Thermal oxidation of titanium to improve corrosion resistance in boiling nitric acid medium

被引:29
作者
Shankar, A. Ravi [1 ]
Karthiselva, N. S. [2 ]
Mudali, U. Kamachi [1 ]
机构
[1] Indira Gandhi Ctr Atom Res, Corros Sci & Technol Grp, Kalpakkam 603102, Tamil Nadu, India
[2] Indian Inst Technol Madras, Dept Met & Mat Engn, Chennai 600036, Tamil Nadu, India
关键词
Titanium; Thermal oxidation; Nitric acid; Corrosion; Nano-rod structure; Roughness; STAINLESS-STEEL; CP-TI; BEHAVIOR; ZIRCALOY-4; WELDS;
D O I
10.1016/j.surfcoat.2013.07.010
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Commercially pure titanium (Cp-Ti) is being used as structural material for fabrication of dissolver in the reprocessing of carbide fuel from fast breeder test reactor. Thermal oxidation of titanium is one of the most simple and feasible options to extend the life of such critical components. In the present study thermal oxidation of titanium has been carried out at 923 K for 96 h. The thermally oxidized Cp-Ti samples were characterized by SEM, XRD, microscratch test and profilometry. Corrosion studies were carried out in boiling nitric acid medium as per ASTM A262 practice-C test and three phase corrosion test and the results were compared with Cp-Ti and Ti-5Ta-1.8Nb alloy. ASTM A262 practice-C test revealed reproducible outstanding corrosion resistance of thermally oxidized Cp-Ti compared to Cp-Ti and Ti-5Ta-1.8Nb alloy. Three phase corrosion test results also indicated better corrosion resistance of thermally oxidized Cp-Ti. The protective thick rutile TiO2 oxide layer with nano-rod structure formed on the surface improved the corrosion resistance of thermally oxidized Cp-Ti in boiling nitric acid as evident from SEM and XRD results. The hardness of thermally oxidized Cp-Ti sample was found to be 2.5 times higher than that of Cp-Ti and the surface roughness of the thermally oxidized Cp-Ti samples was found to be smooth before and after corrosion when compared to the as-polished surface. The corrosion resistance of the thermally oxidized Cp-Ti samples can be further improved by optimizing the parameters to achieve good adhesion strength. The paper highlights the results of the present investigation. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:45 / 53
页数:9
相关论文
共 30 条
[1]  
Ahluwalia H.S., 2006, ASM HDB, P668
[2]  
[Anonymous], 2002, ASTM, D. 4253-00Standard test method for maximum index density and unit weight of soils using a vibratory table Annual Book of ASTM Standards, P1
[3]  
[Anonymous], 2003, ASTM Int, V03, P1
[4]  
[Anonymous], 2003, Standard Test Method for Open Hole Tensile Strength of Polymer Matrix Composite Laminates, D 5766/D 5766M - 02a, DOI DOI 10.1520/C0039
[5]   Influence of Surface Roughness on Corrosion and Tribological Behavior of CP-Ti After Thermal Oxidation Treatment [J].
Arslan, E. ;
Totik, Y. ;
Demirci, E. ;
Alsaran, A. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2010, 19 (03) :428-433
[6]   Surface modification of titanium alloys for combined improvements in corrosion and wear resistance [J].
Bloyce, A ;
Qi, PY ;
Dong, H ;
Bell, T .
SURFACE & COATINGS TECHNOLOGY, 1998, 107 (2-3) :125-132
[7]   The corrosion-wear behaviour of thermally oxidised CP-Ti and Ti-6Al-4V [J].
Dearnley, PA ;
Dahm, KL ;
Çimenoglu, H .
WEAR, 2004, 256 (05) :469-479
[8]  
Fukuzuka T., 1980, TITANIUM 80 SCI TECH, P2783
[9]   Effect of Thermal Oxidation on Corrosion Resistance of Commercially Pure Titanium in Acid Medium [J].
Jamesh, M. ;
Kumar, Satendra ;
Narayanan, T. S. N. Sankara .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2012, 21 (06) :900-906
[10]  
Jamesh M., 2009, 23 INT C SURF MOD TE, P479