Structural transition from two-dimensional ZIF-L to three-dimensional ZIF-8 nanoparticles in aqueous room temperature synthesis with improved CO2 adsorption

被引:56
作者
Khan, Imran Ullah [1 ,2 ,3 ]
Othman, Mohd Hafiz Dzarfan [1 ]
Ismail, A. F. [1 ]
Ismail, N. [1 ]
Jaafar, Juhana [1 ]
Hashim, Haslenda [1 ]
Rahman, Mukhlis A. [1 ]
Jilani, Asim [1 ,4 ]
机构
[1] Univ Teknol Malaysia, Fac Chem & Energy Engn, Adv Membrane Technol Res Ctr AMTEC, Skudai 81310, Johor, Malaysia
[2] NUST, SCME, H-12, Islamabad, Pakistan
[3] Univ Teknol Malaysia, Fac Chem & Energy Engn, Proc Syst Engn Ctr PROSPECT, Skudai 81310, Johor, Malaysia
[4] King Abdulaziz Univ, Ctr Nanotechnol, Jeddah 21589, Saudi Arabia
关键词
Rapid synthesis; Particle size; Molar ratio; Transition; Basicity; Desorption; ZEOLITIC-IMIDAZOLATE FRAMEWORK; METAL-ORGANIC FRAMEWORKS; THIN-FILMS; CARBON-DIOXIDE; GAS SEPARATION; SIZE; MEMBRANES; NANOCRYSTALS; MORPHOLOGY; CRYSTALS;
D O I
10.1016/j.matchar.2018.01.003
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A new micron-sized leaf- two-dimensional (2D) structured zeolitic imidazolate framework (ZIF-L) and nano sized ZIF-8 were successfully synthesised in aqueous basic solution at room temperature with the same molar ratio of reagents (Zn+2/Hmim = 8). Both ZIFs have attracted tremendous research interest due to their wide applications including absorption, separation, and catalysis. This phase and morphology change could be tailored by changing the concentration of base-type additive triethylamine (TEA). Also, this morphology change from 2D (ZIF-L) to three-dimensional (3D) (ZIF-8) was observed by X-ray diffraction (XRD), transmission electron microscopy (TEM), field emission scanning electron microscopy (FESEM), thermogravimetric analysis (TGA), attenuated total reflectance infrared (ATR-IR) spectroscopy analysis, and surface area and pore textural properties using micromeritics gas adsorption analyser. The total amount of basic sites and carbon dioxide (CO2) desorption capacity were also calculated using CO2 temperature-programmed desorption (CO2-TPD) technique. Furthermore, TEA/total mole ratio of 0.0006 was proved as transition loading between two phases. Also, the particle and crystal size of samples decreased with increasing TEA/total mole ratio. The smallest ZIF-L and ZIF-8 particles obtained were 1.6 mu m and 177 nm, respectively that showed excellent thermal stability. The basicity and uptakes of CO2 improved proportionally with TEA and followed this order: ZIF-8 > ZIF-L. This study provides some new insights into zeolitic imidazolate framework by controlling crystal growth and morphology.
引用
收藏
页码:407 / 416
页数:10
相关论文
共 53 条
[1]   Enhanced the photocatalytic activity of Ni-doped ZnO thin films: Morphological, optical and XPS analysis [J].
Abdel-wahab, M. Sh. ;
Jilani, Asim ;
Yahia, I. S. ;
Al-Ghamdi, Attieh A. .
SUPERLATTICES AND MICROSTRUCTURES, 2016, 94 :108-118
[2]   High-throughput synthesis of zeolitic imidazolate frameworks and application to CO2 capture [J].
Banerjee, Rahul ;
Phan, Anh ;
Wang, Bo ;
Knobler, Carolyn ;
Furukawa, Hiroyasu ;
O'Keeffe, Michael ;
Yaghi, Omar M. .
SCIENCE, 2008, 319 (5865) :939-943
[3]   Control of Pore Size and Functionality in Isoreticular Zeolitic Imidazolate Frameworks and their Carbon Dioxide Selective Capture Properties [J].
Banerjee, Rahul ;
Furukawa, Hiroyasu ;
Britt, David ;
Knobler, Carolyn ;
O'Keeffe, Michael ;
Yaghi, Omar M. .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2009, 131 (11) :3875-+
[4]   Metal-Organic Framework Thin Films: From Fundamentals to Applications [J].
Betard, Angelique ;
Fischer, Roland A. .
CHEMICAL REVIEWS, 2012, 112 (02) :1055-1083
[5]   A two-dimensional zeolitic imidazolate framework with a cushion-shaped cavity for CO2 adsorption [J].
Chen, Rizhi ;
Yao, Jianfeng ;
Gu, Qinfen ;
Smeets, Stef ;
Baerlocher, Christian ;
Gu, Haoxue ;
Zhu, Dunru ;
Morris, William ;
Yaghi, Omar M. ;
Wang, Huanting .
CHEMICAL COMMUNICATIONS, 2013, 49 (82) :9500-9502
[6]   Controlling Zeolitic Imidazolate Framework Nano- and Microcrystal Formation: Insight into Crystal Growth by Time-Resolved In Situ Static Light Scattering [J].
Cravillon, Janosch ;
Nayuk, Roman ;
Springer, Sergej ;
Feldhoff, Armin ;
Huber, Klaus ;
Wiebcke, Michael .
CHEMISTRY OF MATERIALS, 2011, 23 (08) :2130-2141
[7]   Rapid Room-Temperature Synthesis and Characterization of Nanocrystals of a Prototypical Zeolitic Imidazolate Framework [J].
Cravillon, Janosch ;
Muenzer, Simon ;
Lohmeier, Sven-Jare ;
Feldhoff, Armin ;
Huber, Klaus ;
Wiebcke, Michael .
CHEMISTRY OF MATERIALS, 2009, 21 (08) :1410-1412
[8]   Opening the Gate: Framework Flexibility in ZIF-8 Explored by Experiments and Simulations [J].
Fairen-Jimenez, D. ;
Moggach, S. A. ;
Wharmby, M. T. ;
Wright, P. A. ;
Parsons, S. ;
Dueren, T. .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2011, 133 (23) :8900-8902
[9]   A review on contemporary Metal-Organic Framework materials [J].
Gangu, Kranthi Kumar ;
Maddila, Suresh ;
Mukkamala, Saratchandra Babu ;
Jonnalagadda, Sreekantha B. .
INORGANICA CHIMICA ACTA, 2016, 446 :61-74
[10]   Aqueous room temperature synthesis of cobalt and zinc sodalite zeolitic imidizolate frameworks [J].
Gross, Adam F. ;
Sherman, Elena ;
Vajo, John J. .
DALTON TRANSACTIONS, 2012, 41 (18) :5458-5460