XRD and FTIR crystallinity indices in sound human tooth enamel and synthetic hydroxyapatite

被引:176
作者
Reyes-Gasga, Jose [1 ]
Martinez-Pineiro, Esmeralda L. [1 ]
Rodriguez-Alvarez, Galois [1 ]
Tiznado-Orozco, Gaby E. [2 ]
Garcia-Garcia, Ramiro [1 ]
Bres, Etienne F. [3 ]
机构
[1] Univ Nacl Autonoma Mexico, Inst Fis, Mexico City 04510, DF, Mexico
[2] Univ Autonoma Nayark, Unidad Acad Odontol, Tepic 63190, Nayarit, Mexico
[3] Univ Lille Sci & Technol 1, Unite Mat & Transformat, F-59650 Villeneuve Dascq, France
来源
MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS | 2013年 / 33卷 / 08期
关键词
Hydroxyapatite; Enamel crystallinity index; X-ray analysis; Fourier Transform Infrared spectroscopy; DIAGENETIC EVOLUTION; BONE; DIFFRACTION; PHOSPHATE; AGE;
D O I
10.1016/j.msec.2013.07.014
中图分类号
TB3 [工程材料学]; R318.08 [生物材料学];
学科分类号
0805 ; 080501 ; 080502 ;
摘要
The crystallinity index (Cl) is a measure of the percentage of crystalline material in a given sample and it is also correlated to the degree of order within the crystals. In the literature two ways are reported to measure the Cl: X-ray diffraction and infrared spectroscopy. Although the Cl determined by these techniques has been adopted in the field of archeology as a structural order measure in the bone with the idea that it can help e.g. in the sequencing of the bones in chronological and/or stratigraphic order, some debate remains about the reliability of the Cl values. To investigate similarities and differences between the two techniques, the Cl of sound human tooth enamel and synthetic hydroxyapatite (HAP) was measured in this work by X-ray diffraction (XRD) and Fourier Transform Infrared spectroscopy (FTIR), at room temperature and after heat treatment. Although the (CI)(XRD) index is related to the crystal structure of the samples and the (CI)(FTIR) index is related to the vibration modes of the molecular bonds, both indices showed similar qualitative behavior for heat-treated samples. At room temperature, the (CI)(XRD) value indicated that enamel is more crystalline than synthetic HAP, while (CI)(FTIR) indicated the opposite. Scanning (SEM) and transmission (TEM) images were also used to corroborate the measured Cl values. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:4568 / 4574
页数:7
相关论文
共 36 条
[1]  
ADLER HH, 1964, AM MINERAL, V49, P1002
[2]   Bioactive nanocrystalline sol-gel hydroxyapatite coatings [J].
Chai, CS ;
Ben-Nissan, B .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 1999, 10 (08) :465-469
[3]   Structural and microstructural characterization of bioapatites and synthetic hydroxyapatite using X-ray powder diffraction and Fourier transform infrared techniques [J].
Chakraborty, Santu ;
Bag, Sandip ;
Pal, Subrata ;
Mukherjee, Alok K. .
JOURNAL OF APPLIED CRYSTALLOGRAPHY, 2006, 39 :385-390
[4]   Structure refinements by the Rietveld method of partially substituted hydroxyapatite:: Ca9Na0.5(PO4)4.5(CO3)1.5(OH)2 [J].
El Feki, H ;
Savariault, JM ;
Ben Salah, A .
JOURNAL OF ALLOYS AND COMPOUNDS, 1999, 287 (1-2) :114-120
[5]  
Gutiérrez-Salazar Maria del Pilar, 2003, Mat. Res., V6, P367
[6]  
Kimura I, 2007, RES LETT MAT SCI, V2007, P1, DOI DOI 10.1155/2007/71284
[7]  
Klug H.P., 1974, XRAY DIFFRACTION PRO, V2nd, P656
[8]  
LARMAS MA, 1993, SCAND J DENT RES, V101, P185
[9]   New parameters for the characterization of diagenetic alterations and heat-induced changes of fossil bone mineral using Fourier transform infrared spectrometry [J].
Lebon, M. ;
Reiche, I. ;
Bahain, J-J. ;
Chadefaux, C. ;
Moigne, A-M. ;
Froehlich, F. ;
Semah, F. ;
Schwarcz, H. P. ;
Falgueres, C. .
JOURNAL OF ARCHAEOLOGICAL SCIENCE, 2010, 37 (09) :2265-2276
[10]   Crystal Structure Studies of Human Dental Apatite as a Function of Age [J].
Leventouri, Th. ;
Antonakos, A. ;
Kyriacou, A. ;
Venturelli, R. ;
Liarokapis, E. ;
Perdikatsis, V. .
INTERNATIONAL JOURNAL OF BIOMATERIALS, 2009, 2009