Recovery of Scratch Grooves in Ti-6Al-4V Alloy Caused by Reversible Phase Transformations

被引:15
作者
Shugurov, Artur R. [1 ]
Panin, Alexey V. [1 ,2 ]
Dmitriev, Andrey I. [1 ,3 ]
Nikonov, Anton Yu. [1 ,3 ]
机构
[1] RAS, ISPMS Inst Strength Phys & Mat Sci SB, Akad Pr 2-4, Tomsk 634055, Russia
[2] TPU Natl Res Tomsk Polytech Univ, Sch Nucl Sci & Engn, Lenin Av 30, Tomsk 634050, Russia
[3] TSU Tomsk State Univ, Dept Met Phys, Lenin Av 36, Tomsk 634050, Russia
基金
俄罗斯基础研究基金会;
关键词
Ti-6Al-4V; scratch testing; molecular dynamics; microstructure; phase transformations; MECHANICAL-PROPERTIES; TITANIUM-ALLOY; CRYSTALLOGRAPHIC ORIENTATION; WEAR; NANOINDENTATION; DEFORMATION; SIMULATIONS; CONTACT; SILICON; SURFACE;
D O I
10.3390/met10101332
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The deformation behaviors of Ti-6Al-4V alloy samples with lamellar and bimodal microstructures under scratch testing were studied experimentally and using molecular dynamics simulation. It was found that the scratch depth in the sample with a bimodal microstructure was twice as shallow as that measured in the sample with a lamellar microstructure. This effect is attributed to the higher hardness of the sample with a bimodal microstructure and the larger amount of elastic recovery of scratch grooves in this sample. On the basis of the results of molecular dynamics simulation, a mechanism was proposed, which associates the recovery of the scratch grooves with the inhomogeneous vanadium distribution in the beta-areas. The calculations showed that at a vanadium content typical for Ti-6Al-4V alloy, both the body-centered cubic (BCC) and hexagonal close-packed (HCP) structures can be more energetically favorable depending on the atomic volume. Therefore, compressive or tensile stresses induced by the indenter could facilitate beta ->alpha and alpha ->beta phase transformations, respectively, in the vanadium-depleted domains of the beta-areas, which contribute to the recovery of the Ti-6Al-4V alloy subjected to scratching.
引用
收藏
页码:1 / 14
页数:14
相关论文
共 50 条
  • [11] Phase transformations in the Ti-6Al-4V - Hydrogen system
    Qazi, JI
    Rahim, J
    Senkov, ON
    Patankar, SN
    Froes, FH
    ADVANCED MATERIALS FORUM I, 2002, 230-2 : 344 - 349
  • [12] Effect of Ultrasonic Impact Treatment on Structural Phase Transformations in Ti-6Al-4V Titanium Alloy
    Perevalova, O. B.
    Panin, A., V
    Kazachenok, M. S.
    Sinyakova, E. A.
    PHYSICAL MESOMECHANICS, 2022, 25 (03) : 248 - 258
  • [13] Decomposition of deformed α′(α") martensitic phase in Ti-6Al-4V alloy
    Motyka, Maciej
    Baran-Sadleja, Anna
    Sieniawski, Jan
    Wierzbinska, Malgorzata
    Gancarczyk, Kamil
    MATERIALS SCIENCE AND TECHNOLOGY, 2019, 35 (03) : 260 - 272
  • [14] Dry sliding wear behavior of Ti-6Al-4V alloy in vacuum
    Liu, Y
    Yang, DZ
    He, SY
    Wu, WL
    ACTA METALLURGICA SINICA, 2003, 39 (07) : 711 - 714
  • [15] Phase constituents and microhardness of laser alloyed Ti-6Al-4V alloy
    Adebiyi, D. I.
    Popoola, A. P. I.
    Pityana, S. L.
    JOURNAL OF LASER APPLICATIONS, 2015, 27
  • [16] STRUCTURE AND PITTING CORROSION OF Ti-6Al-4V ALLOY AND Ti-6Al-4V WELDS
    Ferdinandov, Nikolay Vasilev
    Gospodinov, Danail Dimitrov
    Ilieva, Mariana Dimitrova
    Radev, Rossen Hristov
    PROCEEDINGS OF THE 7TH INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND SYSTEMS, 2018, : 325 - 330
  • [17] Ti-6Al-4V alloy strengthening via instantaneous phase transformation induced by electropulsing
    Xu, Xiaofeng
    Yan, Xudong
    Qian, Yu
    Chong, Xueying
    Zhou, Yachong
    Zhao, Yuguang
    Yang, Xuehui
    Liu, Gaofeng
    Wu, Chao
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 899
  • [18] Texture Evolution in Warm Rolled Ti-6Al-4V Alloy
    Yang Huanping
    Wang Yaomian
    Li Zhiyang
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (09) : 2655 - 2660
  • [19] Electrochemical Polishing of Additively Manufactured Ti-6Al-4V Alloy
    Zhang, Yifei
    Li, Jianzhong
    Che, Shuanghang
    Tian, Yanwen
    METALS AND MATERIALS INTERNATIONAL, 2020, 26 (06) : 783 - 792
  • [20] Robotic Nd:YAG Fiber Laser Welding of Ti-6Al-4V Alloy
    Kose, Ceyhun
    Karaca, Engin
    METALS, 2017, 7 (06):