Microwave dielectric properties of rubber compounds undergoing vulcanisation - Part 1. Natural rubber with and without carbon black filler

被引:0
作者
Bovtun, V
Stark, W
Kelm, J
Porokhonskyy, V
Yakimenko, Y
机构
[1] Fed Inst Mat Res & Testing, BAM 5 2, Lab Tech Elastomers & Reference Mat, D-12205 Berlin, Germany
[2] Natl Tech Univ Ukraine, Kiev Polytech Inst, Kiev, Ukraine
[3] Acad Sci Czech Republ, Inst Phys, Prague, Czech Republic
来源
KAUTSCHUK GUMMI KUNSTSTOFFE | 2001年 / 54卷 / 12期
关键词
dielectric parameters; microwave methods; vulcanisation; elastomers; monitoring;
D O I
暂无
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The application of microwave measurements to the characterisation of rubber compounds vulcanisation is considered. The change of mechanical and microwave (20 GHz) dielectric parameters during vulcanisation was measured for three kinds of compounds: pure natural rubber, a compound with vulcanisation system and the corresponding compound containing carbon black. Changes of microwave dielectric permittivity and loss, probably caused by the change of concentration of the polar molecules and groups during vulcanisation, were detected. The difference in behaviour between unvulcanised and vulcanised compounds was clearly seen. Our study proves that microwave dielectric measurements are a highly sensitive and informative tool for following and monitoring the progress of vulcanisation reactions.
引用
收藏
页码:673 / +
页数:5
相关论文
共 14 条
  • [1] BOSTROM S, 1959, KAUTSCHUK HDB, V1, P100
  • [2] BOVTOUN VP, 1997, P INT C DIEL INS BUD, P59
  • [3] BOVTOUN VP, 1995, P S KER SCHIHT KOBL, P270
  • [4] BOVTUN V, 2001, IN PRESS MATERIALPRU, V43
  • [5] Grigas J., 1996, Microwave Dielectric Spectroscopy of Ferroelectrics and Related Materials
  • [6] Hamed G, 1992, ENG RUBBER, P11
  • [7] HEDVIG P, 1991, APPL POLYM ANAL CHAR, V2, P131
  • [8] HIPPEL A, 1959, DIELECTRICS THEIR AP
  • [9] Kelm J, 1998, KAUT GUMMI KUNSTST, V51, P364
  • [10] MCCRUM NG, 1967, ANELASTIC DIELECTRIC