Comparison of potassium chloride and potassium carbonate with respect to their tendency to cause high temperature corrosion of stainless 304L steel

被引:62
作者
Lehmusto, J. [1 ]
Skrifvars, B. -J. [1 ]
Yrjas, P. [1 ]
Hupa, M. [1 ]
机构
[1] Abo Akad Univ, SF-20500 Turku, Finland
关键词
High temperature oxidation; Potassium chloride; Potassium carbonate; Water vapor; 304 L steel; FE-CR ALLOYS; WASTE INCINERATION ENVIRONMENTS; OXIDE HYDROXIDE EVAPORATION; WATER-VAPOR; HOT CORROSION; OXIDIZING ATMOSPHERES; ACCELERATED OXIDATION; METALLIC MATERIALS; MOLTEN CHLORIDES; SALT DEPOSITS;
D O I
10.1016/j.fuproc.2011.12.016
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
The influence of both solid KCl as well as K2CO3 on the oxidation of the 304 L steel has been investigated in the laboratory. Three temperatures were used; 500 degrees C, 550 degrees C, and 600 degrees C. The steel samples were covered either with KCl or K2CO3 and held in two different atmospheres; dried air and air with a water content of 30%. Exposures with no salt were carried out as well. The exposure time in every test was 168 h. The extent of corrosion, the elemental distribution as well as the identification of corrosion products was determined using a scanning electron microscope equipped with an energy dispersive x-ray analyzer (SEM/EDXA). Both salts were found to be corrosive. The structure of the formed oxide layer was similar with both salts, i.e., the outermost iron oxide layer was followed by an oxide layer containing chromium, iron and nickel, followed by a nickel-rich region before the bulk metal. With both salt indications of a potassium-chromium compound, most likely potassium chromate (K2CrO4) was found to be formed as an intermediate. The oxide layer thickness distributions showed some differences between the salts as well as differences within a salt under different conditions. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:98 / 105
页数:8
相关论文
共 36 条
[1]  
Abd El-Rahman HA, 1999, J APPL ELECTROCHEM, V29, P1205
[2]   Evidence for chromium evaporation influencing the oxidation of 304L: The effect of temperature and flow rate [J].
Asteman, H ;
Svensson, JE ;
Johansson, LG .
OXIDATION OF METALS, 2002, 57 (3-4) :193-216
[3]   Influence of water vapor and flow rate on the high-temperature oxidation of 304L; Effect of chromium oxide hydroxide evaporation [J].
Asteman, H ;
Svensson, JE ;
Norell, M ;
Johansson, LG .
OXIDATION OF METALS, 2000, 54 (1-2) :11-26
[4]   Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873 K in the presence of 10% water vapor [J].
Asteman, H ;
Svensson, JE ;
Johansson, LG ;
Norell, M .
OXIDATION OF METALS, 1999, 52 (1-2) :95-111
[5]   High temperature corrosion of superheater materials below deposited biomass ashes in biomass combusting atmospheres [J].
Cha, S. C. .
CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2007, 42 (01) :50-60
[6]   Fundamental studies on alkali chloride induced corrosion during combustion of biomass [J].
Cha, SC ;
Spiegel, M .
HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 :1055-1062
[7]   Utilizing biomass and waste for power production - a decade of contributing to the understanding, interpretation and analysis of deposits and corrosion products [J].
Frandsen, FJ .
FUEL, 2005, 84 (10) :1277-1294
[8]   THE EFFECTS OF CHLORIDES, HYDROGEN-CHLORIDE, AND SULFUR-DIOXIDE IN THE OXIDATION OF STEELS BELOW DEPOSITS [J].
GRABKE, HJ ;
REESE, E ;
SPIEGEL, M .
CORROSION SCIENCE, 1995, 37 (07) :1023-1043
[9]   Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600°C [J].
Halvarsson, M. ;
Tang, J. E. ;
Asteman, H. ;
Svensson, J. -E. ;
Johansson, L. -G. .
CORROSION SCIENCE, 2006, 48 (08) :2014-2035
[10]   Stability of protective oxide films in waste incineration environment - solubility measurement of oxides in molten chlorides [J].
Ishitsuka, T ;
Nose, K .
CORROSION SCIENCE, 2002, 44 (02) :247-263