Fabrication of Al-20 wt%Si powder using scrap Si by ultra high-energy milling process

被引:25
|
作者
Kang, Won-Kyung [1 ,2 ]
Yilmaz, Fikret [3 ]
Kim, Hyo-Seob [1 ,2 ]
Koo, Jar-Myung [1 ,2 ]
Hong, Soon-Jik [1 ,2 ]
机构
[1] Kongju Natl Univ, Div Adv Mat Engn, Cheonan 330717, Chungnam, South Korea
[2] Kongju Natl Univ, Inst Rare Met, Cheonan 330717, Chungnam, South Korea
[3] Gaziosmanpasa Univ, Fac Art & Sci, Dept Phys, TR-60240 Tokat, Turkey
关键词
Ultra-high energy ball milling; Milling time; Al-20Si; Microstructure; Mechanical properties; MECHANICAL-PROPERTIES; ALLOY; BEHAVIOR;
D O I
10.1016/j.jallcom.2012.01.106
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, microstructural evolution and mechanical properties of Al-20 wt%Si and pure Al powders fabricated by ultra high-energy ball milling technique were investigated as a function of milling time. The microstructure and mechanical properties of the as-milled powders were examined by scanning electron microscope (SEM), energy dispersive spectrometry (EDS), X-ray diffractometer (XRD) and Vickers hardness tester. SEM observation showed that the particle size increased at an early stage of milling, and then decreased drastically with further milling. XRD and cross-sectional EDS-mapping analyses revealed that Si particles were not dissolved but uniformly dispersed in the Al matrix in a milled state. Vickers hardness of both pure Al and Al-Si powder increases with milling time, which attributes to the grain size strengthening and dispersion strengthening. (c) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:S45 / S49
页数:5
相关论文
共 50 条
  • [1] Production of Al-20 wt.% Al2O3 composite powder using high energy milling
    Tousi, S. S. Razavi
    Rad, R. Yazdani
    Salahi, E.
    Mobasherpour, I.
    Razavi, M.
    POWDER TECHNOLOGY, 2009, 192 (03) : 346 - 351
  • [2] Influence of high-energy ball milling on Al-30Si powder and ceramic particulate
    Li, Yuan-Yuan
    Zhang, Da-Tong
    Xiao, Zhi-Yu
    Ngai, Tungwai Leo
    Transactions of Nonferrous Metals Society of China (English Edition), 2000, 10 (03): : 324 - 327
  • [3] Influence of high-energy ball milling on Al-30Si powder and ceramic particulate
    Li, YY
    Zhang, DT
    Xiao, ZY
    Ngai, TL
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2000, 10 (03) : 324 - 327
  • [4] Effects of Cr and Cooling Rate on Segregation and Refinement of Primary Si in Al-20 WT %Si Alloy
    Kesheng S. Zuo
    Haitao T. Zhang
    Xing Han
    Hailong L. Jia
    Ke Qin
    Jianzhong Z. Cui
    International Journal of Metalcasting, 2014, 8 : 55 - 62
  • [5] EFFECTS OF Cr AND COOLING RATE ON SEGREGATION AND REFINEMENT OF PRIMARY Si IN Al-20 WT %Si ALLOY
    Zuo, Kesheng S.
    Zhang, Haitao T.
    Han, Xing
    Jia, Hailong L.
    Qin, Ke
    Cui, Jianzhong Z.
    INTERNATIONAL JOURNAL OF METALCASTING, 2014, 8 (04) : 55 - 62
  • [6] Effect of Sr on the Microstructure and Properties of Hypereutectic Al-20 wt% Si Alloy
    Li, Xiaosong
    Cai, Anhui
    Liu, Gang
    Zhou, Yong
    Zeng, Jijie
    ADVANCES IN SUPERALLOYS, PTS 1 AND 2, 2011, 146-147 : 454 - +
  • [7] Effects of Cr and cooling rate on segregation and refinement of primary Si in Al-20 Wt %Si alloy
    1600, American Foundry Society, 1695 North Penny Lane, Schaumburg, IL 60173-4555, United States (08):
  • [8] Mechanical properties and fracture mechanism of nanostructured Al-20 wt% Si alloy
    Hong, SJ
    Suryanarayana, C
    PROCESSING AND PROPERTIES OF STRUCTURAL NANOMATERIALS, 2003, : 133 - 140
  • [9] Fabrication of Al-7wt%Si-0.4wt%Mg/SiC nanocomposite powders and bulk nanocomposites by high energy ball milling and powder metallurgy
    Woo, KD
    Zhang, DL
    CURRENT APPLIED PHYSICS, 2004, 4 (2-4) : 175 - 178
  • [10] Enhanced nucleation of primary silicon in Al-20 wt. % Si alloy with Ni-Si inoculation
    Yu, Wenhui
    Zhang, Yong
    Yan, Tingliang
    Liu, Yue
    Jiang, Aolei
    Zheng, Hongliang
    Tian, Xuelei
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 693 : 303 - 307