Production of surface chilled ductile iron

被引:0
|
作者
Ovali, I. [1 ]
Kilicli, V. [2 ]
Erdogan, M. [2 ]
机构
[1] Pamukkale Univ, Fac Technol, Dept Mfg Engn, Denizli, Turkey
[2] Gazi Univ, Fac Technol, Dept Met & Mat Engn, Ankara, Turkey
关键词
Ductile iron; surface chilled ductile iron; carbide; chill; graphite; CAST-IRON; WEAR CHARACTERISTICS; TENSILE PROPERTIES; IMPACT PROPERTIES; HEAT-TREATMENTS; MICROSTRUCTURE; BEHAVIOR; RESISTANCE; ABRASION; LASER;
D O I
10.1002/mawe.201500442
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Surface chilled ductile iron has become a promising material for machine parts exposed the wearing and impact because of good combination of high wear resistance and toughness. In this study, the effect of the chemical composition, mold wall thickness and sample diameter on the chill formation, chill depth, and carbide precipitation in the ductile iron were studied. The casting having four different chemical compositions were carried out to copper molds having various samples diameter (empty set 10-50mm) and mold wall thickness (5, 15, 20, 30 and 50 mm). Microstructural and hardness profile evaluation were carried out from surface to center of part in order to define the effects of cooling rate on the chill formation. Experimental results showed that the production of surface chilled ductile iron having various chill depths can be achieved with controlling of the cooling rate. Hardness profile increases with increasing of mold wall thickness (cooling rate). High chromium content increases chill depth and decrease graphite formation. High silicon content promotes graphite formation while it decreases carbide precipitation. Chill formation on the ductile iron can be optimized with controlling mold wall thickness and sample diameter (cooling rate).
引用
收藏
页码:949 / 961
页数:13
相关论文
共 50 条
  • [1] Production of surface chilled ductile iron: Herstellung von oberflächengekühltem schmiedbarem Gusseisen
    Department of Manufacturing Engineering, Faculty of Technology, Pamukkale University, Denizli, Turkey
    不详
    Mater.wis. Werkstofftech., 9 (949-961): : 949 - 961
  • [2] Microstructural study and wear behavior of ductile iron surface alloyed by Inconel 617
    Jeshvaghani, R. Arabi
    Jaberzadeh, M.
    Zohdi, H.
    Shamanian, M.
    MATERIALS & DESIGN, 2014, 54 : 491 - 497
  • [3] Improvement of ductile iron wear resistance through local surface reinforcement
    Podgornik, B.
    Vizintin, J.
    Thorbjornsson, I.
    Johannesson, B.
    Thorgrimsson, J. T.
    Celis, M. Martinez
    Valle, N.
    WEAR, 2012, 274 : 267 - 273
  • [4] Microstructure evolution during surface alloying of ductile iron and austempered ductile iron by electron beam melting
    Gulzar, A.
    Akhter, J. I.
    Ahmad, M.
    Ali, G.
    Mahmood, M.
    Ajmal, M.
    APPLIED SURFACE SCIENCE, 2009, 255 (20) : 8527 - 8532
  • [5] Laser Surface Hardening of Austempered Ductile Iron (ADI)
    Zahon, Ladislav
    Kuchar, Jiri
    Hornik, Jakub
    Krcil, Jan
    Kudlacek, Jan
    COATINGS, 2024, 14 (08)
  • [6] Microstructural study of surface melted and chromium surface alloyed ductile iron
    Sohi, M. Heydarzadeh
    Ebrahimi, M.
    Ghasemi, H. M.
    Shahripour, A.
    APPLIED SURFACE SCIENCE, 2012, 258 (19) : 7348 - 7353
  • [7] Fracture toughness of austempered chilled ductile iron
    Hemanth, J
    MATERIALS & DESIGN, 1998, 19 (5-6): : 269 - 277
  • [8] Wear characteristics of austempered chilled ductile iron
    Hemanth, J
    MATERIALS & DESIGN, 2000, 21 (03) : 139 - 148
  • [9] Enhancement of wear resistance of ductile iron surface alloyed by stellite 6
    Jeshvaghani, R. Arabi
    Shamanian, M.
    Jaberzadeh, M.
    MATERIALS & DESIGN, 2011, 32 (04): : 2028 - 2033
  • [10] Production of Ductile Iron Castings with Different Matrix Structure
    Bockus, Stasys
    Zaldarys, Gintautas
    MATERIALS SCIENCE-MEDZIAGOTYRA, 2010, 16 (04): : 307 - 310