009, 29 (09) :1613-1624
[35]   Thermal microstress measurements in Al2O3/SiC nanocomposites by Cr3+ fluorescence microscopy [J].
Merino, JLO ;
Todd, RI .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2003, 23 (11) :1779-1783
[36]   Preparation and properties of nano-SiC strengthening Al2O3 composite ceramics [J].
Shi, Xiaolei ;
Dong, Yali ;
Xu, Fumin ;
Tan, Yi ;
Wang, Lai ;
Yang, Jenn-ming .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (06) :2246-2249
[37]   Preparation of β-SiC/Al2O3 composite from kaolinite gangue by carbothermal reduction [J].
Han, BQ ;
Li, N .
CERAMICS INTERNATIONAL, 2005, 31 (02) :227-231
[38]   Thermal behavior, electrical conductivity and microstructure of hot pressed Al2O3/SiC nanocomposites [J].
Parchoviansky, M. ;
Galusek, D. ;
Svancarek, P. ;
Sedlacek, J. ;
Sajgalik, P. .
CERAMICS INTERNATIONAL, 2014, 40 (09) :14421-14429
[39]   Toughness enhancement in graphene nanoplatelet/SiC reinforced Al2O3 ceramic hybrid nanocomposites [J].
Ahmad, Iftikhar ;
Islam, Mohammad ;
Subhani, Tayyab ;
Zhu, Yanqiu .
NANOTECHNOLOGY, 2016, 27 (42)
[40]   Investigation of preparation and properties of Ti3SiC2/Al2O3 multilayered composites [J].
Chen, Yingying ;
Ma, Deli ;
Li, Qinggang ;
Ji, Jun ;
Zhang, Zhenyu ;
Du, Yuhang ;
Chen, Sique ;
Yang, Hailing ;
Wei, Yulin ;
Shi, Guopu ;
Pan, Baocai ;
Wu, Junyan ;
Wang, Zhi .
INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2023, 20 (02) :1248-1259