Effect of tensile stress in elastic and plastic range on hydrogen permeation of high-strength steel in sour environment

被引:68
作者
Kim, Sung Jin [1 ]
Jung, Hwan Gyo [2 ]
Kim, Kyoo Young [1 ]
机构
[1] Pohang Univ Sci & Technol POSTECH, GIFT, Pohang 790784, South Korea
[2] POSCO Tech Res Labs, Pohang 790704, South Korea
关键词
Electrochemical hydrogen permeation; Tensile stress; High-strength steel; Corrosion; Iron sulfide; INDUCED CRACKING; ATMOSPHERIC CORROSION; MICROSTRUCTURE; DEFORMATION; SUSCEPTIBILITY; TEMPERATURE; TRANSPORT; ENTRY; IRON;
D O I
10.1016/j.electacta.2012.05.147
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The new hydrogen permeation technique developed for the electrochemical permeation method makes it possible to evaluate the effect of applied tensile stress in both elastic and plastic range on hydrogen permeation behavior in high-strength steels. This study suggests that the iron sulfide film acts as sites for hydrogen reduction reaction and that the applied elastic stress weakens the stability of the sulfide film due to lots of cracks forming in the local sulfur deficient region, resulting in increase in both the anodic dissolution and hydrogen reduction reaction. In addition, the effect of applied stress in plastic range on hydrogen permeation behavior was clearly evaluated by excluding other side effects such as the reduced rate of hydrogen oxidation caused by the disruption of the Pd layer under stress. Furthermore, by evaluating hydrogen permeation behavior in the transient range from elastic to plastic stress, the effect of newly generated dislocation on the permeation current was accurately investigated without any side effect. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:139 / 146
页数:8
相关论文
共 27 条
[1]   Susceptibility of conventional pressure vessel steel to hydrogen-induced cracking and stress-oriented hydrogen-induced cracking in hydrogen sulfide-containing diglycolamine solutions [J].
Al-Anezi, MA ;
Frankel, GS ;
Agrawal, AK .
CORROSION, 1999, 55 (11) :1101-1109
[2]   Effect of bainitic microstructure on the susceptibility of pipeline steels to hydrogen induced cracking [J].
Arafin, M. A. ;
Szpunar, J. A. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (15) :4927-4940
[3]   HYDROGEN PERMEATION IN METALS AS A FUNCTION OF STRESS TEMPERATURE AND DISSOLVED HYDROGEN CONCENTRATION [J].
BECK, W ;
BOCKRIS, JOM ;
MCBREEN, J ;
NANIS, L .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL AND PHYSICAL SCIENCES, 1966, 290 (1421) :220-&
[4]  
Berkowitz B.J., 1983, P NATO ADV RES I AT
[5]   Influence of tensile straining on the permeation of hydrogen in low alloy Cr-Mo steels [J].
Brass, AM ;
Chêne, J .
CORROSION SCIENCE, 2006, 48 (02) :481-497
[6]  
Chiaberge M., 2011, HIGH MN TWIP STEELS, P101
[7]   ADSORPTION AND DIFFUSION OF ELECTROLYTIC HYDROGEIN IN PALLADIUM [J].
DEVANATHAN, MAV ;
STACHURSKI, Z .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL AND PHYSICAL SCIENCES, 1962, 270 (1340) :90-&
[8]   Impact of iron sulfide transformation on trichloroethylene degradation [J].
He, Y. Thomas ;
Wilson, John T. ;
Wilkin, Richard T. .
GEOCHIMICA ET COSMOCHIMICA ACTA, 2010, 74 (07) :2025-2039
[9]   Effect of mechanical deformation on permeation of hydrogen in iron [J].
Huang, YL ;
Nakajima, A ;
Nishikata, A ;
Tsuru, T .
ISIJ INTERNATIONAL, 2003, 43 (04) :548-554
[10]   HYDROGEN TRANSPORT IN FERRITIC STAINLESS-STEEL UNDER ELASTIC STRESS [J].
HWANG, LC ;
PERNG, TP .
MATERIALS CHEMISTRY AND PHYSICS, 1994, 36 (3-4) :231-235