Effects of steam concentration and flow rate on the high temperature oxidation of PEO-coated zirconium alloy at 1000 °C and 1200 °C

被引:3
|
作者
Guan, Haohao [1 ,2 ]
Wang, Xingping [1 ,2 ]
Xu, Chi [1 ,2 ]
Liao, Yizhao [1 ,2 ]
Gao, Chuanli [1 ,2 ]
Du, Jiancheng [1 ,2 ]
Jin, Xiaoyue [2 ]
Xue, Wenbin [1 ,2 ]
Zhang, Jinlong [3 ]
机构
[1] Beijing Normal Univ, Coll Nucl Sci & Technol, Key Lab Beam Technol, Minist Educ, Beijing 100875, Peoples R China
[2] Beijing Acad Sci & Technol, Inst Radiat Technol, Beijing 100875, Peoples R China
[3] Shanghai Univ, Inst Mat, Shanghai 200072, Peoples R China
基金
中国国家自然科学基金;
关键词
ZIRLO zirconium alloy; High-temperature steam oxidation; Plasma electrolytic oxidation; Steam flow rate; Steam concentration; ZIRCALOY-4; BEHAVIOR; OXIDE; ZR-1NB-1SN-0.1FE; ELECTROLYTE; ENVIRONMENT; RESISTANCE; MORPHOLOGY; MIXTURES; KINETICS;
D O I
10.1016/j.surfcoat.2022.128896
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A compact oxide coating of 7 mu m thick on ZIRLO zirconium alloy was fabricated by plasma electrolytic oxidation (PEO) in phosphate electrolyte. The effects of steam concentration and flow rate on the steam oxidation behavior of PEO-coated ZIRLO alloy at 1000 degrees C and 1200 degrees C were evaluated by thermogravimetric analysis (TGA). The morphologies, compositions, phase constituents before and after the steam oxidation were characterized. It is found that the critical steam concentration without steam starvation for PEO-coated ZIRLO alloy at 50 ml/min flow rate is 35 % at 1000 degrees C. Meanwhile, the critical flow rate at 50 % steam concentration is 35 ml/min at 1000 degrees C and 150 ml/min at 1200 degrees C. A dimensionless number (P = 39) is suggested corresponding to the critical steam concentration and flow rate. It means that the minimum mass of steam injection is about 39 per unit mass gain of sample, in order to avoid the steam starvation for Zr alloys after 3600 s steam exposure. The steam oxide layers consist of monoclinic zirconia (M-ZrO2) and a little tetragonal zirconia (T-ZrO2) phase at different temperatures, steam concentrations and flow rates. The hydrogen has not diffused into the steam oxide layer and ZIRLO substrate due to the hindrance of ZrO2 coating to the hydrogen diffusion.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Microstructural analysis of preformed oxides on a zirconium alloy before and after subsequent oxidation at 1000-1200 °C
    Lee, Cheol Min
    Jeong, Hu Young
    Yoon, Aram
    Mok, Yong-Kyoon
    Sohn, Dong-Seong
    CORROSION SCIENCE, 2018, 139 : 410 - 420
  • [22] High temperature steam oxidation of chromium-coated zirconium-based alloys: Kinetics and process
    Brachet, Jean-Christophe
    Rouesne, Elodie
    Ribis, Joel
    Guilbert, Thomas
    Urvoy, Stephane
    Nony, Guillaume
    Toffolon-Masclet, Caroline
    Le Saux, Matthieu
    Chaabane, Nihed
    Palancher, Herve
    David, Amandine
    Bischoff, Jeremy
    Augereau, Julien
    Pouillier, Edouard
    CORROSION SCIENCE, 2020, 167
  • [23] Oxidation mechanism and high-temperature strength of Mo-B-C-coated diamonds in the 700°C-1200 °C temperature range
    Mao, Xinyue
    Meng, Qingnan
    Wang, Sifan
    Huang, Shiyin
    Yuan, Mu
    Qiu, Yuting
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 33 : 7829 - 7841
  • [24] Microstructural evolution of intermetallic phase precipitates in Cr-coated Zirconium alloy cladding in high-temperature steam oxidation up to 1400 °C
    Mohamad, Afiqa
    Nemoto, Yoshiyuki
    Furumoto, Kenichiro
    Okada, Yuji
    Sato, Daiki
    CORROSION SCIENCE, 2023, 224
  • [25] Oxidation Behaviors of Zr-Sn-Nb Alloy in 1000∼1250 °C Steam
    Zhang Feng
    Zhang Chengyu
    Zhao Wanqian
    Zhang Yao
    Chen Le
    Li Mei
    Song Pengcheng
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (10) : 3677 - 3683
  • [26] Oxidation resistance of Mo/Cr bilayer coating on Zr alloy in a 1200 °C steam environment
    Wang, Zheng
    Zhang, Yingpeng
    Zhou, Shenghao
    Wang, Zhenyu
    Yao, Yirong
    Wang, Aiying
    Li, Ming
    Ke, Peiling
    CORROSION COMMUNICATIONS, 2024, 14 : 49 - 57
  • [27] HIGH TEMPERATURE STEAM CORROSION OF MICROARC OXIDATION COATINGS ON 6061 ALUMINUM ALLOY AT 300°C/3 MPa STEAM
    Qu, Yao
    Yang, Chaolin
    Jin, Xiaoyue
    Du, Jiancheng
    Xue, Wenbin
    SURFACE REVIEW AND LETTERS, 2021, 28 (01)
  • [28] High Temperature Steam Oxidation Behavior of Cr-coated Zr-4 Alloy Prepared by Multi-arc Ion Plating at 1000 and 1100 °C
    Liu, Shihong
    Xiao, Weiwei
    Luo, Biao
    Huang, Jinghao
    Zou, Shuliang
    Liu, Yilong
    Ren, Zhenghao
    RARE METAL MATERIALS AND ENGINEERING, 2024, 53 (07) : 1962 - 1969
  • [29] Oxidation of Advanced Zirconium Cladding Alloys in Steam at Temperatures in the Range of 600-1200 °C
    Steinbrueck, Martin
    Ver, Nora
    Grosse, Mirco
    OXIDATION OF METALS, 2011, 76 (3-4): : 215 - 232
  • [30] High Temperature Steam Oxidation Resistance of Mo/Al/Cr Composite Coating on Zirconium Alloy
    Zhang, Tengfei
    Liao, Haiyan
    Ruan, Haibo
    Su, Yongyao
    Wang, Jinbiao
    Xu, Zhaoying
    Dong, Jingren
    CHINA SURFACE ENGINEERING, 2023, 36 (02) : 97 - 103