Influence of crystallite size and surface morphology on electrochemical properties of annealed TiO2 nanotubes

被引:68
作者
Munirathinam, Balakrishnan [1 ]
Pydimukkala, Haveela [1 ]
Ramaswamy, Narayanan [2 ]
Neelakantan, Lakshman [1 ]
机构
[1] IIT Madras, Dept Met & Mat Engn, Madras, Tamil Nadu, India
[2] VIT Univ, Sch Mech & Bldg Sci, Madras, Tamil Nadu, India
关键词
Anodization; TiO2; nanotubes; Crystallite size; Impedance; Polarization; CORROSION BEHAVIOR; TITANIA NANOTUBES; VOIGT-FUNCTION; ANODIZATION PARAMETERS; HYDROXYAPATITE GROWTH; ANODIC GROWTH; OXIDE; ELECTROLYTE; FABRICATION; TI-6AL-4V;
D O I
10.1016/j.apsusc.2015.08.017
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The current study investigates the effect of crystallite size and surface morphology of TiO2 nanotubes on their wettability and electrochemical properties. Self-organized amorphous TiO2 nanotubes were synthesized by anodization process in an acidic (0.5 wt% HF) and a neutral electrolyte (1 M Na2SO4 + 0.5 wt% NaF). Subsequently, the nanotubes were annealed at 450 degrees C to achieve crystalline phase. Scanning electron microscope micrographs revealed that nanotubes formed from the neutral bath are four times longer (1.2 mu m) than the ones synthesized from the acidic bath (325 nm). The charge consumed during anodization is greater under the acidic conditions implying the severity of the attack on the nanotubes by the electrolyte. X-Ray diffraction analysis showed that after annealing TiO2 crystallizes in the tetragonal lattice as anatase structure. Peak fitting method for line profile analysis was employed to estimate the crystallite size and the micro strain. The oxide nanotubes formed in neutral medium showed smaller crystallite size (28.91 nm) than the one formed in acidic medium (4337 nm). Wettability measurements showed wetting angles <60, indicating hydrophilic nature of the anatase nanotubes. Further, both the dimensional aspect (i.e., length and diameter of nanotubes) and the crystallite size have significant effect on the hydrophilic behavior. Electrochemical impedance spectroscopy in a simulated body fluid environment confirmed that structural changes in the oxide layer influence the electrochemical properties. Polarization studies demonstrated that crystallite size affects the passive behavior of the nanotubes. Smaller crystallite size (28.91 nm) lowers the passive current density (0.11 mu A cm(-2)), indicating the good protectiveness. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:1245 / 1253
页数:9
相关论文
共 55 条
[21]   Influence of thermal annealing on the composition and structural parameters of DC magnetron sputtered titanium dioxide thin films [J].
Karunagaran, B ;
Kumar, RTR ;
Mangalaraj, D ;
Narayandass, SK ;
Rao, GM .
CRYSTAL RESEARCH AND TECHNOLOGY, 2002, 37 (12) :1285-1292
[22]   Synthesis of Self-ordered Titanium Oxide Nanotubes by Anodization of Titanium [J].
Krishnan, A. Yaadhav ;
Sivabalan, S. ;
Subhachandhar, S. ;
Balakrishnan, M. ;
Narayanan, R. .
FUNCTIONAL MATERIALS-BOOK, 2012, 1461 :222-224
[23]   Incorporation of Ca and P on anodized titanium surface: Effect of high current density [J].
Laurindo, Carlos A. H. ;
Torres, Ricardo D. ;
Mali, Sachin A. ;
Gilbert, Jeremy L. ;
Soares, Paulo .
MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2014, 37 :223-231
[24]   Titanium dioxide nanotube arrays fabricated by anodizing processes - Electrochemical properties [J].
Lee, Woo-Jin ;
Alhoshan, Mansour ;
Smyrl, William H. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2006, 153 (11) :B499-B505
[25]   High purity anatase TiO2 nanocrystals:: Near room-temperature synthesis, grain growth kinetics, and surface hydration chemistry [J].
Li, GS ;
Li, LP ;
Boerio-Goates, J ;
Woodfield, BF .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2005, 127 (24) :8659-8666
[26]   Electrochemical stability of TiO2 nanotubes with different diameters in artificial saliva [J].
Liu, Chenglong ;
Wang, Yueji ;
Wang, Meng ;
Huang, Weijiu ;
Chu, Paul K. .
SURFACE & COATINGS TECHNOLOGY, 2011, 206 (01) :63-67
[27]   Electrochemical Corrosion Behavior of Nanocrystalline Materials-a Review [J].
Liu, Li ;
Li, Ying ;
Wang, Fuhui .
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2010, 26 (01) :1-14
[28]   Anodic growth of self-organized anodic TiO2 nanotubes in viscous electrolytes [J].
Macak, Jan M. ;
Schmuki, Patrik .
ELECTROCHIMICA ACTA, 2006, 52 (03) :1258-1264
[29]   Smooth anodic TiO2 nanotubes [J].
Macak, JM ;
Tsuchiya, H ;
Taveira, L ;
Aldabergerova, S ;
Schmuki, P .
ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2005, 44 (45) :7463-7465
[30]   Self-organized porous titanium oxide prepared in Na2SO4/NaF electrolytes [J].
Macak, JM ;
Sirotna, K ;
Schmuki, P .
ELECTROCHIMICA ACTA, 2005, 50 (18) :3679-3684