High-strength and high-toughness polyethylene (PE) fibers are prepared by the melt-spinning and subsequent drawing in the semimolten state of high-density PE (HDPE) combined with ultrahigh-molecular-weight PE (UHMW-PE). As-spun fibers are prepared by the melt-spinning of HDPE/UHMW-PE blended powder with 0-30 wt% UHMW-PE. The as-spun fiber is drawn at 100 (solid state) and 130 degrees C (semimolten state). Well-arranged stacked lamellae with highly oriented crystals are formed based on the difference in relaxation time for the drawn fiber with 30 wt% UHMW-PE prepared at 130 degrees C in the semimolten state. This composite structure results in a PE fiber with high tensile strength (1.11 GPa) and high toughness (297 MJ m(-3)).
机构:
Cent South Univ, Sch Met & Environm, Changsha 410083, Peoples R China
Cent South Univ, Natl Ctr Int Res Clean Met, Changsha 410083, Peoples R ChinaCent South Univ, Sch Met & Environm, Changsha 410083, Peoples R China
Zhang, Lei
Zhai, Bingyu
论文数: 0引用数: 0
h-index: 0
机构:
Cent South Univ, Sch Met & Environm, Changsha 410083, Peoples R China
Cent South Univ, Natl Ctr Int Res Clean Met, Changsha 410083, Peoples R ChinaCent South Univ, Sch Met & Environm, Changsha 410083, Peoples R China
Zhai, Bingyu
Wang, Wanlin
论文数: 0引用数: 0
h-index: 0
机构:
Cent South Univ, Sch Met & Environm, Changsha 410083, Peoples R China
Cent South Univ, Natl Ctr Int Res Clean Met, Changsha 410083, Peoples R ChinaCent South Univ, Sch Met & Environm, Changsha 410083, Peoples R China
Wang, Wanlin
Sohn, Il
论文数: 0引用数: 0
h-index: 0
机构:
Yonsei Univ, Mat Sci & Engn Dept, Seoul 120749, South KoreaCent South Univ, Sch Met & Environm, Changsha 410083, Peoples R China