Effect of Strain Hardened Inner Surface Layers on Stress Corrosion Cracking of Type 316 Stainless Steel in Simulated PWR Primary Water

被引:8
作者
Yonezawa, Toshio [1 ]
Watanabe, Masashi [1 ]
Hashimoto, Atsushi [2 ]
Olson, M. D. [3 ]
Dewald, A. T. [3 ]
Hill, M. R. [4 ]
机构
[1] Tohoku Univ, NICHe, FRI, Aoba Ku, 6-6-10 Aoba, Sendai, Miyagi 9808579, Japan
[2] Kobe Mat Testing Lab Co Ltd, 47-13 Niijima, Harima 6750155, Japan
[3] Hill Engn LLC, 3083 Gold Canal Dr, Rancho Cordova, CA USA
[4] Univ Calif Davis, Dept Mech & Aerosp Engn, One Shields Ave, Davis, CA 95616 USA
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2019年 / 50A卷 / 05期
关键词
DISSOLVED HYDROGEN; INITIATION; BEHAVIOR; GROWTH;
D O I
10.1007/s11661-019-05137-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the relationship between SCC growth rate and Vickers hardness for Type 316 stainless steel at various temperatures in simulated PWR primary water was investigated. In addition, IGSCC growth measurements were conducted using so-called functionally graded cold-rolled specimens made of Type 316 stainless steel, in simulated PWR primary water. Residual stress measurements were performed using the contour and slitting methods on the functionally graded cold-rolled specimens. The contour method measurements found highly tensile stress (350MPa) toward the surface of the side with a larger thickness reduction and low-magnitude stress elsewhere. The purpose of these latter specimens was to evaluate the effect of heavily cold-worked layers on the inner surface of components made of Type 316 stainless steel on the possibility that IGSCC could penetrate through the wall thickness. The test data showed that the work-hardened inner surface does not always have a detrimental effect on SCC susceptibility. However, if any surface cracks exist within the work-hardened inner surface layer of any components, the stress at the crack tip becomes very large and SCC easily initiates. Nevertheless, even if IGSCC initiates from a heavily cold-worked layer at the inner surface, IGSCC growth rate in Type 316 stainless steel was found to eventually become negligibly small or arrests in the soft base material. (C) The Minerals, Metals & Materials Society and ASM International 2019
引用
收藏
页码:2462 / 2485
页数:24
相关论文
共 50 条
[31]   Stress corrosion cracking in the heat affected zone of a stainless steel 308L-316L weld joint in primary water [J].
Dong, Lijin ;
Peng, Qunjia ;
Han, En-Hou ;
Ke, Wei ;
Wang, Lei .
CORROSION SCIENCE, 2016, 107 :172-181
[32]   Effect of Strain Rate on Stress Corrosion Cracking of 316L Austenitic Stainless Steel in Boiling MgCl2 Environment [J].
Hassani, A. ;
Habibolahzadeh, A. ;
Javadi, A. H. ;
Hosseini, S. M. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2013, 22 (06) :1783-1789
[33]   Corrosion and Stress Corrosion Cracking Susceptibility of Type 347H Stainless Steel in Supercritical Water [J].
Guo, Xianglong ;
Gao, Wenhua ;
Chen, Kai ;
Shen, Zhao ;
Zhang, Lefu .
CORROSION, 2018, 74 (01) :83-95
[34]   Effect of δ-ferrite on stress corrosion cracking of CF8A austenitic stainless steels in a simulated pressurised water reactor environment [J].
Xu, Youwei ;
Jing, Hongyang ;
Xu, Lianyong ;
Han, Yongdian ;
Zhao, Lei .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (06) :6420-6426
[35]   Intergranular oxidation of 316L stainless steel in the PWR primary water environment [J].
Matthews, R. P. ;
Knusten, R. D. ;
Westraadt, J. E. ;
Couvant, T. .
CORROSION SCIENCE, 2017, 125 :175-183
[36]   Mean Stress Effect on Fatigue Properties of Type 316 Stainless Steel in Pressurized Water Reactors Primary Water Environment [J].
Kamaya, Masayuki .
JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 2019, 141 (05)
[37]   Dependence of corrosion fatigue crack propagation rate of 316LN stainless steel on dissolved hydrogen concentration in simulated PWR primary circuit loop water [J].
Wu, Panpan ;
Wang, Xiujie ;
Li, Entong ;
Lu, Zhanpeng ;
Chen, Junjie ;
Cui, Tongming ;
Xu, Xinhe ;
Shoji, Tetsuo .
JOURNAL OF NUCLEAR MATERIALS, 2025, 615
[38]   Monitoring of stress corrosion cracking of duplex stainless steel by electrochemical potential noise and load signal in simulated pressurised water reactor primary water [J].
Zajec, Bojan ;
Leban, Mirjam Bajt ;
Kosec, Tadeja ;
Legat, Andraz .
CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2025, 60 (04) :307-322
[39]   On the exceptional stress corrosion cracking susceptibility of selective laser melted 316L stainless steel under the individual effect of surface residual stresses [J].
Yazdanpanah, Arshad ;
Franceschi, Mattia ;
Bergamo, Gianluca ;
Bonesso, Massimiliano ;
Dabala, Manuele .
ENGINEERING FAILURE ANALYSIS, 2022, 136
[40]   Characterization of internal and intergranular oxidation in Alloy 690 exposed to simulated PWR primary water and its implications with regard to stress corrosion cracking [J].
Lim, Yun Soo ;
Kim, Dong Jin ;
Kim, Sung Woo ;
Hwang, Seong Sik ;
Kim, Hong Pyo .
MATERIALS CHARACTERIZATION, 2019, 157