High-temperature material degradation of Q345 cold-formed steel during full-range compartment fires

被引:27
作者
Chen, Wei [1 ,2 ]
Ye, Jihong [1 ]
Jin, Lei [1 ]
Jiang, Jian [1 ]
Liu, Kun [1 ]
Zhang, Meng [1 ]
Chen, Wenwen [3 ]
Zhang, Hua [4 ]
机构
[1] China Univ Min & Technol, Jiangsu Key Lab Environm Impact & Struct Safety E, Xuzhou 221116, Jiangsu, Peoples R China
[2] China Univ Min & Technol, Xuzhou Key Lab Fire Safety Engn Struct, Xuzhou 221116, Jiangsu, Peoples R China
[3] Southeast Univ, Sch Civil Engn, Nanjing 210096, Peoples R China
[4] Huzhou Univ, Dept Architecture, Huzhou 313000, Peoples R China
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
Rising and falling temperature periods; Cold-formed steel; Full-range compartment fire; Degradation law; Maximum temperature influence coefficient; MECHANICAL-PROPERTIES; STAINLESS-STEEL; WALLS; RESISTANCE; BEHAVIOR; PERFORMANCE;
D O I
10.1016/j.jcsr.2020.106366
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
High-temperature material properties are the most important input parameters for the study of the fire resistance of steel structures. Meanwhile, the structural failure of steel structures might occur during compartment fires. This paper presents steady-state experiments on Q345 cold-formed steel (CFS) during the rising and falling temperature periods. The results show that whether in the rising or falling temperature periods, the material properties of Q345 CFS decrease as the load testing temperature increases. Meanwhile, the difference between the test results of the rising and falling temperature periods can not be ignored. Under the same load testing temperatures, the differences in the elastic modulus reduction factors of Q345 CFS between the rising and falling temperature periods are within -0.16 to 0.057; meanwhile, the differences in the yield strength reduction factors between the rising and falling temperature periods are within -0.009 to 0.142. For the fire resistance design, if the material properties during the rising temperature period are used to replace those during the falling temperature period, the calculation results of the fire-induced deformation for Q345 CFS members may be conservative, but the corresponding high temperature bearing capacity will be over-predicted. In addition, the differences in the reduction factors of material properties for Q345 CFS caused by the maximum temperature are significantly lower than those for G550 CFS. Finally, a maximum temperature influence coefficient is introduced and unified expressions are put forward, which can be appropriately used to predict the material properties and stress-strain curves of Q345 CFS during full-range compartment fires. (C) 2020 Elsevier Ltd. All rights reserved.
引用
收藏
页数:18
相关论文
共 44 条
[1]  
AFNOR, 2000, ISO 15671 RUBBER RUB
[2]  
Alfawakhiri F., 2001, THESIS
[3]  
[Anonymous], 11 INT
[4]  
[Anonymous], 2016, AS41001998
[5]   Fire performance of load bearing LSF wall systems made of low strength steel studs [J].
Ariyanayagam, Anthony Deloge ;
Mahendran, Mahen .
THIN-WALLED STRUCTURES, 2018, 130 :487-504
[6]   Experimental study of non-load bearing light gauge steel framed walls in fire [J].
Ariyanayagam, Anthony Deloge ;
Mahendran, Mahen .
JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2018, 145 :529-551
[7]  
ASTM, 2017, E2117 ASTM
[8]   Mechanical response of ultra-high strength (Grade 1200) steel under extreme cooling conditions [J].
Azhari, Fatemeh ;
Apon, Al-Amin Hossain ;
Heidarpour, Amin ;
Zhao, Xiao-Ling ;
Hutchinson, Christopher R. .
CONSTRUCTION AND BUILDING MATERIALS, 2018, 175 :790-803
[9]   Mechanical properties of ultra-high strength (Grade 1200) steel tubes under cooling phase of a fire: An experimental investigation [J].
Azhari, Fatemeh ;
Heidarpour, Amin ;
Zhao, Xiao-Ling ;
Hutchinson, Christopher R. .
CONSTRUCTION AND BUILDING MATERIALS, 2015, 93 :841-850
[10]   Experimental investigation of cold-formed steel material at elevated temperatures [J].
Chen, Ju ;
Young, Ben .
THIN-WALLED STRUCTURES, 2007, 45 (01) :96-110