Effects of large amounts of Mg (5-13 wt%) on hot compressive deformation behavior and processing maps of Al-Mg alloys

被引:48
作者
Jeong, H. T. [1 ]
Han, S. H. [2 ]
Kim, W. J. [1 ]
机构
[1] Hongik Univ, Dept Mat Sci & Engn, Sangsu Dong 72-1, Seoul 121791, South Korea
[2] Korea Inst Mat Sci, 797 Changwondaero, Chang Won 642831, Gyeongnam, South Korea
基金
新加坡国家研究基金会;
关键词
Metals and alloys; Liquid-solid reactions; Mechanical properties; Microstructure; SOLID-SOLUTION ALLOYS; DYNAMIC RECRYSTALLIZATION; VISCOUS GLIDE; CREEP-BEHAVIOR; GRAIN-SIZE; STRESS; MECHANISMS; DUCTILITY; STRENGTH; RANGE;
D O I
10.1016/j.jallcom.2019.02.293
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effects of the addition of large amounts of Mg (5-13 wt%) on the hot compressive behavior and processing maps of Al-Mg alloys were systematically examined in a wide strain rate range between 5 x 10(-4) s(-1) and 10 s(-1) in a temperature range between 598 and 698 K. As the Mg content in the Al-Mg alloy increased from 5 to 7 wt%, the fraction of dynamically recrystallized (DRXed) grains decreased and then increased, followed by the further increase of Mg content up to 13 wt%. The Al-13Mg alloy exhibited superior post-deformation microstructures compared to the Al-Mg alloys with the lower Mg Al-Mg alloys. For example, after compressive deformation at high strain rates of 1 and 10 s(-1) at 698 K, the Al-13Mg alloy had considerably higher fractions of DRXed grains (67-98%) and much smaller average grain sizes (13-19 mm) than the fractions of DRXed grains (5e43%) and the average grain sizes (63-485 mu m) of the Al-Mg alloys with the Mg contents <= 10 wt%. The decreased fraction of DRXed grains with an increase in Mg content from 5 to 7 wt% was attributed to the suppression of dynamic recovery, resulting in a decrease in the kinetics of continuous dynamic recrystallization (CDRX). The increased fraction of DRX grains with the increase in Mg from 7 to 13 wt% could be attributed to the transition from CDRX to discontinuous dynamic recrystallization by the significant reduction in stacking fault energy with the addition of large amounts of Mg. The Al-Mg alloys exhibited the solute drag creep at low strain rates and power law breakdown (PLB) at high strain rates. With the addition of large amounts of Mg, however, the onset of PLB was delayed to a higher strain rate and a lower temperature. As a result, the Al-13Mg alloy could exhibit higher power dissipation efficiency and smaller instability regions compared to that of the lower Mg content Al-Mg alloys in the processing maps. This outcome agreed with the observations on the microstructures after compressive deformation. (c) 2019 Elsevier B.V. All rights reserved.
引用
收藏
页码:1282 / 1299
页数:18
相关论文
共 52 条
[11]   Microhardness measurements and the Hall-Petch relationship in an Al-Mg alloy with submicrometer grain size [J].
Furukawa, M ;
Horita, Z ;
Nemoto, M ;
Valiev, RZ ;
Langdon, TG .
ACTA MATERIALIA, 1996, 44 (11) :4619-4629
[12]   The prediction of hot flow behavior of Al-6%Mg alloy [J].
Gholamadeh, A. ;
Taheri, A. Karimi .
MECHANICS RESEARCH COMMUNICATIONS, 2009, 36 (02) :252-259
[13]   An experimental study of the recrystallization mechanism during hot deformation of aluminium [J].
Gourdet, S ;
Montheillet, F .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 283 (1-2) :274-288
[14]  
Hill R., 1965, PROGR SOLID MECH, V4, P93
[15]   NEW YIELDING PHENOMENON IN SOME ALUMINIUM ALLOYS AT HIGH TEMPERATURES [J].
HORIUCHI, R ;
YOSHINAG.H ;
HAMA, S .
TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1965, 6 (03) :123-&
[16]   MECHANISM OF HIGH-TEMPERATURE CREEP OF ALUMINUM-MAGNESIUM SOLID-SOLUTION ALLOYS [J].
HORIUCHI, R ;
OTSUKA, M .
TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1972, 13 (04) :284-&
[17]   A review of dynamic recrystallization phenomena in metallic materials [J].
Huang, K. ;
Loge, R. E. .
MATERIALS & DESIGN, 2016, 111 :548-574
[18]   The flow stress evolution and grain refinement mechanisms during hot deformation of Al-Mg alloy [J].
Huang, Ke ;
Loge, Roland E. .
INTERNATIONAL CONFERENCE ON THE TECHNOLOGY OF PLASTICITY, ICTP 2017, 2017, 207 :25-30
[19]   The effect of solutes on grain boundary mobility during recrystallization and grain growth in some single-phase aluminium alloys [J].
Huang, Y. ;
Humphreys, F. J. .
MATERIALS CHEMISTRY AND PHYSICS, 2012, 132 (01) :166-174
[20]   Microstructure and hot deformation behavior of AlMg6 alloy produced by equal-channel angular pressing [J].
Khalaj, Gholamreza ;
Khalaj, Mohammad Javad ;
Nazari, Ali .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 542 :15-20