STUDY ON CORROSION BEHAVIOR OF HOT DIP COATINGS IN WET-DRY CYCLIC CONDITIONS

被引:0
作者
Xie, Bin [1 ,2 ]
Xing, Shaohua [2 ,3 ]
Chen, Jida [1 ]
Yan, Yonggui [2 ]
Li, Yan [3 ]
机构
[1] Chongqing Univ, Coll Chem & Chem Engn, Chongqing 630044, Peoples R China
[2] Luoyang Ship Mat Res Inst, Marine Corros & Protect Lab, Sci & Technol, Qingdao, Peoples R China
[3] China Univ Petr, Dept Mech & Mfg Engn, Qingdao, Peoples R China
来源
SENSORS, MEASUREMENT AND INTELLIGENT MATERIALS, PTS 1-4 | 2013年 / 303-306卷
关键词
hot dip coating; fastener coating; anticorrosion performance; wet-dry cyclic conditions; THIN ELECTROLYTE LAYERS; ATMOSPHERIC CORROSION; ELECTROCHEMICAL IMPEDANCE; GALVANIZED STEEL;
D O I
10.4028/www.scientific.net/AMM.303-306.2545
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion of fasteners in ballast tank is much serious, due to the wet-dry corrosive conditions. Now most fasteners are protected by zinc-aluminium coating. In order to evaluate the anticorrosion performance of hot dip Galvanized (GI), Galfan (GF) and Galvalume (GL) coated fasteners in wet-dry cyclic conditions, the corrosion behavior of these coatings in 1h wet and 7h drying condition were investigated by electrochemical impedance spectroscopy technology. The corrosion rate of GI coating in drying condition is much faster than that in wet condition before 23rd cycle, after that time the corrosion rate in sea water is faster than that in drying condition, however the corrosion rate of GF coatings in drying condition is much slower than that in wet condition, and for GL coating, the polarization resistance is both than 10(4)Omega.cm(2), whether it is immersed in seawater or in drying condition, which suggests it has better anticorrosion performance. The corrosion rate of the GI, GF and GL coating is 30 mu m per year, 1.5 mu m per year and 1.3 mu m per year respectively and corrosion resistance of GL and GF is therefore twenty two and twenty times as that of GI.
引用
收藏
页码:2545 / +
页数:3
相关论文
共 50 条
[31]   The inhibition effect of tannic acid on mild steel corrosion in seawater wet/dry cyclic conditions [J].
Qian, Bei ;
Hou, Baorong ;
Zheng, Meng .
CORROSION SCIENCE, 2013, 72 :1-9
[32]   Degradation mechanism of galvanized steel in wet-dry cyclic environment containing chloride ions [J].
Yadav, AP ;
Nishikata, A ;
Tsuru, T .
CORROSION SCIENCE, 2004, 46 (02) :361-376
[33]   Corrosion behavior of X65 pipeline steel: Comparison of wet-Dry cycle and full immersion [J].
Yu, Jianxing ;
Wang, Huakun ;
Yu, Yang ;
Luo, Zhen ;
Liu, Weidong ;
Wang, Caimei .
CORROSION SCIENCE, 2018, 133 :276-287
[34]   Pitting corrosion of sensitised type 304 stainless steel under wet-dry cycling condition [J].
Cheng, Cong-Qian ;
Klinkenberg, Laura-Isabell ;
Ise, Yaoki ;
Zhao, Jie ;
Tada, Eiji ;
Nishikata, Atsushi .
CORROSION SCIENCE, 2017, 118 :217-226
[35]   Growth Process of Passive Films on Austenitic Stainless Steels under Wet-dry Cyclic Condition [J].
Jung, Rock-Hoon ;
Tsuchiya, Hiroaki ;
Fujimoto, Shinji .
ISIJ INTERNATIONAL, 2012, 52 (07) :1356-1361
[36]   Effects of Rare Earth (Ce and La) on Steel Corrosion Behaviors under Wet-Dry Cycle Immersion Conditions [J].
Lian, Xintong ;
Zhu, Jianan ;
Wang, Ruiqian ;
Liu, Tengshi ;
Xu, Jing ;
Xu, Dexiang ;
Dong, Han .
METALS, 2020, 10 (09) :1-14
[37]   Stages and mechanism of Q420B hot-dip galvanized steel corrosion in simulated dry/wet coastal atmosphere [J].
Chu, Hongqiang ;
Zhai, Jiqiang ;
Guan, Yanjin ;
Chen, Fengjiao ;
Lin, Jun .
CORROSION SCIENCE, 2025, 245
[38]   Electrochemical noise study on 2024-T3 Aluminum alloy corrosion in simulated acid rain under cyclic wet-dry condition [J].
Shi, Yanyan ;
Zhang, Zhao ;
Su, Jingxin ;
Cao, Fahe ;
Zhang, Jianqing .
ELECTROCHIMICA ACTA, 2006, 51 (23) :4977-4986
[39]   Corrosion Behavior of Sn-Bearing Steel under Wet/Dry Cyclic Environments Containing Cl- [J].
Sugae, Kiyonobu ;
Kamimura, Takayuki ;
Miyuki, Hideaki ;
Kudo, Takeo .
MATERIALS TRANSACTIONS, 2018, 59 (05) :779-786
[40]   AC impedance monitoring of pitting corrosion of stainless steel under a wet-dry cyclic condition in chloride-containing environment [J].
Cruz, RPV ;
Nishikata, A ;
Tsuru, T .
CORROSION SCIENCE, 1996, 38 (08) :1397-1406