Macromolecular coupling agents for flame retardant materials

被引:52
作者
Nachtigall, Sonia Marli Bohrz
Miotto, Maximiliano
Schneider, Elisangela Edila
Mauler, Raquel Santos
Forte, Maria Madalena Camargo
机构
[1] Univ Fed Rio Grande do Sul, Inst Quim, BR-91501970 Porto Alegre, RS, Brazil
[2] Univ Fed Rio Grande do Sul, Dept Mat Engn, BR-91501970 Porto Alegre, RS, Brazil
关键词
polymer composites; aluminum hydroxide; coupling agent; morphology; degradation;
D O I
10.1016/j.eurpolymj.2005.10.017
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Polypropylene (PP) is a large-consumed polymer employed in many applications. For some uses, good flame resistance is desirable and this can be achieved by the addition of metallic hydroxides. However, high loads of metallic hydroxides are needed causing marked deterioration of the physical properties. Addition of interfacial agents is a useful way of minimizing these effects. In this study, PP was modified with vinyltriethoxysilane (VTES) and maleic anhydride (MA) and the products were used as coupling agents for PP/aluminum hydroxide (ATH) composites. The composites were characterized by TGA, SEM, tensile and flammability tests. It was observed that both coupling agents were efficient but PP modified with VTES showed better effect on the mechanical properties. Two types of ATH were used for comparison. (C) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:990 / 999
页数:10
相关论文
共 31 条
[1]  
Cook M, 1998, ADV POLYM TECH, V17, P53, DOI 10.1002/(SICI)1098-2329(199821)17:1<53::AID-ADV5>3.0.CO
[2]  
2-H
[3]   Flame retardants for polypropylene based on lignin [J].
De Chirico, A ;
Armanini, M ;
Chini, P ;
Cioccolo, G ;
Provasoli, F ;
Audisio, G .
POLYMER DEGRADATION AND STABILITY, 2003, 79 (01) :139-145
[4]  
Dubois P, 1998, J MACROMOL SCI R M C, VC38, P511
[5]  
Gallo JB, 1998, POLIMEROS, V8, P23, DOI DOI 10.1590/S0104-14281998000100005
[6]   Compatibilization of polyethylene/aluminum hydroxide (PE/ATH) and polyethylene/magnesium hydroxide (PE/MH) composites with functionalized polyethylenes [J].
Hippi, U ;
Mattila, J ;
Korhonen, M ;
Seppälä, J .
POLYMER, 2003, 44 (04) :1193-1201
[7]   INTERFACIAL MODIFICATION OF POLYPROPYLENE COMPOSITES FILLED WITH MAGNESIUM-HYDROXIDE [J].
HORNSBY, PR ;
WATSON, CL .
JOURNAL OF MATERIALS SCIENCE, 1995, 30 (21) :5347-5355
[8]   An investigation into the decomposition and burning behaviour of Ethylene-vinyl acetate copolymer nanocomposite materials [J].
Hull, TR ;
Price, D ;
Liu, Y ;
Wills, CL ;
Brady, J .
POLYMER DEGRADATION AND STABILITY, 2003, 82 (02) :365-371
[9]   The effect of flame retardants on the flammability and mechanical properties of paper-sludge/phenolic composite [J].
Jang, JS ;
Chung, HS ;
Kim, M ;
Sung, HJ .
POLYMER TESTING, 2000, 19 (03) :269-279
[10]   Effect of morphological features and surface area of hydroxyapatite on the fatigue behavior of hydroxyapatite-polyethylene composites [J].
Joseph, R ;
Tanner, KE .
BIOMACROMOLECULES, 2005, 6 (02) :1021-1026