Effect of an internal coating technique on tensile bond strengths of resin cements to zirconia ceramics

被引:55
作者
Kitayama, Shuzo [1 ,2 ]
Nikaido, Toru [1 ]
Maruoka, Rena [1 ]
Zhu, Lei [1 ]
Ikeda, Masaomi [3 ]
Watanabe, Akihiko [4 ]
Foxton, Richard M. [5 ,6 ,7 ]
Miura, Hiroyuki [1 ]
Tagami, Junji [1 ,2 ]
机构
[1] Tokyo Med & Dent Univ, Dept Restorat Sci, Grad Sch, Bunkyo Ku, Tokyo 1138549, Japan
[2] Tokyo Med & Dent Univ, Global Ctr Excellence Program, Int Res Ctr Mol Sci Tooth & Bone Dis, Bunkyo Ku, Tokyo 1138549, Japan
[3] Tokyo Med & Dent Univ, Fac Dent, Sch Dent Technol, Bunkyo Ku, Tokyo 1138549, Japan
[4] Tokyo Med & Dent Univ, Inst Biomat & Bioengn, Chiyoda Ku, Tokyo 1010062, Japan
[5] Kings Coll London, Dept Conservat Dent, Inst Dent, Guys Hosp, London SE1 9RT, England
[6] Kings Coll London, Dept Conservat Dent, Inst Dent, Kings Hosp, London SE1 9RT, England
[7] Kings Coll London, Dept Conservat Dent, Inst Dent, St Thomas Hosp, London SE1 9RT, England
关键词
Zirconia ceramics; Resin cement; Internal coating technique; IN-VITRO EVALUATION; LUTING CEMENTS; CONDITIONING METHODS; STABILIZED ZIRCONIA; SURFACE TREATMENTS; FLEXURAL STRENGTH; ALUMINA; RESTORATIONS; DURABILITY; ADHESION;
D O I
10.4012/dmj.28.446
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
This study was conducted to enhance the tensile bond strengths of resin cements to zirconia ceramics. Fifty-six zirconia ceramic specimens (Cercon Base) and twenty-eight silica-based ceramic specimens (GN-1., GN-1. Ceramic Block) were air-abraded using alumina. Thereafter, the zirconia ceramic specimens were divided into two subgroups of 28 each according to the surface pretreatment: no pretreatment (Zr); and the internal coating technique (INT). For INT, the surface of zirconia was coated by fusing silica-based ceramics (Cercon Ceram Kiss). Ceramic surfaces were conditioned with/without a silane coupling agent followed by bonding with one of two resin cements; Panavia F 2.0 (PF) and Superbond C&B (SB). After 24 hours storage in water, the tensile bond strengths were tested (n=7). For both PF and SB, silanization significantly improved the bond strength to GN-1 and INT (p<0.05). The INT coating followed by silanizaton demonstrated enhancement of bonding to zirconia ceramics.
引用
收藏
页码:446 / 453
页数:8
相关论文
共 48 条
[1]   Microtensile bond strength of different components of core veneered all-ceramic restorations [J].
Aboushelib, MN ;
de Jager, N ;
Kleverlaan, CJ ;
Feiler, AJ .
DENTAL MATERIALS, 2005, 21 (10) :984-991
[2]   Effect of conditioning methods on the microtensile bond strength of phosphate monomer-based cement on zirconia ceramic in dry and aged conditions [J].
Amaral, Regina ;
Ozcan, Mutlu ;
Valandro, Luiz Felipe ;
Balducci, Ivan ;
Bottino, Marco Antonio .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2008, 85B (01) :1-9
[3]   Shear bond strength of a resin cement to densely sintered high-purity alumina with various surface conditions [J].
Awliya, W ;
Oden, A ;
Yaman, P ;
Dennison, JB ;
Razzoog, ME .
ACTA ODONTOLOGICA SCANDINAVICA, 1998, 56 (01) :9-13
[4]   Marginal and internal fits of fixed dental prostheses zirconia retainers [J].
Beuer, Florian ;
Aggstaller, Hans ;
Edelhoff, Daniel ;
Gernet, Wolfgang ;
Sorensen, John .
DENTAL MATERIALS, 2009, 25 (01) :94-102
[5]  
Blatz MB, 2007, QUINTESSENCE INT, V38, P745
[6]   In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling [J].
Blatz, MB ;
Sadan, A ;
Martin, J ;
Lang, B .
JOURNAL OF PROSTHETIC DENTISTRY, 2004, 91 (04) :356-362
[7]   In vitro evaluation of long-term bonding of Procera AllCeram alumina restorations with a modified resin luting agent [J].
Blatz, MB ;
Sadan, A ;
Arch, GH ;
Lang, BR .
JOURNAL OF PROSTHETIC DENTISTRY, 2003, 89 (04) :381-387
[8]   Resin-ceramic bonding: a review of the literature [J].
Blatz, MB ;
Sadan, A ;
Kern, M .
JOURNAL OF PROSTHETIC DENTISTRY, 2003, 89 (03) :268-274
[9]  
Blatz MB, 2002, QUINTESSENCE INT, V33, P415
[10]  
Blixt M, 2000, INT J PROSTHODONT, V13, P221