Influence of pre-oxidation on the hot corrosion of M38G superalloy in the mixture of Na2SO4-NaCl melts

被引:37
作者
Liu, G. M. [1 ]
Yu, F. [2 ]
Tian, J. H. [1 ]
Ma, J. H. [1 ]
机构
[1] Nanchang Hangkong Univ, Sch Mat Sci & Engn, Nanchang 330063, Peoples R China
[2] Nanchang Hangkong Univ, Sch Aeronaut & Mech Engn, Nanchang 330063, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2008年 / 496卷 / 1-2期
关键词
M38; superalloy; Pre-oxidation; Hot corrosion; Na2SO4-NaCl melts;
D O I
10.1016/j.msea.2008.04.046
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ni-based M38G superalloy suffered from serious hot corrosion attack in the mixture of 75wt.%Na2SO4+25wt.%NaCl melts at temperatures above 800 degrees C. In order to investigate the influence of pre-oxidation on the hot corrosion resistance of this superalloy, pre-oxidation treatment was conducted at 950 degrees C in air for 8 h. A compact scale composed of Cr2O3, NiCr2O4 and TiO2 formed on the alloy surface after the pre-oxidation. The pre-oxidized specimens exhibited good hot corrosion resistance during exposure to the mixture of 75wt.%Na2SO4+25wt.%NaCl melts at 800 degrees C for 102h. With increasing the temperature, however, the degradation of the oxide scale was accelerated. For the corrosion at 850 degrees C, the pre-oxidized samples exhibited good hot corrosion resistance for 60h, while at 875 degrees C, the pre-oxidation treatment could not improve the hot corrosion resistance of this superalloy with obvious mass loss. The degradation mechanism of pre-oxidation sample in the mixture of 75 wt.%Na2SO4+25wt.%NaCl melts was discussed in this paper. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:40 / 44
页数:5
相关论文
共 15 条
[1]  
Barin I., 1973, THERMOCHEMICAL PROPE
[2]  
Birks N., 1983, INTRO HIGH TEMPERATU
[3]  
BORNSTEIN NS, 1969, T METALL SOC AIME, V245, P1947
[4]  
BORNSTEIN NS, 1970, CORROSION-US, V26, P209
[5]   Hot-corrosion of silicon carbide in combustion gases at temperatures above the dew point of salts [J].
Carruth, M ;
Baxter, D ;
Oliveira, F ;
Coley, K .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1998, 18 (16) :2331-2338
[6]   MECHANISMS FOR HOT CORROSION OF NICKEL-BASE ALLOYS [J].
GOEBEL, JA ;
PETTIT, FS ;
GOWARD, GW .
METALLURGICAL TRANSACTIONS, 1973, 4 (01) :261-278
[7]   NA2SO4-INDUCED ACCELERATED OXIDATION (HOT CORROSION) OF NICKEL [J].
GOEBEL, JA ;
PETTIT, FS .
METALLURGICAL TRANSACTIONS, 1970, 1 (07) :1943-&
[8]  
Kofstad P., 1988, Elsevier Appl. Sci., V24, DOI [10.1002/crat.2170240408, DOI 10.1002/CRAT.2170240408]
[9]   Oxidation behavior of a Single-crystal Ni-base superalloy in air.: I:: At 800 and 900°C [J].
Li, MH ;
Sun, XF ;
Li, JG ;
Zhang, ZY ;
Jin, T ;
Guan, HR ;
Hu, ZQ .
OXIDATION OF METALS, 2003, 59 (5-6) :591-605
[10]  
Li T.P., 2003, High Temperature Oxidation and Corrosion of Metals