摘要
The effect of cerium on Al-Zn alloys with T6 and T5 treatments was investigated for mechanical and impact properties. Alloys were prepared by controlled melting and casting. The cast alloys were solution heat treated at 500-550 degrees C, for up to 24 h, followed by artificial aging at 165 degrees C for 6 h (T6). The T5 type temper was produced merely by applying a precipitation treatment to the as-cast castings, without previous solution treatment. All the tests were conducted according to ASTM standards. From the investigation, it was found that there was an improvement in mechanical and impact properties. Scanning electron microscopy was carried out to characterize the structural properties of different heat treatments and the effect of cerium. In addition, the fractured specimens were examined using a scanning electron microscopy in order to clarify fracture. Crown Copyright (C) 2009 Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:S24 / S29
页数:6
相关论文
共 30 条
[1]  
ASM Handbook, 1990, ASM HDB PROP SEL NON, V2, P291
[2]  
ASM publications. ASM International, 2007, JPED, V28, P453
[3]   Devitrification of Al-Ni-rare earth amorphous alloys [J].
Battezzati, L ;
Kusy', M ;
Rizzi, P ;
Ronto', V .
JOURNAL OF MATERIALS SCIENCE, 2004, 39 (12) :3927-3934
[4]  
Belov N. A., 1996, Journal of Advanced Materials, V3, P228
[5]   The ternary Al-Ce-Cu phase diagram in the aluminum-rich corner [J].
Belov, N. A. ;
Khvan, A. V. .
ACTA MATERIALIA, 2007, 55 (16) :5473-5482
[6]  
Belov NA, 1996, MATER SCI FORUM, V217, P222
[7]  
Belov NA, 1991, MAT SCI ENG A-STRUCT, VA271, P134
[8]  
Belov NA, 2002, ADV METALL ALLOYS, P342
[9]   Refinement of cast microstructure of hypereutectic Al-Si alloys through the addition of rare earth metals [J].
Chang, JY ;
Moon, IG ;
Choi, CS .
JOURNAL OF MATERIALS SCIENCE, 1998, 33 (20) :5015-5023
[10]   Structure of rapidly solidified aluminum alloys [J].
Dobatkin, VI ;
Elagin, VI ;
Fedorov, VM .
ADVANCED PERFORMANCE MATERIALS, 1995, 2 (01) :89-98