HYDROGEN EMBRITTLEMENT OF THE LOW-CARBON STEEL PRODUCED BY ELECTRON BEAM ADDITIVE MANUFACTURING

被引:3
作者
Panchenko, M. Yu. [1 ]
Melnikov, E. V. [1 ]
Astafurov, S. V. [1 ]
Reunova, K. A. [1 ]
Kolubaev, E. A. [1 ]
Astafurova, E. G. [1 ]
机构
[1] Russian Acad Sci, Inst Strength Phys & Mat Sci, Siberian Branch, Tomsk, Russia
关键词
additive technologies; low-carbon steel; hydrogen embrittlement; fracture; MICROSTRUCTURE; DEFORMATION; CORROSION; FRACTURE; PROGRESS;
D O I
10.1007/s11182-022-02720-3
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
The effect of cathodic hydrogen charging of the Fe-(1.8-2.1)Mn-(0.7-1.0)Si-(0.05-0.11)C low-carbon steel, produced by electron-beam additive manufacturing and industrial casting, on its mechanical properties and fracture mechanisms is studied in different electrolytic solutions. Hydrogen charging causes an increase in the yield strength and a decrease in the elongation both for the steel manufactured by the additive method (ferritic steel) and for the normalized steel produced by the industrial method (ferritic-pearlitic steel). An increased duration of hydrogen charging from 5 to 20 hours at a current density of j(H) = 250 mA/cm(2) (NaCl+NH4SCN aqueous solution) is accompanied by an increase of the hydrogen embrittlement index for the additively produced specimens (I-H(5h) = 13%, I-H(20h) = 19%), but does not affect the I-H-value for the normalized industrial steel (I-H(5h) = 28%, I-H(20h) = 30%). Even at a lower current density and a shorter charging duration, the use of an aqueous solution of sulfuric acid (H2SO4+CH4N2S) causes stronger hydrogen-induced effects than the charging in an aqueous solution of sodium chloride. Regardless of the manufacturing method and charging regime, hydrogen charging contributes to the formation of fish-eye defects on the fracture surfaces of steels. It is found out that under similar hydrogen charging regimes, the deteriorative effect of hydrogen is less pronounced in the steel produced by the additive manufacture.
引用
收藏
页码:966 / 974
页数:9
相关论文
共 29 条
  • [21] On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels
    Martin, May L.
    Fenske, Jamey A.
    Liu, Grace S.
    Sofronis, Petros
    Robertson, Ian M.
    [J]. ACTA MATERIALIA, 2011, 59 (04) : 1601 - 1606
  • [22] X-RAY CHARACTERIZATION OF ERODED 316 STAINLESS-STEEL
    NAIDU, SVN
    SINGH, T
    [J]. WEAR, 1993, 166 (02) : 141 - 145
  • [23] Additive manufacturing (3D printing): A review of materials, methods, applications and challenges
    Ngo, Tuan D.
    Kashani, Alireza
    Imbalzano, Gabriele
    Nguyen, Kate T. Q.
    Hui, David
    [J]. COMPOSITES PART B-ENGINEERING, 2018, 143 : 172 - 196
  • [24] Environmental Behavior of Low Carbon Steel Produced by a Wire Arc Additive Manufacturing Process
    Ron, Tomer
    Levy, Galit Katarivas
    Dolev, Ohad
    Leon, Avi
    Shirizly, Amnon
    Aghion, Eli
    [J]. METALS, 2019, 9 (08)
  • [25] HVEM STUDIES OF THE EFFECTS OF HYDROGEN ON THE DEFORMATION AND FRACTURE OF AISI TYPE 316 AUSTENITIC STAINLESS-STEEL
    ROZENAK, P
    ROBERTSON, IM
    BIRNBAUM, HK
    [J]. ACTA METALLURGICA ET MATERIALIA, 1990, 38 (11): : 2031 - 2040
  • [26] Song J, 2013, NAT MATER, V12, P145, DOI [10.1038/NMAT3479, 10.1038/nmat3479]
  • [27] Anisotropic mechanical properties and deformation behavior of low-carbon high-strength steel component fabricated by wire and arc additive manufacturing
    Sun, Laibo
    Jiang, Fengchun
    Huang, Ruisheng
    Yuan, Ding
    Guo, Chunhuan
    Wang, Jiandong
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 787
  • [28] Microstructural evolution and chemical corrosion of electron beam wire-feed additively manufactured AISI 304 stainless steel
    Tarasov, S. Yu
    Filippov, A., V
    Shamarin, N. N.
    Fortuna, S., V
    Maier, G. G.
    Kolubaev, E. A.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 803 : 364 - 370
  • [29] Effects of ferrite/pearlite alignment on the hydrogen permeation in a AISI 4130 steel
    Tau, L
    Chan, SLI
    [J]. MATERIALS LETTERS, 1996, 29 (1-3) : 143 - 147