Creep deformation and its correspondence to the microstructure of different polyester industrial yarns at room temperature

被引:25
作者
Chen, Kang [1 ]
Yu, Jinchao [1 ]
Liu, Yanping [2 ]
Song, Minggen [3 ]
Jiang, Quan [3 ]
Ji, Hong [1 ]
Zou, Jiaxiong [1 ]
Zhang, Yumei [1 ]
Wang, Huaping [1 ]
机构
[1] Donghua Univ, Coll Mat Sci & Engn, State Key Lab Modificat Chem Fibers & Polymer Mat, Shanghai 201620, Peoples R China
[2] Donghua Univ, Coll Text, Engn Res Ctr Tech Text, Shanghai, Peoples R China
[3] Zhejiang Unifull Ind Fiber Co Ltd, Huzhou City, Zhejiang, Peoples R China
关键词
poly(ethylene terephthalate) industrial yarn; microstructure; creep mechanism; WAXS; SAXS; X-RAY-SCATTERING; SIMULTANEOUS SMALL-ANGLE; POLYETHYLENE TEREPHTHALATE; STRUCTURAL-CHANGES; FIBERS; CRYSTALLINE; MORPHOLOGY; ORIENTATION; DIFFRACTION; PERFORMANCE;
D O I
10.1002/pi.5745
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The room temperature creep behaviors and related microstructural changes of a high-tenacity (HT) poly(ethylene terephthalate) (PET) industrial yarn and a super-low-shrinkage (SLS) PET industrial yarn were investigated and compared by using wide-angle X-ray scattering (WAXS), small-angle X-ray scattering (SAXS), birefringence measurements and Fourier transform infrared spectroscopy (FTIR) in order to identify their respective underlying creep mechanisms. The crystal structure including crystalline orientation and crystallinity of fibers did not show obvious changes after the creep process, while the amorphous structures varied with creep stress. The HT yarn creep deformation was mainly elastic, and its creep recovery ratio was high. The amorphous orientation, amorphous layer thickness and degree of conformation change from gauche to trans conformers showed a slight increase. The mechanism of this slight change is that the coiled molecular chains are oriented under tensile loading and most of the extended chains are disoriented under offloading in the small amorphous region. By contrast, the SLS yarn underwent plastic creep deformation with a low recovery ratio. After the creep test, the amorphous orientation and lamellar thickness both increased but the crystallinity remained unchanged. The creep mechanism for the SLS yarn is that the molecular chains in the large amorphous domain are easily extended and oriented subjected to tensile loading, while conformation transition from gauche to trans conformers and the formation of irreversible mesophase take place. (c) 2018 Society of Chemical Industry
引用
收藏
页码:555 / 563
页数:9
相关论文
共 40 条
  • [21] Effect of deformation ratios on microstructure and mechanical properties of ZK60 magnesium alloy by hydrostatic extruded at room temperature
    Wang Rong
    Zhu Xiu-rong
    Chen Gang
    Nie Jing-jiang
    Xu Yongdong
    Wang Jun
    Yang Bo
    ADVANCED MATERIALS AND PROCESSES II, PTS 1-3, 2012, 557-559 : 13 - +
  • [22] Microstructure and Room Temperature Compressive Deformation Behavior of Cold-Sprayed High-Strength Cu Bulk Material
    Kim, Young-Kyun
    Kim, Kyu-Sik
    Kim, Hyung-Jun
    Park, Chan-Hee
    Lee, Kee-Ahn
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2017, 26 (07) : 1498 - 1508
  • [23] Microstructure and Room Temperature Compressive Deformation Behavior of Cold-Sprayed High-Strength Cu Bulk Material
    Young-Kyun Kim
    Kyu-Sik Kim
    Hyung-Jun Kim
    Chan-Hee Park
    Kee-Ahn Lee
    Journal of Thermal Spray Technology, 2017, 26 : 1498 - 1508
  • [24] Microstructure of MgAl5Ca3Sr alloy after creep deformation and high-temperature heat treatment
    Rzychon, T.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2014, 45 (05) : 344 - 353
  • [25] Microstructure and deformation behavior of extruded 7A43 alloy in solid solution state under room temperature compression
    Shao, Hongbang
    Huang, Yuanchun
    Wang, Duanzhi
    Guo, Xiaofang
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2023, 51 (05): : 76 - 86
  • [26] Microstructure Stability of 4th Generation Single Crystal Superalloy, PWA 1497, during High Temperature Creep Deformation
    Zietara, Maciej
    Cetel, Alan
    Czyrska-Filemonowicz, Aleksandra
    MATERIALS TRANSACTIONS, 2011, 52 (03) : 336 - 339
  • [27] Deformation and damage mechanisms in an α/β 6242 Ti alloy in fatigue, dwell-fatigue and creep at room temperature. Influence of internal hydrogen
    Gerland, M.
    Lefranc, P.
    Doquet, V.
    Sarrazin-Baudoux, C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 507 (1-2): : 132 - 143
  • [28] Microstructure and Room Temperature Mechanical Properties of Different 3 and 4 Element Medium Entropy Alloys from HfNbTaTiZr System
    Zyka, Jiri
    Malek, Jaroslav
    Vesely, Jaroslav
    Lukac, Frantisek
    Cizek, Jakub
    Kuriplach, Jan
    Melikhova, Oksana
    ENTROPY, 2019, 21 (02)
  • [29] Microstructure evolution and accelerated magnetocaloric phase formation of LaFe13.1Co0.7Si1.4 alloy by forging deformation at room temperature
    Chen, RuZhao
    Fu, Bin
    Zhang, Hu
    Hu, Jie
    Yang, Xu
    Zhang, LianQi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 925
  • [30] Synthesis of a New Polycarboxylate at Room Temperature and Its Influence on the Properties of Cement Pastes with Different Supplementary Cementitious Materials
    Xiang, Shuncheng
    Gao, Yingli
    Shi, Caijun
    ADVANCES IN CIVIL ENGINEERING, 2020, 2020