Reinforcements stimulated dynamic recrystallization behavior and tensile properties of extruded (TiB + TiC + La2O3)/Ti6Al4V composites

被引:51
作者
Qiu, Peikun [1 ]
Li, Hong [2 ]
Sun, Xianglong [1 ]
Han, Yuanfei [1 ]
Huang, Guangfa [1 ]
Lu, Weijie [1 ]
Zhang, Di [1 ]
机构
[1] Shanghai Jiao Tong Univ, State Key Lab Met Matrix Composites, Shanghai 200240, Peoples R China
[2] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 70072, Peoples R China
关键词
Hot extrusion; Titanium matrix composites; Dynamic recrystallization; Tensile properties; Ti6Al4V; IN-SITU TECHNIQUE; MECHANICAL-PROPERTIES; MATRIX COMPOSITES; TIBW/TI6AL4V COMPOSITE; VOLUME FRACTION; HEAT-TREATMENT; MICROSTRUCTURE; TIB; EXTRUSION; TEMPERATURE;
D O I
10.1016/j.jallcom.2016.12.418
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
TiB, TiC and La2O3 multiple-reinforced Ti6Al4V matrix composites were successfully fabricated by common casting based on the in situ reaction of Ti, B4C, LaB6, and oxygen in the raw materials and forged subsequently. Hot extrusion was carried out on the as-forged composites to investigate its effect on microstructure and tensile properties of Ti6Al4V composites reinforced by low volume fraction of reinforcements. The microstructure showed that the TiBw and TiCp distributed homogeneously and the clustered reinforcements disappeared after hot extrusion. Besides, TiBw exhibited favorable alignment, rotating parallel to the extrusion direction and TiCp also distributed along the same direction. Moreover, the microstructure of as-extruded composites tended to formed two kind of microstructure zones: finer basket-weave zones containing few reinforcements, and equiaxial zones embedded with abundant reinforcements, which indicated that reinforcements stimulated dynamic recrystallization during hot extrusion. The tensile test results revealed that the hot extrusion can significantly improve the ductility of (TiB + TiC + La2O3)/Ti6Al4V composites accompanied by slight decrease of tensile strength, among which the 1.5 vol% (TiB + TiC + La2O3)/Ti6Al4V increased by nearly four times from 2.71% to 13.2% With ultimate strength decreasing by 8.5%. from 954 MPa to 903 MPa, compared with that of the as-forged composites. (C) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:874 / 881
页数:8
相关论文
共 40 条
  • [21] Fabrication and mechanical properties of in situ TiC/Ti metal matrix composites
    Liu Yanbin
    Liu Yong
    Tang Huiping
    Wang Bin
    Liu Bin
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (08) : 3592 - 3601
  • [22] Synthesis of a TiBw/Ti6Al4V composite by powder compact extrusion using a blended powder mixture
    Lu, Huiyang
    Zhang, Deliang
    Gabbitas, Brian
    Yang, Fei
    Matthews, Steven
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 606 : 262 - 268
  • [23] The effect of forging temperature on microstructure and mechanical properties of in situ TiC/Ti composites
    Ma, Feng-cang
    Lu, Wei-jie
    Qin, Ji-ning
    Zhang, Di
    Ji, Bo
    [J]. MATERIALS & DESIGN, 2007, 28 (04) : 1339 - 1342
  • [24] Effect of TiB Whiskers Orientation on Mechanical Properties in an In Situ TiB/Ti-1100 Composite
    Ma Feng-cang
    Liu Ping
    Li Wei
    Liu Xin-kuan
    Chen Xiao-hong
    Zhang Di
    [J]. MATERIALS TRANSACTIONS, 2010, 51 (07) : 1277 - 1280
  • [25] Processing and properties of titanium-titanium boride (TiBw) matrix composites -: a review
    Morsi, K.
    Patel, V. V.
    [J]. JOURNAL OF MATERIALS SCIENCE, 2007, 42 (06) : 2037 - 2047
  • [26] Tensile and creep properties of thermomechanically processed boron modified Timetal 834 titanium alloy
    Prasad, Kartik
    Sarkar, Rajdeep
    Ghosal, P.
    Satyanarayana, D. V. V.
    Kamat, S. V.
    Nandy, T. K.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (22-23): : 6733 - 6741
  • [27] Microstructure development and fracture of in-situ reinforced Ti-8.5Al-1B-1Si
    Rangarajan, S
    Aswath, PB
    Soboyejo, WO
    [J]. SCRIPTA MATERIALIA, 1996, 35 (02) : 239 - 245
  • [28] Producing Ti-6Al-4V/TiC composite with good ductility by vacuum induction melting furnace and hot rolling process
    Rastegari, H. A.
    Asgari, S.
    Abbasi, S. M.
    [J]. MATERIALS & DESIGN, 2011, 32 (10): : 5010 - 5014
  • [29] Microstructural effects on the mechanical behavior of B-modified Ti-6Al-4V alloys
    Sen, Indrani
    Tamirisakandala, S.
    Miracle, D. B.
    Ramamurty, U.
    [J]. ACTA MATERIALIA, 2007, 55 (15) : 4983 - 4993
  • [30] The influences of trace TiB and TiC on microstructure refinement and mechanical properties of in situ synthesized Ti matrix composite
    Sun, Shuyu
    Wang, Minmin
    Wang, Liqiang
    Qin, Jining
    Lu, Weijie
    Zhang, Di
    [J]. COMPOSITES PART B-ENGINEERING, 2012, 43 (08) : 3334 - 3337