摘要
The characterization of electroless Pd contacts to p-ZnTe has been carried out by measuring the current-voltage curves and Auger sputter depth profiles. On the basis of the shape of the I-V characteristics, it can be concluded that electroless Pd makes a contact of much better quality than electroless Au and Pt contacts. The best contacts are achievable for Pd electrode by annealing at 200 degrees C. The specific contact resistance under this condition is estimated to be as low as 6 x 10(-4) Ohm cm(2) for p-ZnTe with a hole concentration of 3 x 10(17) cm(-3) by the method of Cox and Strack. For electroless Pd, Pd-ZnTe alloy is formed. On the other hand, electroless Au leaves oxygen contamination near the interface between ZnTe and metal, whereas electroless Pt brings out the Te intermediate layer. (C) 1999 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:508 / 511
页数:4
相关论文
共 50 条
[41]   Low temperature Ni/Si/Al ohmic contacts to p-type 4H-SiC [J].
Xu, Yang-Xi ;
Sui, Jin-Chi ;
Cao, Fei ;
Li, Xing-Ji ;
Yang, Jian-Qun ;
Wang, Ying .
SOLID-STATE ELECTRONICS, 2021, 186
[42]   Formation mechanism of low contact resistance PdZn-based ohmic contacts for p-type InP [J].
Asamizu, H ;
Yamaguchi, A ;
Iguchi, Y ;
Saitoh, T ;
Murakami, M .
MATERIALS TRANSACTIONS, 2002, 43 (06) :1352-1359
[43]   High temperature stability of chromium boride ohmic contacts to p-type 6H-SiC [J].
T. N. Oder ;
J. R. Williams ;
M. J. Bozack ;
V. Iyer ;
S. E. Mohney ;
J. Crofton .
Journal of Electronic Materials, 1998, 27 :324-329
[44]   Low temperature Cu/Ti/Al Ohmic contacts to p-type 4H-SiC [J].
Cao, Fei ;
Xu, Yang-xi ;
Sui, Jin-chi ;
Li, Xing-ji ;
Yang, Jian-qun ;
Wang, Ying .
JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 901
[45]   High temperature stability of chromium boride ohmic contacts to p-type 6H-SiC [J].
Oder, TN ;
Williams, JR ;
Bozack, MJ ;
Iyer, V ;
Mohney, SE ;
Crofton, J .
JOURNAL OF ELECTRONIC MATERIALS, 1998, 27 (04) :324-329
[46]   Ohmic contacts simultaneously formed on n-type and p-type 4H-SiC at low temperature [J].
He, Yanjing ;
Lv, Hongliang ;
Tang, Xiaoyan ;
Song, Qingwen ;
Zhang, Yimeng ;
Han, Chao ;
Guo, Tao ;
He, Xiaoning ;
Zhang, Yimen ;
Zhang, Yuming .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 805 :999-1003
[47]   Thermal stability of Pd Schottky contacts to p-type 6H-SiC [J].
Samiji, ME ;
Venter, A ;
Leitch, AWR .
SILICON CARBIDE AND RELATED MATERIALS - 2002, 2002, 433-4 :681-684
[48]   Ag nanodot/Mg/Al reflective Ohmic contacts simultaneously suitable for n-type and p-type GaN [J].
Jin, Nan ;
Zhou, Yugang ;
Guo, Yan ;
Pan, Sai ;
Zhang, Rong ;
Zheng, Youdou .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2023, 56 (21)
[49]   Ti/Al/Si Ohmic Contacts for Both n-Type and p-Type 4H-SiC [J].
Tamaso, Hideto ;
Yamada, Shunsuke ;
Kitabayashi, Hiroyuki ;
Horii, Taku .
SILICON CARBIDE AND RELATED MATERIALS 2013, PTS 1 AND 2, 2014, 778-780 :669-672
[50]   Characterization of Pd/Ni/Au ohmic contacts on p-GaN [J].
Cho, HK ;
Hossain, T ;
Bae, JW ;
Adesida, I .
SOLID-STATE ELECTRONICS, 2005, 49 (05) :774-778