An experimental study of recovery in embossing of polycarbonate below the glass transition temperature

被引:3
|
作者
Wang, Jin [1 ,2 ,3 ]
Deng, Yujun [1 ]
Yi, Peiyun [1 ]
Peng, Linfa [1 ]
Lai, Xinmin [1 ,4 ]
机构
[1] Shanghai Jiao Tong Univ, State Key Lab Mech Syst & Vibrat, Shanghai 200240, Peoples R China
[2] South China Univ Technol, Natl Engn Res Ctr Novel Equipment Polymer Proc, Guangzhou 510640, Peoples R China
[3] South China Univ Technol, Minist Educ, Key Lab Polymer Proc Engn, Guangzhou 510640, Peoples R China
[4] Shanghai Jiao Tong Univ, Shanghai Key Lab Digital Manufacture Thin Walled, Shanghai 200240, Peoples R China
基金
中国国家自然科学基金;
关键词
embossing; polycarbonate; below Tg; recovery; loading rate; MICROFLUIDIC DEVICES; POLYMER DEFORMATION; HOT; NANOIMPRINT; FABRICATION; MICROSTRUCTURES; POLYSTYRENE; EXTENSION; FIDELITY; BEHAVIOR;
D O I
10.1088/1361-6439/ab931c
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The hot embossing process is a cost-effective replication technology for the fabrication of polymeric micro/nano-structures. Nevertheless, there is a need to reduce the embossing temperature as industrial applications of the hot embossing process are limited by the high temperature required. For amorphous thermoplastic polymers, the hot embossing process can be conducted below the polymer's glass transition temperature (Tg), which is promising for many industrial applications. However, it is generally difficult to achieve a high replication fidelity in such a below-Tg embossing process. The large resistance to plastic flow and the significant deformation recovery of the glassy polymer (the amorphous thermoplastic polymer in its glassy state) are two main causes. The problem of plastic flow may be solved by designing and developing a hot embossing system with large force capability, but the recovery problem may not and needs further study. In this research, the recovery of a polycarbonate (PC) glass in the below-Tg embossing process was quantified and investigated systematically. The effects of embossing depth, holding time, temperature, and loading rate on the recovery were discussed and analyzed. The research results reveal that it is the recovery (usually more than 20%) that severely limits the replication fidelity of the below-Tg embossing process. The recovery is strain-dependent due to the strain-dependent chain tension of the PC glass. As the chain tension generated in the strain-hardening region cannot be effectively reduced by increasing the embossing force, holding time, and temperature, the recovery problem poses a great challenge to be overcome. Considering the strain-rate dependence of the segmental mobility of glassy polymers, a strategy of increasing the loading rate to reduce the recovery was proposed and verified. Hence, this research advances our understanding of the below-Tg embossing process and provides new insights into how to improve the hot embossing process.
引用
收藏
页数:11
相关论文
共 50 条
  • [11] Theoretical and Experimental Investigation of Shape Memory Polymers Programmed below Glass Transition Temperature
    Shahi, Kartikey
    Ramachandran, Velmurugan
    POLYMERS, 2022, 14 (13)
  • [12] Physical aging of polycarbonate far below the glass transition temperature:: Evidence for the diffusion mechanism -: art. no. 224213
    Cangialosi, D
    Wübbenhorst, M
    Groenewold, J
    Mendes, E
    Schut, H
    van Veen, A
    Picken, SJ
    PHYSICAL REVIEW B, 2004, 70 (22): : 224213 - 1
  • [13] Excitations and structure above and below the glass transition temperature
    Keys, Aaron S.
    Chandler, David
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2012, 244
  • [14] Viscosity of glasses near and below the glass transition temperature
    Kobayashi, H
    Takahashi, H
    Hiki, Y
    JOURNAL OF APPLIED PHYSICS, 2000, 88 (06) : 3776 - 3778
  • [15] Viscosity and relaxation of glasses below the glass transition temperature
    Koide, M
    Sato, R
    Komatsu, T
    Matusita, K
    THERMOCHIMICA ACTA, 1996, 280 : 401 - 415
  • [16] Recovery of amorphous poly(ethylene terephthalate) film uniaxially drawn just below the glass transition temperature
    Sun, Nan-Jian
    Yang, Juan
    Shen, De-Yan
    Qian, Ren-Yuan
    Chinese Journal of Polymer Science (English Edition), 2000, 18 (01): : 69 - 75
  • [17] Recovery of amorphous poly(ethylene terephthalate) film uniaxially drawn just below the glass transition temperature
    Sun, NJ
    Yang, J
    Shen, DY
    Qian, RY
    CHINESE JOURNAL OF POLYMER SCIENCE, 2000, 18 (01) : 69 - 75
  • [18] Permanent deformation in Armos fibre at a temperature below the glass transition temperature
    Tsobkallo, ES
    Nachinkin, OI
    Kvartskheliya, VA
    FIBRE CHEMISTRY, 1999, 31 (03) : 215 - 218
  • [19] Permanent deformation in armos fibre at a temperature below the glass transition temperature
    E. S. Tsobkallo
    O. I. Nachinkin
    V. A. Kvartsheliya
    Fibre Chemistry, 1999, 31 : 215 - 218
  • [20] RECOVERY OF AMORPHOUS POLY(ETHYLENE TEREPHTHALATE)FILM UNIAXIALLY DRAWN JUST BELOW THE GLASS TRANSITION TEMPERATURE
    Nan-jian Sun
    Juan Yang
    De-yan Shen
    Ren-yuan Qian Institute of Chemistry