Effect of tension on corrosive and thermal properties of Cu60Zr30Ti10 metallic glass

被引:9
作者
An, W. K. [1 ]
Cai, A. H. [1 ,2 ]
Xiong, X. [2 ]
Liu, Y. [2 ]
Zhou, G. J. [1 ]
Luo, Y. [1 ]
Li, T. L. [1 ]
Li, X. S. [1 ]
机构
[1] Hunan Inst Sci & Technol, Coll Mech Engn, Yueyang 414000, Peoples R China
[2] Cent S Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
关键词
Cu60Zr30Ti10 metallic glasses; Thermal property; Corrosion; CU-ZR-TI; MECHANICAL-PROPERTIES; FORMING ABILITY; CHLORIDE MEDIA; BEHAVIOR; RESISTANCE; ALLOY; STRESS; HF; PLASTICITY;
D O I
10.1016/j.jallcom.2013.01.187
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Cu60Zr30Ti10 (at.%) glassy ribbon was prepared by melt spinning. The effect of the tension on its thermal and corrosive properties was investigated by differential scanning calorimetry and electrochemical polarization experiments, respectively. The glass transition temperature T-g, onset crystallization temperature T-x, and crystallization peak temperature T-p increase with increasing heating rate, but the increasing rate of these temperatures is larger for low heating rate (5-20 K min(-1)) than for rapid heating rate (20-80 K min(-1)) for the as-cast and tensile ribbons. The T-g for the tensile ribbon is smaller than that for the as-cast one in studied heating rates. The T-x and the T-p for the tensile ribbon are smaller than those for the a-cast ribbon when the heating rate is less than 80 K min(-1), while inversely when the heating rate reaches up to 80 K min(-1). There is a critical heating rate for the characteristic temperatures of the tensile ribbon surpassing those of the as-cast one. The heating rates are estimated to be 114.7 K min(-1) for T-g, 65.3 K min(-1) for T-x, and 64.9 K min(-1) for T-p, respectively. In addition, the activation energies for the glass transition and the crystallization decrease. On the other hand, the corrosion potential is larger in 0.5 M H2SO4 than in 1 M chloride-ion-containing solutions for the as-cast and tensile specimens. However, the corrosion current density is smaller in the former than in the latter for the tensile and as-cast specimens. After the tension, the corrosion potential sharply increases in 0.5 M H2SO4 and decreases in 1 M chloride-ion-containing solutions. The passive potential decreases and the pitting corrosion can be observed in 0.5 M H2SO4. The potential for the sharp decrease of the current density decreases in 1 M HCl, and maintains almost the same in 1 M NaCl. The corroded surface micrographs in all studied solutions are remarkably changed. In addition, the difference of corrosive behavior in 0.5 M H2SO4, 1 M HCl, and 1 M NaCl is also discussed. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:55 / 62
页数:8
相关论文
共 50 条
  • [41] High thermal stability of the amorphous oxide in Ti44.5Cu44.5Zr7Be4 metallic glass
    Park, Sung Hyun
    Lim, Ka Ram
    Na, Min Young
    Kim, Kang Cheol
    Kim, Won Tae
    Kim, Do Hyang
    AIP ADVANCES, 2015, 5 (11):
  • [42] Improving plasticity of the Zr46Cu46Al8 bulk metallic glass via thermal rejuvenation
    Song, Wenli
    Meng, Xiaohe
    Wu, Yuan
    Cao, Di
    Wang, Hui
    Liu, Xiongjun
    Wang, Xianzhen
    Lu, Zhaoping
    SCIENCE BULLETIN, 2018, 63 (13) : 840 - 844
  • [43] Effect of Cold Rolling on Thermal Stability of Zr55Al10Ni5Cu30 Bulk Metallic Glass
    Hu, Manhong
    Hu, Yong
    ADVANCED MATERIALS, PTS 1-4, 2011, 239-242 : 490 - +
  • [44] Effect of Al Addition on the Mechanical Properties and Microstructure of Zr35Ti30Cu7.5Be27.5 Bulk Metallic Glass
    Zong Haitao
    Ma Mingzhen
    Li Lixin
    Jing Qin
    Zhang Baoqing
    Liu Riping
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 (03) : 470 - 473
  • [45] Crystallization kinetics of Cu60Zr25Ti15 and (Cu60Zr25Ti15)95Ni5 bulk metallic glasses by differential scanning calorimetry (DSC)
    Mandal, Soumen
    Lee, Dong-Eun
    Park, Taejoon
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2021, 145 (02) : 467 - 474
  • [46] Enhanced mechanical properties and in vitro corrosion behavior of amorphous and devitrified Ti40Zr10Cu38Pd12 metallic glass
    Fornell, J.
    Van Steenberge, N.
    Varea, A.
    Rossinyol, E.
    Pellicer, E.
    Surinach, S.
    Baro, M. D.
    Sort, J.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2011, 4 (08) : 1709 - 1717
  • [47] Crystallization of Cu60Zr20Ti20 bulk metallic glass by high pressure torsion
    Revesz, Adam
    Horvath, Andras
    Ribarik, Gabor
    Schafler, Erhard
    Browne, David J.
    Kovacs, Zsolt
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2019, 58 (01) : 304 - 312
  • [48] Microstructure and Mechanical Properties of Cu-Zr-Al Bulk Metallic Glass with Addition of Co
    Zhou, Wei
    Tao, Yiming
    Liu, Li
    Kong, Lingti
    Li, Jinfu
    Zhou, Yaohe
    MATERIALS TRANSACTIONS, 2013, 54 (03) : 286 - 290
  • [49] The Effect of Er Addition on the Air-Oxidation of a Zr55Cu30Al10Ni5-Based Bulk Metallic Glass
    Kai, W.
    Ren, I. F.
    Chen, W. S.
    Kao, P. C.
    Huang, R. T.
    Xing, D.
    Liaw, P. K.
    OXIDATION OF METALS, 2014, 81 (3-4): : 453 - 465
  • [50] Effect of thermal cycling on the mechanical properties of Zr41Ti14Cu12.5Ni10Be22.5 alloy
    Wang Xin
    Shao Yang
    Gong Pan
    Yao KeFu
    SCIENCE CHINA-PHYSICS MECHANICS & ASTRONOMY, 2012, 55 (12) : 2357 - 2361