Correlation of processing parameters and ageing with the phase morphology of styrene-butadiene-styrene block co-polymer modified bitumen

被引:14
|
作者
Kaya, Derya [1 ]
Topal, Ali [1 ]
McNally, Tony [2 ]
机构
[1] Dokuz Eylul Univ, Fac Engn, Dept Civil Engn, TR-35160 Izmir, Turkey
[2] Univ Warwick, IINM, WMG, Coventry CV4 7AL, W Midlands, England
关键词
morphology; aging; optical microscopy; confocal laser scanning microscopy; SBS modified bitumen; RHEOLOGICAL PROPERTIES; MODIFIED ASPHALT; STORAGE STABILITY; VISCOELASTIC BEHAVIOR; SBS; BLENDS; MICROSTRUCTURE; EVOLUTION; EVA;
D O I
10.1088/2053-1591/ab349c
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The morphology development of styrene-butadiene-styrene (SBS) block copolymer modified bitumen as a function of processing parameters was investigated using a combination of optical (OM) and confocal laser scanning microscopy (CLSM). The homogeneity of blends of SBS and bitumen increased with increasing mixing time, where the application of higher shear rates enhances the dispersion and distribution of the SBS phase in the bitumen matrix. For higher shear rates, SBS was swollen between 6 and 8 times that of its initial volume and shear rate is more influential than mixing time in achieving a highly dispersed SBS phase in bitumen. The bitumen components having fluorescence properties (i.e. saturates and aromatics) were homogenously dispersed in the bitumen phase, confirmed by highly uniform fluorescence intensity 3D colour maps (CLSM). The fluorescence intensity of the SBS modified bitumen samples was much more variable with regions of high and low intensity due to inhomogeneous dispersion of the polymer in the bitumen and, the absorption of the fluorescence components of the bitumen by the PS and PB phases of SBS. For longer mixing times the SBS modified bitumen aged, observed from a decrease in fluorescence intensity. Long term in-service aging of the SBS modified bitumen blends, simulated using a pressure aging vessel, resulted in a decrease in fluorescence intensity. Only the sample prepared at the lowest shear rate (1000 rpm) and shortest mixing time (15 min) displayed variable intensity in the 3D colour maps as the SBS copolymer was poorly mixed in the bitumen phase.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Influence of morphology on high-temperature rheological properties of bitumen modified with styrene-butadiene-styrene (SBS) copolymer
    Zhu, Jiqing
    Lu, Xiaohu
    FRONTIERS OF STRUCTURAL AND CIVIL ENGINEERING, 2021, 15 (03) : 806 - 819
  • [22] Compatibilization of styrene-butadiene-styrene block copolymer in polypropylene/polystyrene blends by analysis of phase morphology
    Li, Yun-yan
    Wang, Ya
    Li, Wei-qing
    Sheng, Jing
    JOURNAL OF APPLIED POLYMER SCIENCE, 2007, 103 (01) : 365 - 370
  • [23] The Influence of Emulsifier Type on Conventional Properties, Thermal Behavior, and Microstructure of Styrene-butadiene-styrene Polymer Modified Bitumen
    Zhang, Q.
    Fan, W.
    Wang, T.
    Sunarso, J.
    Nan, G.
    PETROLEUM SCIENCE AND TECHNOLOGY, 2014, 32 (10) : 1184 - 1190
  • [24] Asphalt modified by styrene-butadiene-styrene triblock copolymer: Morphology and model
    Chen, JS
    Liao, MC
    Shiah, MS
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2002, 14 (03) : 224 - 229
  • [25] Influence of Carbon Nanotubes on Morphology of Asphalts Modified with Styrene-Butadiene-Styrene
    Wang, Peng
    Dong, Ze-jiao
    Liu, Zhi-yang
    TRANSPORTATION RESEARCH RECORD, 2017, (2632) : 130 - 139
  • [26] Damping of shear vibrations in asphalt modified with styrene-butadiene-styrene polymer
    Stastna, J
    Zanzotto, L
    Vacin, O
    ASPHALT BINDERS 2000: MATERIALS AND CONSTRUCTION, 2000, (1728): : 15 - 20
  • [27] Aging effects on the composition and thermal properties of styrene-butadiene-styrene (SBS) modified bitumen
    Kaya, Derya
    Topal, Ali
    Gupta, Jaipal
    McNally, Tony
    CONSTRUCTION AND BUILDING MATERIALS, 2020, 235 (235)
  • [28] THE MICROSTRUCTURE OF BUTADIENE UNIT IN THE CO-POLYMER OF BUTADIENE WITH STYRENE
    KOBAYASHI, E
    FURUKAWA, J
    OCHIAI, M
    TSUJIMOTO, T
    EUROPEAN POLYMER JOURNAL, 1983, 19 (10-1) : 871 - 875
  • [29] The Effect of Direct-to-Plant Styrene-Butadiene-Styrene Block Copolymer Components on Bitumen Modification
    Zhang, Wengang
    Jia, Zhirong
    Zhang, Yixia
    Hu, Kui
    Ding, Longting
    Wang, Fang
    POLYMERS, 2019, 11 (01)
  • [30] Properties of styrene-butadiene-styrene block copolymer elastomer filled and modified by lignin
    Di, Mingwei (dimingwei@126.com), 1600, Materials China (36):