Process and characterization of reclaimed carbon fiber composites by pyrolysis and oxidation, assisted by thermal plasma to avoid pollutants emissions

被引:13
作者
Caldeira Alves, Silvia Moura [1 ]
da Silva, Fabio Santos [1 ]
Donadon, Mauricio Vicente [2 ]
Garcia, Rafael Razuk [3 ]
Corat, Evaldo Jose [4 ]
机构
[1] Embraer SA, Sao Jose Dos Campos, Brazil
[2] Inst Tecnol Aeronaut, Sao Jose Dos Campos, Brazil
[3] Recaltech, Lorena, SP, Brazil
[4] Inst Nacl Pesquisas Espaciais, Sao Jose Dos Campos, Brazil
关键词
Recycling; composites; carbon fiber; pyrolysis; thermal plasma; tensile testing; interlaminar shear strength; vacuum-assisted RTM;
D O I
10.1177/0021998317724214
中图分类号
TB33 [复合材料];
学科分类号
摘要
This paper shows a developed process to reclaim carbon fiber from end-of-life thermoset composite or pre-preg process waste, which uses pyrolysis and oxidation to remove the matrix (resin) and a plasma reactor to treat the exhaust gases. Laminates were manufactured to be recycled and the reclaimed laminates were remanufactured and then tested. Tensile tests, interlaminar shear strength tests and measurement of the fiber volumetric fraction for both virgin and reclaimed laminates were carried out. The dimensions, masses and permeability were also measured for both virgin and recycled laminates. Additionally, ultrasound inspections, Raman spectroscopy, micrographs using scanning and transmission, as well as microscopy of the fracture surfaces of the composite specimens submitted to the tensile and interlaminar shear strength tests were performed. Monofilament tensile tests in one of the reclaimed and virgin samples were also conducted. All these tests and analysis were conducted aiming at comparing the overall performance of the reference (virgin) composite to the one manufactured with reclaimed carbon fiber, trying to better understand the differences between them, and the origin and cause of these differences.
引用
收藏
页码:1379 / 1398
页数:20
相关论文
共 19 条
[1]  
[Anonymous], 2008, BOEING AERO MAGAZINE
[2]  
Callister WD, 2013, MAT SCI ENG INTRO, P644
[3]   Recycling of CFRP for high value applications: Effect of sizing removal and environmental analysis of the SuperCritical Fluid Solvolysis [J].
Dauguet, Michel ;
Mantaux, Olivier ;
Perry, Nicolas ;
Zhao, Yaoyao Fiona .
22ND CIRP CONFERENCE ON LIFE CYCLE ENGINEERING, 2015, 29 :734-739
[4]   Determining the mechanism controlling glass fibre strength loss during thermal recycling of waste composites [J].
Feih, S. ;
Mouritz, A. P. ;
Case, S. W. .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2015, 76 :255-261
[5]  
Gosau J-M, 2009, CARBON FIBER RECLAMA
[6]  
Hernanz R-P, 2008, J SUPERCRIT FLUID, V83, P92
[7]  
Li X, 2016, J CLEAN PROD, V451, P460
[8]  
Lopes AG., 2012, COMPORTAMENTO MECANI
[9]  
Morin C, 2012, J SUPERCRIT FLUID, V232, P240
[10]  
Oliveux G, 2015, PROGR MAT SCI, V61, P99