Mechanical properties and in vitro degradation of electrospun bio-nanocomposite mats from PLA and cellulose nanocrystals
被引:179
作者:
Shi, Qingfeng
[1
,2
]
Zhou, Chengjun
[1
]
Yue, Yiying
[1
]
Guo, Weihong
[2
]
Wu, Yiqiang
[3
]
Wu, Qinglin
[1
]
机构:
[1] Louisiana State Univ, Ctr Agr, Sch Renewable Nat Resource, Baton Rouge, LA 70803 USA
[2] E China Univ Sci & Technol, Sch Mat Sci & Engn, Shanghai 200237, Peoples R China
[3] Cent S Univ Forestry & Technol, Coll Mat Sci & Engn, Changsha 410004, Hunan, Peoples R China
关键词:
Electrospinning;
Cellulose nanocrystals;
Nanocomposites;
Poly(lactic acid) (PLA);
In vitro degradation;
POLY(LACTIC ACID);
LACTIC-ACID;
FIBERS;
NANOFIBER;
CHEMISTRY;
BEHAVIOR;
BLENDS;
STARCH;
D O I:
10.1016/j.carbpol.2012.05.042
中图分类号:
O69 [应用化学];
学科分类号:
081704 ;
摘要:
Fibrous bio-nanocomposite mats consisting of cellulose nanocrystals (CNCs) and poly(lactic acid) (PIA) were electrospun from a solvent mixture consisting of N,N'-dimethylformamide and chloroform at room temperature. Morphological, mechanical and thermal properties, as well as in vitro degradation of nanocomposite mats were characterized as a function of material composition. Average diameter of the electrospun fibers decreased with increased CNC-loading level. Thermal stability, and tensile strength and modulus of nanocomposite mats were effectively improved by the addition of CNCs up to the 5 wt% level. The reinforcement of CNCs on electrospun mats was illustrated by the observation of SEM-based morphologies on the tensile fracturing process of nanocomposite mats. At the CNC content of 5 wt%, the maximum tensile stress and Young's modulus of the nanocomposite mats increased by 5 and 22 folds than those of neat PEA mats, respectively. Moreover, compared with neat PEA mats, the nanocomposite mats, especially at high CNC-loading levels, degraded more rapidly in phosphate-buffered saline solution. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:301 / 308
页数:8