The mechanical properties and toughening mechanisms of an epoxy polymer modified with polysiloxane-based core-shell particles

被引:184
作者
Chen, J. [1 ]
Kinloch, A. J. [1 ]
Sprenger, S. [2 ]
Taylor, A. C. [1 ]
机构
[1] Univ London Imperial Coll Sci Technol & Med, Dept Mech Engn, London SW7 2AZ, England
[2] Evonik Hanse GmbH, D-21502 Geesthacht, Germany
关键词
Core-shell particles; Epoxy polymers; Fracture; ELASTOMER-MODIFIED EPOXIES; FRACTURE-BEHAVIOR; RUBBER; DEFORMATION; TEMPERATURE; RESINS; SIZE; MORPHOLOGY; MICROSTRUCTURE; COMPOSITES;
D O I
10.1016/j.polymer.2013.06.009
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
An epoxy resin, cured using an anhydride hardener, has been modified by the addition of pre-formed polysiloxane core-shell rubber (S-CSR) particles with a mean diameter of 0.18 mu m. The glass transition temperature, T-g, of the cured unmodified epoxy polymer was 148 degrees C, and this was unchanged after the addition of the S-CSR particles. The polysiloxane rubber particles had a T-g of about -100 degrees C. Atomic force microscopy showed that the S-CSR particles were well-dispersed in the epoxy polymer. The addition of the S-CSR particles reduced the Young's modulus and tensile strength of the epoxy polymer, but at 20 degrees C the fracture energy, G(Ic), increased from 117 J/m(2) for the unmodified epoxy to 947 J/m(2) when 20 wt% of the S-CSR particles were incorporated. Fracture tests were also performed at -55 degrees C, -80 degrees C, and -109 degrees C. The results showed that the measured fracture energy of the S-CSR-modified epoxy polymers decreased significantly below room temperature. For example, at -109 degrees C, a fracture energy of 481 J/m(2) was measured using 20 wt% of S-CSR particles. Nevertheless, this value of toughness still represented a major increase compared with the unmodified epoxy polymer, which possessed a value of G(Ic) of 174 J/m(2) at this very low test temperature. Thus, a clear fact that emerged was that the addition to the epoxy polymer of the S-CSR particles may indeed lead to significant toughening of the epoxy, even at temperatures as low as about -100 degrees C. The toughening mechanisms induced by the S-CSR particles were identified as (a) localised plastic shear-band yielding around the particles and (b) cavitation of the particles followed by plastic void growth of the epoxy polymer. These mechanisms were modelled using the Hsieh et al. approach [33,49] and the values of G(Ic) of the S-CSR-modified epoxy polymers at the different test temperatures were calculated. Excellent agreement was found between the predictions and the experimentally measured fracture energies. Further, the experimental and modelling results of the present study indicated that the extent of plastic void growth was suppressed at low temperatures for the S-CSR-modified epoxy polymers, but that the localised shear-band yielding mechanism was relatively insensitive to the test temperature. (C) 2013 The Authors. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:4276 / 4289
页数:14
相关论文
共 50 条
  • [21] Fracture behavior of epoxy polymers modified with core-shell rubber particles
    Becu, L
    Maazouz, A
    Sautereau, H
    Gerard, JF
    JOURNAL OF APPLIED POLYMER SCIENCE, 1997, 65 (12) : 2419 - 2431
  • [22] High strength epoxy system modified with soft block copolymer and stiff core-shell rubber nanoparticles: Morphology, mechanical properties, and fracture mechanisms
    Bajpai, A.
    Wetzel, B.
    Friedrich, K.
    EXPRESS POLYMER LETTERS, 2020, 14 (04): : 384 - 399
  • [23] Experimental studies of the deformation mechanisms of core-shell rubber-modified diglycidyl ether of bisphenol-A epoxy at cryogenic temperatures
    Brown, Hayley R.
    Schneider, Judy A.
    Murphy, Taylor L.
    JOURNAL OF COMPOSITE MATERIALS, 2014, 48 (11) : 1279 - 1296
  • [24] Incorporation of core-shell particles into methacrylate based composites for improvement of the mechanical properties
    Sandmann, Benedict
    Happ, Bobby
    Perevyazko, Igor
    Rudolph, Tobias
    Schacher, Felix H.
    Hoeppener, Stephanie
    Mansfeld, Ulrich
    Hager, Martin D.
    Fischer, Urs K.
    Burtscher, Peter
    Moszner, Norbert
    Schubert, Ulrich S.
    POLYMER CHEMISTRY, 2015, 6 (29) : 5273 - 5280
  • [25] Preparation of polyacrylate-polysiloxane core-shell latex particles
    Kong, XZ
    Kan, CY
    Yuan, Q
    POLYMERS FOR ADVANCED TECHNOLOGIES, 1996, 7 (12) : 888 - 890
  • [26] Toughening of dicyandiamide-cured DGEBA-based epoxy resin using MBS core-shell rubber particles
    Mousavi, Sayed Rasoul
    Amraei, Iraj Amiri
    JOURNAL OF COMPOSITE MATERIALS, 2015, 49 (19) : 2357 - 2363
  • [27] Effect of matrix deformability on the fracture properties of epoxy resins modified with core-shell and cross-linked rubber particles
    Imanaka, Makoto
    Narita, Ichihito
    Nakamura, Yoshinobu
    Hisaka, Shigeki
    Yoshida, Shun
    Hara, Keisuke
    JOURNAL OF APPLIED POLYMER SCIENCE, 2022, 139 (23)
  • [28] Vibration damping and dynamic mechanical attributes of core-shell particles modified glass epoxy prepregs cured using microwave irradiations
    Bhudolia, Somen K.
    Gohel, Goram
    Joshi, Sunil C.
    Leong, Kah Fai
    COMPOSITES COMMUNICATIONS, 2020, 21
  • [29] Epoxy networks toughened by core-shell particles:: Influence of the particle structure and size on the rheological and mechanical properties
    Bécu-Longuet, L
    Bonnet, A
    Pichot, C
    Sautereau, H
    Maazouz, A
    JOURNAL OF APPLIED POLYMER SCIENCE, 1999, 72 (06) : 849 - 858
  • [30] Toughening mechanism of polypropylene bends with polymer particles in core-shell structure: Equivalent rubber content effect related to core-shell interfacial strength
    Jia, Erwen
    Zhao, Shunjie
    Shangguan, Yonggang
    Zheng, Qiang
    POLYMER, 2019, 178