Effect of Adhesive Resin Type for Bonding to Zirconia Using Two Surface Pretreatments
被引:19
作者:
Samimi, Pouran
[1
,2
]
Hasankhani, Amineh
[1
,2
]
Matinlinna, Jukka Pekka
[3
]
Mirmohammadi, Hesam
[1
,2
,4
,5
]
机构:
[1] Isfahan Univ Med Sci, Sch Dent, Dent Mat Res Ctr, Esfahan, Iran
[2] Isfahan Univ Med Sci, Sch Dent, Dept Operat Dent, Esfahan, Iran
[3] Univ Hong Kong, Fac Dent, Dent Mat Sci, Hong Kong, Hong Kong, Peoples R China
[4] Univ Amsterdam, Acad Ctr Dent Amsterdam, Dept Cariol Endodontol & Pedodontol, Amsterdam, Netherlands
[5] Vrije Univ Amsterdam, Amsterdam, Netherlands
关键词:
adhesive strength;
microshear bond strength;
resin composite cement;
surface treatment;
zirconia;
MDP monomer;
FINITE-ELEMENT-ANALYSIS;
LUTING CEMENTS;
OXIDE CERAMICS;
CONDITIONING METHODS;
PHOSPHATE MONOMER;
SELF-ADHESIVE;
STRENGTH;
ALUMINA;
DENTIN;
DURABILITY;
D O I:
10.3290/j.jad.a34593
中图分类号:
R78 [口腔科学];
学科分类号:
1003 ;
摘要:
Purpose: This laboratory study evaluated the short-term adhesive properties of one 10-MDP-containing and two MDP-free resin composite cements, using two types of zirconia surface pretreatments. Materials and Methods: Eighteen sintered zirconia disks (Procera, Nobel Biocare) were randomly divided into three study groups according to their surface treatment: (a) polished surface (control group); (b) airborne-particle abraded (grit blasted) with 50-mu m aluminum trioxide (APA); and (c) selective infiltration etching (SIE). The zirconia disks were then bonded to 180 pre-aged composite resin disks (0.9 mm x 0.7 mm) using three different resin composite cements (Panavia F2.0, Esthetic, and Aegis). Resin-zirconia adhesion strength was evaluated using the microshear bond strength test (mu SBS) after 24 h (baseline) and 2 weeks of storage in deionized water at 37 degrees C. Three-way ANOVA, one-way ANOVA, and Scheff's post-hoc tests were used to analyze the data (p = 0.05). Results: Surface treatments significantly influenced the mu SBS (p < 0.001). The highest mean mu SBS values were recorded with the MDP-containing resin composite cement (Panavia F2.0) in both SIE (32.4 +/- 5.3 MPa) and APA (28.6 +/- 8.8 MPa) groups. Water storage significantly reduced the bond strength obtained with the MDP-free cements (Esthetic and Aegis) and in the control group, while the bond strength in SIE and APA groups using the 10MDP-containing resin composite cement exhibited relatively unchanged values. Conclusion: SIE and APA in combination with the 10-MDP-containing resin composite cement established a strong, durable bond to zirconia substrates under short-term aging conditions. The cement containing amorphous calcium phosphate (Aegis) did not bond to zirconia surfaces. During the observation period, mu SBS decreased significantly due to hydrolytic degradation, except when the 10-MDP-containing resin composite cement (Panavia F2.0) was used in the SIE and APA groups.