Capacity fading mechanism during long-term cycling of over-discharged LiCoO2/mesocarbon microbeads battery

被引:103
|
作者
Zhang, Lingling [1 ]
Ma, Yulin [1 ]
Cheng, Xinqun [1 ]
Du, Chunyu [1 ]
Guan, Ting [1 ]
Cui, Yingzhi [1 ]
Sun, Shun [1 ]
Zuo, Pengjian [1 ]
Gao, Yunzhi [1 ]
Yin, Geping [1 ]
机构
[1] Harbin Inst Technol, Sch Chem Engn & Technol, Inst Adv Chem Power Sources, Harbin 15001, Peoples R China
基金
美国国家科学基金会;
关键词
LiCoO2/MCMB battery; Over-discharge; Long-term cycling; Capacity fading mechanism; LITHIUM-ION BATTERY; X-RAY-DIFFRACTION; HIGH-TEMPERATURE; HIGH-POWER; PERFORMANCE; ELECTRODES; OVERDISCHARGE; STABILITY; COMPOSITE; ABUSE;
D O I
10.1016/j.jpowsour.2015.06.040
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The LiCoO2/mesocarbon microbeads (MCMB) batteries are over-discharged to 102% DOD, 105% DOD and 115% DOD, respectively, then are fully charged and cycled 1000 times at 0.6 C with 30% DOD. The capacity fading mechanism during long-term cycling of over-discharged batteries is analyzed by electrochemical and physical characterization. No remarkable difference is found on the morphology of LiCoO2 material from SEM. However, copper is detected on anode over-discharged to 115% DOD by EDS and XRD. The structures of LiCoO2 and MCMB materials have almost no change according to the result of XRD test. The performance of MCMB material can be degraded by over-discharge, however the LiCoO2 material still keeps good performance. The capacity of MCMB electrode is improved after being washed with water to remove the SEI film, indicating that the capacity loss of MCMB electrode is mainly attributed to the increase of SEI film. The capacity deterioration of over-discharged battery is mainly caused by the dissolution of copper current collector and the deposition of Cu on the surface of anode during the following charging process. The copper deposited on the surface of anode can hinder the lithium intercalation into/de-intercalation from the anode and promote the increase of SE! film. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:1006 / 1015
页数:10
相关论文
共 28 条
  • [1] Effect of short-time external short circuiting on the capacity fading mechanism during long-term cycling of LiCoO2/mesocarbon microbeads battery
    Zhang, Lingling
    Cheng, Xinqun
    Ma, Yulin
    Guan, Ting
    Sun, Shun
    Cui, Yingzhi
    Du, Chunyu
    Zuo, Pengjian
    Gao, Yunzhi
    Yin, Geping
    JOURNAL OF POWER SOURCES, 2016, 318 : 154 - 162
  • [2] Degradation mechanism of over-charged LiCoO2/mesocarbon microbeads battery during shallow depth of discharge cycling
    Zhang, Lingling
    Ma, Yulin
    Cheng, Xinqun
    Cui, Yingzhi
    Guan, Ting
    Gao, Yunzhi
    Du, Chunyu
    Yin, Geping
    Lin, Feng
    Nordlund, Dennis
    JOURNAL OF POWER SOURCES, 2016, 329 : 255 - 261
  • [3] Identifying the aging mechanism in multiple overdischarged LiCoO2/mesocarbon microbeads batteries
    Zhang, Lingling
    Liu, Jilong
    Du, Lei
    Xu, Xing
    Ma, Yulin
    Qu, Bin
    Fan, Peng
    Yin, Geping
    Yang, Fan
    Zhu, Li
    CERAMICS INTERNATIONAL, 2021, 47 (15) : 21253 - 21262
  • [4] Origins of capacity and voltage fading of LiCoO2 upon high voltage cycling
    Jiang, Yuyuan
    Qin, Changdong
    Yan, Pengfei
    Sui, Manling
    JOURNAL OF MATERIALS CHEMISTRY A, 2019, 7 (36) : 20824 - 20831
  • [5] Capacity Fading Mechanism of Large Scale Li4Ti5O12/LiCoO2 Battery
    Wu, Ke
    Gao, Ya
    Sun, Xiaoman
    Liu, Sha
    Wu, Ningning
    Zhao, Hailei
    Zhang, Yingchun
    2014 IEEE TRANSPORTATION ELECTRIFICATION CONFERENCE AND EXPO (ITEC) ASIA-PACIFIC 2014, 2014,
  • [6] Expanded mesocarbon microbead cathode for sodium-based dual-ion battery with superior specific capacity and long-term cycling stability
    Wang, Yu-Jia
    Yu, Xue-Wen
    Zhang, Peng
    Wang, Zheng-Jie
    Yan, Lei
    He, Liang
    Wang, Ze-Kai
    Shi, Zhi-Qiang
    RARE METALS, 2023, 42 (05) : 1545 - 1556
  • [7] On the capacity fading of LiCoO2 intercalation electrodes:: the effect of cycling, storage, temperature, and surface film forming additives
    Aurbach, D
    Markovsky, B
    Rodkin, A
    Levi, E
    Cohen, YS
    Kim, HJ
    Schmidt, M
    ELECTROCHIMICA ACTA, 2002, 47 (27) : 4291 - 4306
  • [8] Understanding the mechanism of cycling degradation and novel strategy to stabilize the cycling performance of graphite/LiCoO2 battery at high voltage
    Wang, Zaisheng
    Rao, Mumin
    Li, Jianhui
    Ye, Changchun
    Liu, Zidan
    Xu, Qingshuai
    Jin, Xiaojing
    Du, Ruian
    Xie, Qiming
    Luo, Wen
    Li, Weishan
    Qiu, Yongcai
    JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 2019, 851
  • [9] The capacity decay mechanism of the 100% SOC LiCoO2/graphite battery after high-temperature storage
    Liu, Weigang
    Zheng, Jingqiang
    Zhang, Zhi
    Gu, Jiahao
    Chen, Zhiyong
    Jiang, Hao
    Tong, Yan
    Fan, Xinming
    Li, Jie
    Wang, Mengran
    Hong, Bo
    JOURNAL OF POWER SOURCES, 2023, 580
  • [10] Long-Term Low-Rate Cycling of LiCoO2/Graphite Li-Ion Cells at 55°C
    Smith, A. J.
    Dahn, Hannah M.
    Burns, J. C.
    Dahn, J. R.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2012, 159 (06) : A705 - A710