Interfacial layer in friction-bonded joint of low carbon steel to Al-Mg alloy (AA5083) and its influence on bond strength

被引:14
作者
Yamamoto, N [1 ]
Takahashi, M
Ikeuchi, K
Aritoshi, M
机构
[1] Osaka Univ, Joining & Welding Res Inst, Ibaraki 5670047, Japan
[2] Hyogo Prefectural Inst Technol, Kobe, Hyogo 6540037, Japan
关键词
friction bonding; dissimilar metal joint; aluminum magnesium alloy; low carbon steel; transmission electron microscope observation; intermetallic compound; oxide layer;
D O I
10.2320/matertrans.45.296
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The metallographic factor controlling the strength of friction-bonded interface of low carbon steel (approximately 0.10mass%C) to aluminum-magnesium (Al-Mg) alloy (equivalent to AA5083) has been investigated by TEM observations. The bond strength, estimated from the tensile strength of a specimen with a circumferential notch at the interface, rose rapidly with an increase in friction time, and then reduced. A maximum strength of 306 MPa was obtained at a friction time of 2 s (rotation speed = 20 s(-1), friction pressure = 40 MPa, and forge pressure = 230 MPa). At a friction time of 1 s, an IMC layer about 100 nm wide that consisted of (Fe,Mn)Al-6 and Mg2Si was formed at the interface, and an Al-oxide layer of a width less than 10 nm was observed between this IMC layer and low carbon steel substrate. In a joint showing the highest bond strength (friction time = 2 s), no Al-oxide layer could be detected between the low carbon steel substrate and IMC layer which consisted of (Fe,Mn)Al-6, Fe4Al13, Fe2Al5, and Mg2Si. The width of the interfacial layer was increased to about 300 nm. At a friction time of 4 s, a layer of MgAl2O4 was observed in addition to intermetallic compounds of (Fe,Mn)Al-6, Fe4Al13, Fe2Al5 and Mg2Si. The width of this layer was about 700 nm. Thus the phases formed in the interfacial layer as well as its width were altered depending on the friction time. The change in the bond strength with friction time was discussed in view of these differences in the interfacial microstructure.
引用
收藏
页码:296 / 299
页数:4
相关论文
共 8 条
[1]  
[Anonymous], J JAPAN I LIGHT META
[2]  
KAWAI G, 1999, J JPN I LIGHT MET, V49, P83
[3]   Friction bonding of silicon carbide to oxygen-free copper with an intermediate layer of reactive metal (reprinted from Journal of the Japan Institute of Metals, vol 65, pg 895-904, 1999) [J].
Nishimoto, A ;
Ando, M ;
Takahashi, M ;
Aritoshi, M ;
Ikeuchi, K .
MATERIALS TRANSACTIONS JIM, 2000, 41 (12) :1636-1645
[4]  
Ochi H., 1996, Journal of the Society of Materials Science, Japan, V45, P459, DOI 10.2472/jsms.45.459
[5]  
OCHI H, 1996, J JPN I LIGHT MET, V46, P500
[6]  
OCHI H, 1997, P 1997 7 INT OFFSH P, P541
[7]  
Sundaresan S., 1994, Materials Forum, V17, P301
[8]   FRICTION WELDING OF ST-AL AND AL-CU MATERIALS [J].
YILBAS, BS ;
SAHIN, AZ ;
KAHRAMAN, N ;
ALGARNI, AZ .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1995, 49 (3-4) :431-443